Next Article in Journal / Special Issue
Composition-Regulated Photocatalytic Activity of ZnIn2S4@CdS Hybrids for Efficient Dye Degradation and H2O2 Evolution
Previous Article in Journal
An Investigation of Novel Series of 2-Thioxo-1,3-dithiol-carboxamides as Potential Antispasmodic Agents: Design, Synthesis via Coupling Reactions, Density Functional Theory Calculations, and Molecular Docking
Previous Article in Special Issue
Preparation of High-Performance Polyethylene Nanocomposites with Oleic Acid–Siloxene-Supported Ziegler–Natta Catalysts
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

The Utilization of Rice Husk as Both the Silicon Source and Mesoporous Template for the Green Preparation of Mesoporous TiO2/SiO2 and Its Excellent Catalytic Performance in Oxidative Desulfurization

1
College of Agriculture, Yangtze University, Jingzhou 434000, China
2
College of Chemistry and Environmental Engineering, Yangtze University, Jingzhou 434023, China
*
Author to whom correspondence should be addressed.
Molecules 2024, 29(16), 3856; https://doi.org/10.3390/molecules29163856
Submission received: 13 July 2024 / Revised: 4 August 2024 / Accepted: 13 August 2024 / Published: 14 August 2024
(This article belongs to the Special Issue Functional Nanomaterials in Green Chemistry, 2nd Edition)

Abstract

:
In recent years, TiO2-based catalysts have received extensive attention from researchers for their excellent oxidative desulfurization (ODS) performances. In this paper, a series of mesoporous TiO2/SiO2 catalysts with different TiO2 loadings are prepared, using an incipient wetness impregnation method with agricultural waste rice husk as both the silicon source and mesoporous template and tetrabutyl titanate as the titanium source. The effect of different TiO2 loadings on the ODS performance of the samples is investigated, and the appropriate TiO2 loading is 2.5%. Compared with pure TiO2, the 2.5%TiO2/SiO2 sample exhibits high catalytic activity for oxidative desulfurization. This is, on the one hand, due to the high specific surface area and mesopore volume of the 2.5%TiO2/SiO2 sample. On the other hand, it is due to the uniform dispersion of TiO2 grains with an average diameter of 6.1 nm on the surface of the mesoporous SiO2 carrier, which greatly increases the active sites of the 2.5%TiO2/SiO2 sample, thus improving the catalytic activity of the sample. The recycling performances of the 2.5%TiO2/SiO2 sample are further investigated. The results show that, after fifteen cycles, the 2.5%TiO2/SiO2 sample still maintains high conversions of dibenzothiophene (99.8%) and 4,6-dimethyldibenzothiophene (99.7%) without deactivation. In addition, the 2.5%TiO2/SiO2 sample treated with TBHP aqueous solution is characterized by the technique of UV-Vis, and the Ti-peroxo (Ti-OOtBu) species, the active intermediate for the ODS of bulky organic sulfides, is successfully captured. Finally, a possible reaction mechanism for the ODS process over the 2.5%TiO2/SiO2 sample is proposed.

Graphical Abstract

1. Introduction

SOx gases emitted from the combustion of sulfides in fuel oil cause a series of environmental pollution problems [1]. Therefore, many countries around the world are adopting increasingly stringent requirements for the sulfur content in fuel oil, and China has relied on VIA standard gasoline (sulfur content < 10 ppm) since 1 January 2019 [2]. Among the various desulfurization technologies, oxidative desulfurization (ODS) is a desulfurization technology that first oxidizes thiophene sulfides in fuel oils into corresponding sulfoxide or sulfone compounds under the action of catalysts and oxidants, and then separates them from the system using polar solvents. This technology is considered as one of the effective methods for deep desulfurization due to its advantages such as mild reaction conditions, low input costs, and the easier removal of thiophene sulfides without affecting the octane number of fuel oils [3,4].
The commonly used catalysts for oxidative desulfurization mainly include polymetallic oxides [5] and their composites [6], titanium-containing molecular sieves [7,8], and transition metal oxides [9,10,11,12,13,14,15,16], etc. Among these catalysts, TiO2-SiO2 composites are favored by researchers for their excellent desulfurization performance [13,14,15,16]. Ji et al. [13] prepared amorphous TiO2-SiO2 composites with different TiO2 contents using a precipitation method. Among them, the 40%TiO2-SiO2 composite had a desulfurization rate of 78% in the ODS of gasoline with hydrogen peroxide–acetic acid as the oxidant. Liu et al. [14] synthesized amorphous mesoporous TiO2-SiO2 composites by introducing n-propyltriethoxysilane (PTES) into the synthesis system of titanium silicalite-1. Among them, the TS-0.2 (the PTES/Si molar ratio: 0.2) sample showed high catalytic activity and stability in the ODS of dibenzothiophene (DBT) and 4,6-dimethyldibenzothiophene (4,6-DMDBT) model oils. After five cycles, TS-0.2 still maintained high DBT conversion (99.0%) and 4,6-DMDBT conversion (99.8%) rates without deactivation. Bazyaria et al. [15] prepared microporous TiO2-SiO2 nanocomposites with different TiO2 contents by the sol–gel method. Among them, the TiO2-SiO2 (the TiO2 loading: 50 wt.%) had a desulfurization rate of over 99% in the ODS of DBT model oil with TBHP as the oxidant. However, the cyclic experiments were conducted only twice. Ghahramaninezhad et al. [16] synthesized a novel catalyst (TS-4/CM-β-CD) by combining carboxymethyl-functionalized β-cyclodextrin with TiO2/SiO2 nanoparticles under the action of cyanamid. Under the optimized reaction conditions, the TS-4/CM-β-CD catalyst achieved a DBT desulfurization rate of 99.6%. After three cycles, TS-4/CM-β-CD still maintained a high DBT desulfurization rate (99.0%). However, most of the above-mentioned TiO2-SiO2 composites were prepared using commercial tetraethyl silicate (TEOS) as the silicon source. The production process of TEOS is both expensive and environmentally unfriendly [17]. Therefore, in order to minimize the environmental and economic impacts of using TEOS, it is particularly important to find a green, inexpensive, and environmentally friendly silicon source.
Rice husk (RH) is an agricultural residue produced during rice processing. RH mainly contains 22.31% lignin, 36.11% cellulose, 19.45% hemicellulose, and 20.11% silica [18]. RH is rich in amorphous silica, which is a green silicon source that can replace commercially available TEOS. The pathway of using RH as a silica source for the preparation of SiO2-based catalytic materials is an economical and environmentally friendly approach, which is in line with the principles of Green Chemistry [12,19,20,21]. Recently, our team [12] prepared a series of mesoporous WO3/SiO2 catalysts with different WO3 loadings, using the incipient wetness impregnation method with RH as both the silicon source and mesoporous template and phosphotungstic acid as the tungsten source. Among them, the WS-923-15 sample showed good catalytic activity and stability in the ODS of DBT and 4,6-DMDBT model oils. As an extension of the above work, in this paper, a series of mesoporous TiO2/SiO2 catalysts with different TiO2 loadings are continued to be prepared by a similar method, using RH as both the silicon source and mesoporous template and tetrabutyl titanate (TBOT) as the titanium source. The catalytic performances of the TiO2/SiO2 samples in the ODS of DBT and 4,6-DMDBT model oils are studied, the recycling performances of the TiO2/SiO2 samples are investigated, and the catalytic mechanism of the ODS process is explored.

2. Results and Discussion

2.1. Structural Characterizations

For the convenience of readers, the nomenclature of the catalysts is first explained. For example, in ‘TS-RH-2.5c’, ‘TS’ is the abbreviation for TiO2/SiO2 catalysts, ‘RH’ is the abbreviation for rice husk, ‘TS-RH’ denotes TiO2/SiO2 catalysts prepared using RH as feedstock, ‘2.5’ stands for the loading of TiO2, and ‘c’ stands for the regenerated sample (see Section 3.2 and Section 3.5 for details).
Figure 1 shows the XRD patterns of the SiO2-RH, pure TiO2, TS-RH-x, and TS-RH-xc samples. As can be seen from Figure 1a, the SiO2-RH carrier has a broad and diffuse diffraction peak near 23.0°, indicating that it has an amorphous structure. Pure TiO2 exhibits diffraction peaks at 25.3°, 37.8°, 48.0°, 54.0°, 55.1°, and 62.9°, which correspond to the (101), (004), (200), (105), (211), and (204) crystal planes of the anatase phase of TiO2 (JCPDS no. 21-1272), respectively [22]. With an increase in TiO2 loading from 0.5 to 2.5%, the TS-RH-x samples still display a broad and diffuse diffraction peak near 23.0°, indicating that the samples have an amorphous structure and the TiO2 grains are highly dispersed on the surface of the SiO2-RH carrier. Continuing to increase the loading of TiO2, the samples start to exbibit the characteristic peaks of anatase TiO2. In addition, compared with the fresh TS-RH-2.5 sample (Figure 1b), the regenerated samples show an amorphous structure despite the appearance of a very weak diffraction peak of anatase TiO2 at 25.3°.
Figure 2 shows the UV-Vis spectra of the samples. As shown in Figure 2a, the pure TiO2 has distinct absorption bands in the UV region (at 206, 261, and 352 nm) and no photo-response in the visible region [22]. TS-RH-0.5 displays three absorption bands at 205, 255, and 310 nm, corresponding to the tetra-coordinated titanium species, hexa-coordinated titanium species, and anatase-phase TiO2, respectively [14,23,24]. As the TiO2 loading increases from 0.5 to 2.5%, the absorption intensity gradually increases and the peak width gradually broadens. Moreover, the main absorption band redshifts from 205 to 256 nm. Continuing to increase the TiO2 loading, the redshift of the maximum absorption band is not large, the absorption intensity is gradually enhanced, and the peak width is gradually widened. The above results show that the strongest absorption band redshifts occur with increasing the TiO2 loading, indicating an increase in the coordination number of titanium species in the sample [23,24]. It has been shown that both tetra- and hexa-coordinated titanium species exhibit good catalytic oxidation activity in the presence of organic peroxides [24]. As shown in Figure 2b, compared to the spectra of the oxidized products, the TS-RH-2.5c samples are free of DBT and 4,6-DMDBT oxidized products after regeneration by calcinating. Compared with the fresh TS-RH-2.5 sample, the absorption intensity of the regenerated samples is slightly reduced, indicating that their TiO2 loadings are not reduced to a large extent after the recycle tests.
Figure 3 shows the N2 adsorption–desorption isotherms and pore size distributions of the samples. As can be seen from Figure 3a, both the SiO2-RH and TS-RH-x samples show typical type IV isotherms in the IUPAC classification, with a clear H4 hysteresis loop at P/P0 > 0.40, suggesting that the samples have a mesoporous structure. The isothermal shapes of the TS-RH-x samples are similar compared to the SiO2-RH, suggesting that they have similar pore structures. The pores in the SiO2-RH carrier are centrally distributed within the range of 1.9–78 nm, with the most probable pore size being 3.6 nm (Figure 3b). With an increase in the TiO2 loading from 0.5 to 10%, the pore distribution and the most probable pore size of the TS-RH-x samples do not change much, while the SBET and Vmeso decrease slightly, indicating that the TiO2 grains are well dispersed on the surface/pores of the SiO2-RH carrier and do not block its pores. Compared with the pure TiO2, the TS-RH-x samples have a larger SBET and Vmeso, which is conducive to the easy access of bulky substrates to the active sites, overcoming the diffusion effect, thus improving the catalytic performances of the samples [12,25]. As shown in Figure 3c,d, the shapes of the isotherms and pore distribution curves of the regenerated samples do not change much, and the SBET and Vmeso slightly decrease compared with those of the fresh TS-RH-2.5 sample (Table 1). These results indicate that the pore structures of the regenerated samples remain well after the recycle tests.
Figure 4 shows the SEM images of the SiO2-RH, pure TiO2, TS-RH-2.5, and TS-RH-2.5c samples. The pure TiO2 sample exhibits an uneven morphology, which is an aggregated structure composed of micrometer-sized grains (Figure 4a). The SiO2-RH carrier consists of particles of different sizes and no specific shape, with a maximum particle size of about 7 µm (Figure 4b). After TiO2 loading, there is little change in the morphology of the TS-RH-2.5 sample (Figure 4c). Compared with TS-RH-2.5, the morphology of the regenerated samples also does not change much after the recycle tests (Figure 4d,e). As can be seen from Figure 5, the Ti, Si, and O elements of all the samples are uniformly distributed over the entire surface, indicating that the TiO2 grains are relatively uniformly dispersed on the surface of the SiO2-RH carrier. This result is consistent with the results of XRD. Compared with the fresh TS-RH-2.5, there is no significant decrease in the number of Ti spots in the TS-RH-2.5c sample regenerated from 15th ODS reaction of 4,6-DMDBT, while the number of Ti spots in the TS-RH-2.5c sample regenerated from the 15th ODS reaction of DBT is slightly reduced. These results indicate that the TiO2 loadings of the regenerated samples decrease insignificantly after the recycle tests.
Figure 6 and Figure 7 show TEM pictures and histograms of the particle size distributions of the samples, respectively. As shown in Figure 6a, the SiO2-RH sample has a large number of mesopores, which is consistent with the results of the N2 adsorption–desorption isotherms. After TiO2 loading, some TiO2 grains with an average diameter of 6.1 nm appear in the TS-RH-2.5 sample, which are dispersed relatively uniformly on the surface of the SiO2-RH carrier (Figure 6b, yellow circles, and Figure 7a). After the 15th run, nanoscale TiO2 grains are still observed on the SiO2-RH carrier and remain uniformly distributed (Figure 6c,d, yellow circles). In addition, the average diameters of the TiO2 grains in the TS-RH-2.5c samples regenerated from the 15th ODS reactions of DBT and 4,6-DMDBT are 6.1 and 6.3 nm, respectively (Figure 7b,c). These results indicate that the TiO2 grains do not agglomerate during multiple calcination and regeneration, resulting in a good catalytic stability of the TS-RH-2.5 sample.

2.2. Catalytic Performance on Oxidative Desulfurization

The catalytic performances of the TS-RH-x samples are investigated using the ODS reactions of DBT and 4,6-DMDBT model oils as the probe reactions, and the results are shown in Table 1. When the TiO2 loading is 0.5%, the conversions of DBT and 4,6-DMDBT are 97.7% and 96.6%, respectively. As the TiO2 loading increases from 0.5 to 2.5%, the conversions of DBT and 4,6-DMDBT increase. Continuing to increase the TiO2 loading, the conversions of DBT and 4,6-DMDBT do not change much. Therefore, the more suitable TiO2 loading is 2.5%. Figure 8 shows the effect of reaction time on the ODS performance of the TS-RH-2.5 sample. It can be seen that, as the reaction time is prolonged from 15 min to 2 h, the conversions of DBT and 4,6-DMDBT increase linearly. Continuing to prolong the reaction time, the conversions of DBT and 4,6-DMDBT remain basically unchanged. Therefore, the more suitable reaction time for both the DBT and 4,6-DMDBT model oils is 2 h.
In order to investigate the reason for the good catalytic performance of the TS-RH-2.5 sample in the ODS of DBT and 4,6-DMDBT model oils, several blank reactions were designed and carried out under the reaction conditions in Table 1. When the catalyst was not involved in the reaction, the conversions of DBT and 4,6-DMDBT were 21.8 and 15.1%, respectively, indicating that the oxidizing effects of TBHP on DBT and 4,6-DMDBT were poor. When TS-RH-2.5 was used as the catalyst and no oxidant was added, the conversions of DBT and 4,6-DMDBT were 20.0% and 14.0%, respectively, indicating that the TS-RH-2.5 sample had a certain adsorption desulfurization effect, but this effect was poor [15]. Compared to the results of the catalyst blank experiment, the conversions of DBT and 4,6-DMDBT increased slightly when the SiO2-RH and pure TiO2 were used as the catalysts (see Table 1), indicating that the SiO2-RH and pure TiO2 were poorly active. Based on the above characterization results, as well as the results of the blank experiments, the good catalytic oxidative desulfurization performance of TS-RH-2.5 can be attributed to (1) its high specific surface area and mesopore volume and (2) the uniform dispersion of TiO2 grains with an average diameter of 6.1 nm on the surface of the mesoporous SiO2-RH carrier, which greatly increases the active sites of the sample, consequently improving its catalytic activity.
The oxidation products of DBT and 4,6-DMDBT were analyzed by the means of the FT-IR and LC-MS techniques. As shown in Figure 9a, compared with DBT, two new absorption peaks at 1166 and 1288 cm−1 appear in the oxidation product of DBT, which can be attributed to the symmetric and asymmetric stretching vibrations of the sulfone (O=S=O), respectively [26,27]. Similarly, the 4,6-DMDBT oxidation product presents new absorption peaks at 1151 and 1282 cm−1 (Figure 9b), which can be attributed to the symmetric and asymmetric stretching vibrations of the sulfone (O=S=O), respectively [26,27]. As shown in Figure 10, the ion peak at the mass to charge ratio (m/z) of 217.0319 matches well with the m/z of the dibenzothiophene sulfone (DBTO2) quasi-molecular ion ([M+H]+, 217.0318). Moreover, the ion peak at the m/z of 245.0619 has a good match with the m/z of the 4,6-dimethyldibenzothiophene sulfone (4,6-DMDBTO2) quasi-molecular ion ([M+H]+, 245.0631). The above results demonstrate that the oxidation products of DBT and 4,6-DMDBT are DBTO2 and 4,6-DMDBTO2, respectively. It is worth noting that the presence of sulfoxide is not detected in the FT-IR and LC-MS characterizations of the oxidation products of DBT and 4,6-DMDBT. This result indicates that sulfoxide would be very unstable in this reaction system and is further oxidized to the corresponding sulfone, which is consistent with the results reported in the literature [8,28].
Figure 11 shows the results of the cyclic experiments for the TS-RH-2.5 sample. As one can see from Figure 11, after the 15th run, the conversion of DBT remains as high as 99.8%, and the conversion of 4,6-DMDBT remains as high as 99.7%. The samples before and after the recycle tests were characterized by the means of the XRD, UV-Vis, N2 adsorption–desorption isotherms, SEM, TEM, and ICP-OES techniques. The results of XRD (Figure 1b) indicate that the regenerated samples still have an amorphous structure compared to the fresh sample. The results of UV-Vis (Figure 2b) indicate that the regeneration of the spent catalysts using the calcinating method is effective in removing the adsorbed oxidized products from the catalysts, and the reduction in the TiO2 loading of the regenerated samples is not significant compared to the fresh sample. The results of the N2 adsorption–desorption isotherms (Figure 3c,d, Table 1) indicate that the pore structures of the regenerated samples are well-maintained after the recycle tests. The results of SEM and EDS (Figure 4 and Figure 5) demonstrate that the morphology of the regenerated samples remains unchanged, the distribution of the TiO2 grains on the surface of the SiO2-RH carrier remains relatively uniform, and the loading of TiO2 decreases insignificantly. The results of TEM (Figure 6 and Figure 7) suggest that the nano-sized TiO2 grains still remain uniformly distributed on the SiO2-RH carrier without agglomeration after the recycle tests. The results of ICP-OES show that the TiO2 loadings of TS-RH-2.5, TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT are 2.55, 2.21, and 2.28%, respectively. These results indicate that the loss of TiO2 during the recycle tests is negligible. The above results indicate that the TS-RH-2.5 sample has a good catalytic activity and recycling performance. In addition, as shown in Table 2, compared with the TiO2-based catalysts reported in the literature [14,15,16,29,30,31,32], the recycling performance of the TS-RH-2.5 sample prepared in this work is comparable or better than those of the reported samples.

2.3. Reaction Mechanism of the ODS Process

Similar to our previously reported method [7], the samples were treated with an aqueous solution of TBHP and detected by the means of the UV-Vis technique, allowing for the capture of Ti-peroxo species. The color of the TS-RH-2.5 sample changed from white to light yellow after the treatment with the TBHP aqueous solution, and a clear absorption peak appeared at 370–600 nm (see Figure 12), which can be attributed to the charge transfer transition of the peroxo ligand to the titanium center in the Ti-peroxo species, indicating that the Ti-peroxo species (Ti-OOtBu) was produced [7,31,32,33]. Generally, the Ti-peroxo species is considered to be the active intermediate in the catalytic oxidation of various organic substrates in catalytic systems containing TiO2-based catalysts and hydroperoxide [7,31,32,33]. In addition, the TS-RH-2.5c samples regenerated after the 15th recycle test were subjected to the same treatment, and both of them showed significant absorption peaks at 370–600 nm, indicating that the regenerated samples still had a strong ability to bind TBHP to form the Ti-OOtBu species. This result is in agreement with the results of the cyclic experiments.
The UV-Vis results indicate that the TS-RH-2.5 sample contains tetra-coordinated titanium species, hexa-coordinated titanium species, and anatase-phase TiO2. Among them, the hexa-coordinated titanium species is the main component. Generally, the silicon in amorphous SiO2 is interconnected in a silico-oxygen tetrahedron manner. Based on the results of XRD and UV-Vis, as well as the properties of amorphous TiO2/SiO2 [23,24], the structural schematic of the TS-RH-2.5 sample represented by hexa-coordinated titanium species can be illustrated as shown in Scheme 1. From the Scheme 1, it can be seen that the titanium atoms not only bind to two silico-oxygen tetrahedrons through oxo-bridges, but also bind to two water molecules and two hydroxyl groups.
Based on the results of Figure 9, Figure 10 and Figure 12, the reaction mechanism and process flow for the oxidative removal of DBT and 4,6-DMDBT in the TS-RH-2.5 and TBHP catalytic system are proposed, as shown in Scheme 1. First, the catalyst, model oil, and TBHP are fed in a set ratio. The reaction starts with the nucleophilic attack of TBHP on the titanium active sites to form the active intermediate Ti-OOtBu species. Then, the sulfur atoms in DBT (or 4,6-DMDBT) nucleophilically attack the Ti-OOtBu species to generate the sulfoxides, while releasing the TS-RH-2.5 catalyst. The sulfoxides are very unstable in this reaction system and are quickly oxidized by the Ti-OOtBu species to form the corresponding sulfones [8,28]. In this reaction system, the by-product is tert-butanol [28]. Since the sulfones are insoluble in n-octane, the products and catalysts precipitate out of the reaction medium immediately after the reaction. Therefore, at the end of the reaction, a simple filtration or centrifugation is all that is required to obtain the desulfurized model oil and the solid. The solid is centrifuged and washed by hot acetonitrile to obtain the supernatant and the remaining solid. Then, the supernatant is concentrated by rotary evaporation and vacuum-dried to obtain the oxidized product. The remaining solid is then dried and calcined to obtain the regenerated sample. Finally, the regenerated sample can be recycled for cycling experiments of the ODS. The whole ODS process is simple, mild, and easy to control, which is a beneficial supplement to the current industrial hydrodesulfurization process.

3. Materials and Methods

3.1. Materials

RH originated from the College of Agriculture of Yangtze University (Jingzhou, China). Tetrabutyl titanate (TBOT, 97%) and Tert-butyl hydroperoxide (TBHP, ~5.5 mol/L in decane) were purchased from Sigma Aldrich (Shanghai, China) Trading Co., Ltd. Dibenzothiophene (DBT, 99%), 4,6-dimethyldibenzothiophene (4,6-DMDBT, 97%), and TBHP solution (70% in H2O) were purchased from Shanghai Aladdin Biochemical Technology Co., Ltd. (Shanghai, China). Isopropanol (IPA), hydrochloric acid, n-octane, acetonitrile, ethanol, and other reagents (A.R.) were purchased from Sinopharm Chemical Reagent Co., Ltd. (Shanghai, China).

3.2. Synthesis of TiO2/SiO2 Samples

The RH was pretreated with hydrochloric acid according to the method reported by our team [12] to obtain pretreated RH powder. About 20.0 g of the pretreated RH powder was dried at 383 K for 4 h to obtain the absolutely dried RH powder. About 5.0 g of the absolutely dried RH powder was calcined at 873 K for 5 h to obtain the SiO2 powder in RH, which was denoted as SiO2-RH. Accordingly, the mass fraction of SiO2-RH in the absolutely dried RH powder can be calculated as 19.6 wt.%. TiO2/SiO2 catalysts were prepared by the incipient wetness impregnation method using the absolutely dried RH powder as both the mesoporous template and silicon source [12]. A typical preparation operation was as follows: first, 10.0 g of RH powder was placed in a 100 mL beaker. Then, TBOT was dissolved in 10.3 mL of IPA according to the mass ratio of TiO2:SiO2 = x:100 to obtain a light yellow clear solution. The clear solution was added drop by drop to the RH powder with constant stirring until a saturated impregnation state was achieved. Then, the mixture was aged at room temperature for about 24 h and dried at 383 K for 8 h. Finally, white powder was obtained by grinding and calcining at 873 K for 5 h (1 K/min). It was labeled as TS-RH-x, where ‘x’ represents the loading of TiO2. Using a similar method, TS-RH-0.5, TS-RH-1.0, TS-RH-5.0, and TS-RH-10 samples were prepared.
As a comparison, TiO2 was prepared by direct calcination. Typically, about 4.0 g of TBOT was placed in an evaporating dish and hydrolyzed naturally in the air at room temperature for 24 h to obtain a white solid. Then, the white solid was dried at 383 K for 6 h. Finally, the white solid was ground and calcined at 873 K for 4 h to obtain TiO2 powder.

3.3. Treatment of Samples with TBHP Aqueous Solution

The samples were treated with a 70% aqueous solution of TBHP according to the method reported by our team [7]. Typically, 50 mg of the TS-RH-2.5 sample was placed in a 25 mL beaker and 0.5 mL of TBHP aqueous solution was added dropwise. The mixture was stirred thoroughly with a glass rod to achieve a saturated impregnation state. Finally, the mixture was dried in a fume hood at room temperature for about 3 h, and a light yellow powder was obtained.

3.4. Characterization

The XRD patterns were recorded with Cu-Kα radiation on a Panalytical Empyrean X-ray diffractometer (Malvern Panalytical Ltd., Malvern, UK) with a scanning angle (2θ) of 10–80°. The UV-Vis spectra were measured by a Lambda 650S spectrometer (PerkinElmer Inc., Shelton, CT, USA) with a spectral range of 190–800 nm. The FT-IR spectra were measured by a Nicolet 6700 infrared spectrometer (Thermo Fisher Scientific Inc., Waltham, MA, USA) with a pure KBr background. Measurements were made over a wavelength range of 400–4000 cm−1. The SEM images and elemental maps were taken by a TESCAN MIRA3 field emission scanning electron microscope (TESCAN ORSAY Holding, a.s., Brno, Kohoutovice, Czech Republic) equipped with an XFlash Detector 630M energy dispersive spectrometer (EDS, Bruker Nano GmbH, Berlin, Germany). The TEM images were collected by an FEI TECNAI F20 transmission electron microscope (FEI Inc., Hillsboro, OR, USA). The elemental contents of the samples were determined by a PerkinElmer Optima 8000 inductively coupled plasma emission spectrometer (PerkinElmer Inc., Shelton, CT, USA). About 100 mg of the sample was placed in a high-pressure digestion jar, 2.0 mL of aqueous hydrofluoric acid (40%) was added, and low-temperature digestion (2 h at 323 K) was carried out in microwave digestion apparatus (MARS6, CEM Corporation, Matthews, NC, USA). After digestion, the solution was diluted and fixed in a plastic volumetric flask. Blanks were subjected to the same procedure. In addition, a mixed standard solution of silicon and titanium was prepared using standard stock solutions, the absorbances were measured at the set wavelengths, and the standard curves were drawn. The sample solutions were measured and their elemental contents were calculated from the standard curve. Two parallel samples were made for each sample and the final result was taken as the average of the two measurements. The N2 adsorption–desorption isotherms were carried out on a Micromeritics ASAP 2020HD88 physical adsorption instrument (Micromeritics Instrument Corporation, Norcross, GA, USA) at 77 K. Prior to analysis, all of the samples were degassed at 573 K for 4 h. The specific surface area (SBET) was determined by the BET equation. The cumulative pore volume (Vmeso) and pore size distribution were calculated by the Barrett–Joyner–Halenda (BJH) model from the desorption branch of the N2 physisorption isotherms. The absorption spectra and standard curves of the DBT and 4,6-DMDBT model oils were determined by a TU–1900 UV-Vis spectrophotometer (Beijing Puxi general instrument Co., Ltd., Beijing, China). The oxidized products of DBT and 4,6-DMDBT were analyzed by high-resolution liquid chromatography–mass spectrometry (LC-MS, Triple TOF 5600+, AB SCIEX Ltd., Framingham, MA, USA), a hybrid triple quadrupole time-of-flight mass spectrometer equipped with an ESI source operating in positive ion mode.

3.5. Catalytic Activity and Recycle Tests

3.5.1. Catalytic Activity

The selective oxidation reactions of DBT and 4,6-DMDBT were carried out in a 50 mL two-necked flask immersed in an oil bath and equipped with a condenser. The model oils of DBT and 4,6-DMDBT were prepared using n-octane as a solvent, and they all had a sulfur content of 1000 ppmw. Typically, 0.100 g of the TS-RH-2.5 catalyst and 10 mL of the DBT (or 4,6-DMDBT) model oil were added to the flask, and the mixture was stirred and heated to 333 K. The reaction was then initiated by adding 83 μL of TBHP (TBHP/S molar ratio of 2.1). The reaction was stopped after 2 h. The reaction mixture was cooled and centrifuged to obtain the oil phase and the solid.
The absorbance of the oil phase at 236 nm (241 nm for 4,6-DMDBT model oil) was determined on a TU-1900 UV-Vis spectrophotometer using ethanol as the diluent solvent and reference solution. The standard curve method was used to calculate the amount of DBT remaining in the oil phase, and the standard curves of the DBT and 4,6-DMDBT model oils are shown in Figure 13. As can be seen from Figure 13, the linear regression equation of the DBT model oil is y = 1.16516 x, with a correlation coefficient R2 of 0.9999 and a linear range of 0–0.504 ppmw. Similarly, the linear regression equation for the 4,6-DMDBT model oil is y = 1.06447 x, with a correlation coefficient R2 of 0.9997 and a linear range of 0–0.501 ppmw. The conversions of DBT and 4,6-DMDBT (X) were defined as the amount of the sulfide reacted divided by the initial amount of the sulfide added.
Moreover, the DBT and 4,6-DMDBT model oils before and after the ODS reaction were diluted the same number of times (2000 times), and their absorption spectra were determined (see Figure 14). It is obvious from Figure 14 that the absorbances of the reacted DBT and 4,6-DMDBT model oils at the set wavelengths were greatly reduced to almost zero compared with before the reaction. These results indicate that the TS-RH-2.5 sample has high oxidative desulfurization activity.
In addition, the solid was centrifuged and washed several times with hot acetonitrile (323 K) to obtain the supernatant and the remaining solid. Then, the supernatant was concentrated on a rotary evaporator, and the residue was dried in a vacuum oven at room temperature for 24 h to obtain the oxidized product of DBT (or 4,6-DMDBT). Finally, the remaining solid was dried overnight at 383 K and calcined at 823 K for 2 h (1 K/min) to obtain the regenerated sample, which was labeled as TS-RH-xc.

3.5.2. Recycle Tests

Cycling experiments with the TS-RH-2.5 sample were performed in a 250 mL three-necked flask equipped with a condenser. The typical cyclic experimental procedure was similar to that in Section 3.5.1, with the following conditions for the first oxidation reaction: 150 mL of the DBT (or 4,6-DMDBT) model oil, 1.500 g of the catalyst, 1245 μL of TBHP, a temperature of 333 K, and a reaction time of 2 h. In each run, the dosages of TBHP and the model oil were calculated based on the ratio of catalyst to oil (10.0 g/L), the molar ratio of TBHP/S (2.1), and the mass of the catalyst obtained in the previous run.

4. Conclusions

In summary, a series of mesoporous TS-RH-x samples were prepared using the incipient wetness impregnation method with RH as both the silicon source and mesoporous template. The samples were characterized more systematically using a series of characterization techniques. The results showed that, when the loading of TiO2 was lower than 2.5%, the samples had an amorphous structure. When the loading of TiO2 was higher than 2.5%, TiO2 in the anatase phase appeared in the samples. Compared with the pure TiO2, the TS-RH-x samples had a high SBET and Vmeso. For the TS-RH-2.5 sample, TiO2 grains with an average diameter of 6.1 nm were uniformly dispersed on the surface of the mesoporous SiO2-RH carrier, which greatly increased the active sites of the TS-RH-2.5 sample, thus improving its catalytic activity. As a result, the TS-RH-2.5 sample exhibited high catalytic activity in the ODS of the DBT and 4,6-DMDBT model oils. The recycling performances of the TS-RH-2.5 sample were further investigated and the samples before and after the recycle tests were characterized. The results showed that the TS-RH-2.5 sample still maintained high DBT conversion (99.8%) and 4,6-DMDBT conversion (99.7%) rates without inactivation after the 15th run. The relevant characterization results showed that the crystal structure, pore structure, and morphology of the samples were well-maintained after the recycle tests. Using the UV-Vis technique, the Ti-OOtBu species, the active intermediate of the ODS reaction, was successfully captured. In addition, a possible mechanism for the ODS of bulky organic sulfides over TS-RH-2.5 was proposed. The TS-RH-2.5 sample had a good structural stability and recycling performance, and it will be well applied in the deep oxidative desulfurization of fuel oils.

Author Contributions

Conceptualization, X.L. and L.Z.; methodology, X.L. and J.H.; validation, W.Z. and X.X.; formal analysis, W.Z. and L.Q.; investigation, X.L. and L.Q.; resources, L.Z., X.X. and H.C.; data curation, J.H. and W.Z.; writing—original draft preparation, L.Z., X.L. and J.H.; writing—review and editing, H.C., L.Z. and X.L.; visualization, X.L. and H.C.; supervision, X.L. and H.L.; project administration, H.L.; funding acquisition, H.L. All authors have read and agreed to the published version of the manuscript.

Funding

This work is supported by the National Natural Science Foundation of China (21303008) and the Natural Science Foundation of Hubei Province of China (2012FFB00103).

Institutional Review Board Statement

Not applicable.

Data Availability Statement

The original contributions presented in the study are included in the article, further inquiries can be directed to the corresponding author.

Conflicts of Interest

The authors declare no conflicts of interest.

References

  1. Campos-Martin, J.M.; Capel-Sanchez, M.C.; Perez-Presas, P.; Fierro, J.L.G. Oxidative processes of desulfurization of liquid fuels. J. Chem. Technol. Biotechnol. 2010, 85, 879–890. [Google Scholar] [CrossRef]
  2. Announcement No. 16 of 2018 by the National Development and Reform Commission of the People’s Republic of China. Available online: https://www.ndrc.gov.cn/xxgk/zcfb/gg/201812/t20181229_961214_ext.html (accessed on 29 December 2018).
  3. Jiang, Z.; Lü, H.; Zhang, Y.; Li, C. Oxidative desulfurization of fuel oils. Chin. J. Catal. 2011, 32, 707–715. [Google Scholar] [CrossRef]
  4. Haghighi, M.; Gooneh-Farahani, S. Insights to the oxidative desulfurization process of fossil fuels over organic and inorganic heterogeneous catalysts: Advantages and issues. Environ. Sci. Pollut. Res. 2020, 27, 39923–39945. [Google Scholar] [CrossRef] [PubMed]
  5. Wang, R.; Zhang, G.; Zhao, H. Polyoxometalate as effective catalyst for the deep desulfurization of diesel oil. Catal. Today 2010, 149, 117–121. [Google Scholar] [CrossRef]
  6. Yan, X.M.; Mei, P.; Xiong, L.; Gao, L.; Yang, Q.; Gong, L. Mesoporous titania–silica–polyoxometalate nanocomposite materials for catalytic oxidation desulfurization of fuel oil. Catal. Sci. Technol. 2013, 3, 1985–1992. [Google Scholar] [CrossRef]
  7. Huai, J.; Liu, X.; Zhang, Y.; Yang, Y.; Gou, Y.; Qin, L.; Shan, J.; Zheng, Y.; Li, H. Synthesis of hierarchical TS-1 and its recycling catalytic property for oxidative desulfurization. J. Renew. Mater. 2022, 10, 1711–1726. [Google Scholar] [CrossRef]
  8. Du, Q.; Guo, Y.; Wu, P.; Liu, H.; Chen, Y. Facile synthesis of hierarchical TS−1 zeolite without using mesopore templates and its application in deep oxidative desulfurization. Microporous Mesoporous Mater. 2019, 275, 61–68. [Google Scholar] [CrossRef]
  9. Manriquez-Ramirez, M.E.; Valdez, M.T.; Castro, L.V.; Flores, M.E.; Ortiz-Islas, E. Application of CeO2-V2O5 catalysts in the oxidative desulfurization of 4,6-dimethyl dibenzothiophene as a model reaction to remove sulfur from fuels. Mater. Res. Bull. 2022, 153, 111864. [Google Scholar] [CrossRef]
  10. Jiang, W.; Xiao, J.; Gao, X.; An, X.; Leng, Y.; Zhu, L.; Zhu, W.; Li, H. In situ fabrication of hollow silica confined defective molybdenum oxide for enhanced catalytic oxidative desulfurization of diesel fuels. Fuel 2021, 305, 121470. [Google Scholar] [CrossRef]
  11. Mokhtar, W.N.A.W.; Abu Bakar, W.A.W.; Ali, R.; Abdul Kadir, A.A. Catalytic oxidative desulfurization of diesel oil by Co/Mn/Al2O3 catalysts—Tert-butyl hydroperoxide (TBHP) system: Preparation, characterization, reaction, and mechanism. Clean Technol. Environ. Policy 2015, 17, 1487–1497. [Google Scholar] [CrossRef]
  12. Zhang, Y.; Liu, X.; Zhao, R.; Zhang, J.; Zhang, L.; Zhang, W.; Hu, J.; Li, H. The Green Preparation of Mesoporous WO3/SiO2 and Its Application in Oxidative Desulfurization. Catalysts 2024, 14, 103. [Google Scholar] [CrossRef]
  13. Ji, Y.; Liu, J.; Jian, P. Synthesis of amorphous TiO2-SiO2 composite oxides and their catalytic activity for oxidative desulfurization of gasoline. Ind. Catal. 2014, 22, 869–873. [Google Scholar]
  14. Liu, X.; Liu, X.; Shan, J.; Huai, J.; Yang, H.; Yan, X.; Zheng, Y.; Li, H. Synthesis of amorphous mesoporous TiO2-SiO2 and its excellent catalytic performance in oxidative desulfurization. Inorg. Chem. Commun. 2021, 123, 108336. [Google Scholar] [CrossRef]
  15. Bazyari, A.; Khodadadi, A.A.; Mamaghani, A.H.; Beheshtian, J.; Thompson, L.T.; Mortazavi, Y. Microporous titania-silica nanocomposite catalyst-adsorbent for ultra-deep oxidative desulfurization. Appl. Catal. B 2016, 180, 65–77. [Google Scholar] [CrossRef]
  16. Ghahramaninezhad, M.; Ahmadpour, A. Carboxylmethyl-β-cyclodextrin as a good modifier agent for oxidation of dibenzothiophene. Surf. Interfaces 2022, 28, 101612. [Google Scholar] [CrossRef]
  17. Bazani, H.A.G.; Thomé, A.; Affeldt, R.F.; Probst, L.F.D. SBA-15 obtained from rice husk ashes wet-impregnated with metals (Al, Co, Ni) as efficient catalysts for 1,4-dihydropyridine three-component reaction. New J. Chem. 2022, 46, 7899–7909. [Google Scholar] [CrossRef]
  18. Cui, J.; Cheng, F.; Lin, J.; Yang, J.; Jiang, K.; Wen, Z.; Sun, J. High surface area C/SiO2 composites from rice husks as a high-performance anode for lithium ion batteries. Powder Technol. 2017, 311, 1–8. [Google Scholar] [CrossRef]
  19. Grisolia, A.; Dell’Olio, G.; Spadafora, A.; De Santo, M.; Morelli, C.; Leggio, A.; Pasqua, L. Hybrid polymer-silica nanostructured materials for environmental remediation. Molecules 2023, 28, 5105. [Google Scholar] [CrossRef]
  20. Zhao, Y.; Gu, S.; Li, L.; Wang, M. From waste to catalyst: Growth mechanisms of ZSM-5 zeolite from coal fly ash & rice husk ash and its performance as catalyst for tetracycline degradation in fenton-like oxidation. Environ. Pollut. 2024, 345, 123509. [Google Scholar]
  21. Pham, L.K.H.; Alsaiari, M.; Thao, B.T.T.; Hieu, N.H.; Duy, N.P.H.; Vo, D.V.N.; Witoon, T.; Nguyen, V.C.; Kongparakul, S.; Samart, C.; et al. High selective hydrocarbon and hydrogen products from catalytic pyrolysis of rice husk: Role of the ordered mesoporous silica derived from rice husk ash for Ni-nanocatalyst performance. J. Anal. Appl. Pyrolysis 2024, 178, 106383. [Google Scholar] [CrossRef]
  22. Bi, M.; Guo, Y.; Wang, S.; Zhang, B.; Jiang, Y.; Li, H.; Xu, Q.; Chen, L.; Zhao, Q.; Han, N. Titanium dioxide-modified nanosized TS-1 zeolite-supported phosphotungstic acid as a catalyst for deep catalytic oxidative desulfurization of fuel oil. New J. Chem. 2023, 47, 12027–12036. [Google Scholar] [CrossRef]
  23. Gao, X.; Wachs, I.E. Titania–silica as catalysts: Molecular structural characteristics and physico-chemical properties. Catal. Today 1999, 51, 233–254. [Google Scholar] [CrossRef]
  24. Zhang, Y.; Xia, C.; Peng, X.; Lin, M.; Zhu, B.; Duan, Q.; Luo, Y.; Shu, X. Relationship between Ti-Si coordination and catalytic activity for titanosilicates. Acta Pet. Sin. (Pet. Process. Sect.) 2019, 35, 860–867. [Google Scholar]
  25. Bai, R.; Sun, Q.; Song, Y.; Wang, N.; Zhang, T.; Wang, F.; Zou, Y.; Feng, Z.; Miao, S.; Yu, J. Intermediate-crystallization promoted catalytic activity of titanosilicate zeolites. J. Mater. Chem. A 2018, 6, 8757–8762. [Google Scholar] [CrossRef]
  26. Otsuki, S.; Nonaka, T.; Takashima, N.; Qian, W.H.; Ishihara, A.; Imai, T.; Kabe, T. Oxidative desulfurization of light gas oil and vacuum gas oil by oxidation and solvent extraction. Energy Fuels 2000, 14, 750–753. [Google Scholar] [CrossRef]
  27. Socrates, G. Sulphur and selenium compounds. In Infrared and Raman Characteristic Group Frequencies: Tables and Charts, 3rd ed.; John Wiley & Sons Ltd.: Chichester, UK, 2001; pp. 211–218. [Google Scholar]
  28. Serrano, D.P.; Sanz, R.; Pizarro, P.; Moreno, I.; Medina, S. Hierarchical TS−1 zeolite as an efficient catalyst for oxidative desulphurization of hydrocarbon fractions. Appl. Catal. B Environ. 2014, 146, 35–42. [Google Scholar] [CrossRef]
  29. Luo, Q.; Zhou, Q.; Lin, Y.; Wu, S.; Liu, H.; Du, C.; Zhong, Y.; Yang, C. Fast and deep oxidative desulfurization of dibenzothiophene with catalysts of MoO3-TiO2@MCM-22 featuring adjustable Lewis and Bronsted acid sites. Catal. Sci. Technol. 2019, 9, 6166–6179. [Google Scholar] [CrossRef]
  30. Ghahramaninezhad, M.; Ahmadpour, A. A new simple protocol for the synthesis of nanohybrid catalyst for oxidative desulfurization of dibenzothiophene. Environ. Sci. Pollut. Res. 2020, 27, 4104–4114. [Google Scholar] [CrossRef] [PubMed]
  31. Yang, P.; Huang, Y.; Zhang, Z.; Li, N.; Fan, Y. Shape-controlled synthesis of the metal-organic framework MIL-125 towards a highly enhanced catalytic performance for the oxidative desulfurization of 4,6-dimethyldibenzothiophene. Dalton Trans. 2020, 49, 10052–10057. [Google Scholar] [CrossRef]
  32. Lu, S.; Zhong, H.; Mo, D.; Hu, Z.; Zhou, H.; Yao, Y. A H-titanate nanotube with superior oxidative desulfurization selectivity. Green Chem. 2017, 19, 1371–1377. [Google Scholar] [CrossRef]
  33. Bonino, F.; Damin, A.; Ricchiardi, G.; Ricci, M.; Spanò, G.; D’Aloisio, R.; Zecchina, A.; Lamberti, C.; Prestipino, C.; Bordiga, S. Ti-Peroxo Species in the TS-1/H2O2/H2O System. J. Phys. Chem. B 2004, 108, 3573–3583. [Google Scholar] [CrossRef]
Figure 1. The XRD patterns of the SiO2-RH, pure TiO2, and TS-RH-x samples (a), and the fresh and regenerated TS-RH-2.5 samples (b): (1) SiO2-RH, (2) TS-RH-0.5, (3) TS-RH-1.0, (4) TS-RH-2.5, (5) TS-RH-5.0, (6) TS-RH-10, (7) pure TiO2, (8) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (9) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 1. The XRD patterns of the SiO2-RH, pure TiO2, and TS-RH-x samples (a), and the fresh and regenerated TS-RH-2.5 samples (b): (1) SiO2-RH, (2) TS-RH-0.5, (3) TS-RH-1.0, (4) TS-RH-2.5, (5) TS-RH-5.0, (6) TS-RH-10, (7) pure TiO2, (8) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (9) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g001
Figure 2. UV-Vis spectra of the pure TiO2, and TS-RH-x samples (a), and the fresh and regenerated TS-RH-2.5 samples, and oxidation products of DBT and 4,6-DMDBT (b): (1) TS-RH-0.5, (2) TS-RH-1.0, (3) TS-RH-2.5, (4) TS-RH-5.0, (5) TS-RH-10, (6) pure TiO2, (7) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, (8) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT, (9) oxidation product of DBT, and (10) oxidation product of 4,6-DMDBT.
Figure 2. UV-Vis spectra of the pure TiO2, and TS-RH-x samples (a), and the fresh and regenerated TS-RH-2.5 samples, and oxidation products of DBT and 4,6-DMDBT (b): (1) TS-RH-0.5, (2) TS-RH-1.0, (3) TS-RH-2.5, (4) TS-RH-5.0, (5) TS-RH-10, (6) pure TiO2, (7) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, (8) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT, (9) oxidation product of DBT, and (10) oxidation product of 4,6-DMDBT.
Molecules 29 03856 g002
Figure 3. N2 adsorption–desorption isotherms (a,c) and pore size distribution curves (b,d) of the samples: (1) SiO2-RH, (2) TS-RH-0.5, (3) TS-RH-1.0, (4) TS-RH-2.5, (5) TS-RH-5.0, (6) TS-RH-10, (7) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (8) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 3. N2 adsorption–desorption isotherms (a,c) and pore size distribution curves (b,d) of the samples: (1) SiO2-RH, (2) TS-RH-0.5, (3) TS-RH-1.0, (4) TS-RH-2.5, (5) TS-RH-5.0, (6) TS-RH-10, (7) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (8) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g003aMolecules 29 03856 g003b
Figure 4. SEM images of the samples: (a) TiO2, (b) SiO2-RH, (c) TS-RH-2.5, (d) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (e) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 4. SEM images of the samples: (a) TiO2, (b) SiO2-RH, (c) TS-RH-2.5, (d) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (e) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g004
Figure 5. EDS elemental mappings of the samples: (a) TS-RH-2.5, (b) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (c) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 5. EDS elemental mappings of the samples: (a) TS-RH-2.5, (b) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (c) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g005aMolecules 29 03856 g005b
Figure 6. TEM images of the samples: (a) SiO2-RH, (b) TS-RH-2.5, (c) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (d) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 6. TEM images of the samples: (a) SiO2-RH, (b) TS-RH-2.5, (c) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (d) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g006
Figure 7. Particle size distribution histograms of the samples: (a) TS-RH-2.5, (b) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (c) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Figure 7. Particle size distribution histograms of the samples: (a) TS-RH-2.5, (b) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, and (c) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT.
Molecules 29 03856 g007
Figure 8. Effect of reaction time on the ODS of DBT and 4,6-DMDBT model oils catalyzed by the TS-RH-2.5 sample. Reaction conditions: model oils, 10 mL; catalyst to oil ratio, 10.0 g/L; TBHP/S molar ratio, 2.1; and temperature, 333 K.
Figure 8. Effect of reaction time on the ODS of DBT and 4,6-DMDBT model oils catalyzed by the TS-RH-2.5 sample. Reaction conditions: model oils, 10 mL; catalyst to oil ratio, 10.0 g/L; TBHP/S molar ratio, 2.1; and temperature, 333 K.
Molecules 29 03856 g008
Figure 9. FT-IR spectra of the reactants and their corresponding products: (a) DBT and its oxidation product and (b) 4,6-DMDBT and its oxidation product.
Figure 9. FT-IR spectra of the reactants and their corresponding products: (a) DBT and its oxidation product and (b) 4,6-DMDBT and its oxidation product.
Molecules 29 03856 g009
Figure 10. LC-MS spectra of the oxidation products of DBT (a) and 4,6-DMDBT (b).
Figure 10. LC-MS spectra of the oxidation products of DBT (a) and 4,6-DMDBT (b).
Molecules 29 03856 g010
Figure 11. Recycle tests for the ODS of DBT and 4,6-DMDBT model oils over the TS-RH-2.5c samples.
Figure 11. Recycle tests for the ODS of DBT and 4,6-DMDBT model oils over the TS-RH-2.5c samples.
Molecules 29 03856 g011
Figure 12. UV-Vis spectra of fresh TS-RH-2.5 and TS-RH-2.5c samples: (1) fresh TS-RH-2.5, (2) fresh TS-RH-2.5 treated with TBHP, (3) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, (4) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT and treated with TBHP, (5) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT, and (6) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT and treated with TBHP.
Figure 12. UV-Vis spectra of fresh TS-RH-2.5 and TS-RH-2.5c samples: (1) fresh TS-RH-2.5, (2) fresh TS-RH-2.5 treated with TBHP, (3) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT, (4) TS-RH-2.5c regenerated from the 15th ODS reaction of DBT and treated with TBHP, (5) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT, and (6) TS-RH-2.5c regenerated from the 15th ODS reaction of 4,6-DMDBT and treated with TBHP.
Molecules 29 03856 g012
Scheme 1. Schematic representation of the reaction mechanism and process flow for the oxidative removal of DBT and 4,6-DMDBT in the TS-RH-2.5 and TBHP catalytic system (R represents H or CH3).
Scheme 1. Schematic representation of the reaction mechanism and process flow for the oxidative removal of DBT and 4,6-DMDBT in the TS-RH-2.5 and TBHP catalytic system (R represents H or CH3).
Molecules 29 03856 sch001
Figure 13. The standard curves of DBT (a) and 4,6-DMDBT (b) model oils.
Figure 13. The standard curves of DBT (a) and 4,6-DMDBT (b) model oils.
Molecules 29 03856 g013
Figure 14. The absorption spectra of DBT (a) and 4,6-DMDBT (b) model oils before and after the ODS reaction catalyzed by the TS-RH-2.5 sample: (1) DBT model oil before the reaction diluted 2000 times, (2) DBT model oil after the reaction diluted 2000 times, (3), 4,6-DMDBT model oil before the reaction diluted 2000 times, and (4) 4,6-DMDBT model oil after the reaction diluted 2000 times.
Figure 14. The absorption spectra of DBT (a) and 4,6-DMDBT (b) model oils before and after the ODS reaction catalyzed by the TS-RH-2.5 sample: (1) DBT model oil before the reaction diluted 2000 times, (2) DBT model oil after the reaction diluted 2000 times, (3), 4,6-DMDBT model oil before the reaction diluted 2000 times, and (4) 4,6-DMDBT model oil after the reaction diluted 2000 times.
Molecules 29 03856 g014
Table 1. The pore structure parameters and catalytic performances of the samples.
Table 1. The pore structure parameters and catalytic performances of the samples.
SampleSBET (m2/g)Vmeso (cm3/g)XDBT (%)X4,6-DMDBT (%)
SiO2-RH294.40.3933.924.8
Pure TiO23.30.0132.322.6
TS-RH-0.5286.60.3897.798.1
TS-RH-1.0281.50.3898.898.7
TS-RH-2.5277.60.3899.899.7
TS-RH-5.0271.00.3799.799.8
TS-RH-10264.80.3799.899.8
TS-RH-2.5c a246.90.34--
TS-RH-2.5c b229.50.34--
Reaction conditions: model oils, 10 mL; catalyst to oil ratio, 10.0 g/L; TBHP/S molar ratio, 2.1; temperature, 333 K; reaction time, 2 h. a Regenerated from the 15th ODS reaction of DBT; b Regenerated from the 15th ODS reaction of 4,6-DMDBT.
Table 2. Comparison of the TS-RH-2.5 sample in the ODS of DBT and 4,6-DMDBT model oils with the reported similar catalysts.
Table 2. Comparison of the TS-RH-2.5 sample in the ODS of DBT and 4,6-DMDBT model oils with the reported similar catalysts.
SampleTemp. (K)S Content (ppm)Cyclic NumberXDBT a (%)X4,6-DMDBT a (%)Ref.
TS-0.23331000, 500 b599.099.8[14]
TS-503535002100.0[15]
TS-4/CM-β-CD298500399.0[16]
MT-1:4373500894.6[29]
TS-4298500398.0[30]
MIL-125-TRO333250392.3[31]
H-TiNTs3133204~98.0[32]
TS-RH-2.533310001599.899.7This work
a The catalytic results of the last cyclic reaction of DBT and 4,6-DMDBT, respectively; b The sulfur contents of DBT and 4,6-DMDBT model oils are 1000 and 500 ppmw, respectively.
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Share and Cite

MDPI and ACS Style

Liu, X.; Zhang, L.; Hu, J.; Zhang, W.; Xiang, X.; Cheng, H.; Qin, L.; Li, H. The Utilization of Rice Husk as Both the Silicon Source and Mesoporous Template for the Green Preparation of Mesoporous TiO2/SiO2 and Its Excellent Catalytic Performance in Oxidative Desulfurization. Molecules 2024, 29, 3856. https://doi.org/10.3390/molecules29163856

AMA Style

Liu X, Zhang L, Hu J, Zhang W, Xiang X, Cheng H, Qin L, Li H. The Utilization of Rice Husk as Both the Silicon Source and Mesoporous Template for the Green Preparation of Mesoporous TiO2/SiO2 and Its Excellent Catalytic Performance in Oxidative Desulfurization. Molecules. 2024; 29(16):3856. https://doi.org/10.3390/molecules29163856

Chicago/Turabian Style

Liu, Xiaoxue, Lanfen Zhang, Jian Hu, Wei Zhang, Xiaorong Xiang, Huiqing Cheng, Li Qin, and Hao Li. 2024. "The Utilization of Rice Husk as Both the Silicon Source and Mesoporous Template for the Green Preparation of Mesoporous TiO2/SiO2 and Its Excellent Catalytic Performance in Oxidative Desulfurization" Molecules 29, no. 16: 3856. https://doi.org/10.3390/molecules29163856

APA Style

Liu, X., Zhang, L., Hu, J., Zhang, W., Xiang, X., Cheng, H., Qin, L., & Li, H. (2024). The Utilization of Rice Husk as Both the Silicon Source and Mesoporous Template for the Green Preparation of Mesoporous TiO2/SiO2 and Its Excellent Catalytic Performance in Oxidative Desulfurization. Molecules, 29(16), 3856. https://doi.org/10.3390/molecules29163856

Article Metrics

Back to TopTop