Next Article in Journal
Mitigation of Membrane Wetting by Applying a Low Temperature Membrane Distillation
Next Article in Special Issue
Polymyxins and Bacterial Membranes: A Review of Antibacterial Activity and Mechanisms of Resistance
Previous Article in Journal / Special Issue
Experimental Design as a Tool for Optimizing and Predicting the Nanofiltration Performance by Treating Antibiotic-Containing Wastewater
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

WO3/Buckypaper Membranes for Advanced Oxidation Processes

by
Giovanni De Filpo
1,*,
Elvira Pantuso
2,
Aleksander I. Mashin
3,
Mariafrancesca Baratta
1 and
Fiore Pasquale Nicoletta
2,*
1
Department of Chemistry and Chemical Technologies, University of Calabria, 87036 Rende (CS), Italy
2
Department of Pharmacy, Health and Nutritional Sciences, University of Calabria, 87036 Rende (CS), Italy
3
Applied Physics & Microelectronics, Lobachevsky State University of Nizhni Novgorod, 603950 Nizhni Novgorod, Russia
*
Authors to whom correspondence should be addressed.
Membranes 2020, 10(7), 157; https://doi.org/10.3390/membranes10070157
Submission received: 6 June 2020 / Revised: 17 July 2020 / Accepted: 18 July 2020 / Published: 20 July 2020
(This article belongs to the Special Issue Membranes: 10th Anniversary)

Abstract

:
Photocatalytic materials, such as WO3, TiO2, and ZnO nanoparticles, are commonly linked onto porous polymer membranes for wastewater treatment, fouling mitigation and permeation enhancement. Buckypapers (BPs) are entanglements of carbon nanotubes, which have been recently proposed as innovative filtration systems thanks to their mechanical, electronic, and thermal properties. In this work, flexible membranes of single wall carbon nanotubes are prepared and characterized as efficient substrates to deposit by chemical vapor deposition thin layers of WO3 and obtain, in such a way, WO3/BP composite membranes for application in advanced oxidation processes. The photocatalytic efficiency of WO3/BP composite membranes is tested against model pollutants in a small continuous flow reactor and compared with the performance of an equivalent homogeneous WO3-based reactor.

Graphical Abstract

1. Introduction

Advanced oxidation processes, AOPs, allow the mineralization of organic pollutants by the generation of highly reactive hydroxyl radicals [1]. Photocatalytic reactions are particular AOPs, which are carried out when a catalyst is irradiated by a radiation of suitable wavelength [2].
Photocatalysis finds several interesting applications including selective organic reactions, pollutant degradation, photocatalytic surfaces (e.g., tiles, cements, paints, and asphalts), filters for air purification, water splitting in H2 and O2, water purification plants, CO2 reduction to energy fuels and bacterial disinfection [3,4,5,6,7,8]. Semiconductors are the most common used materials used in photocatalytic processes. Upon irradiation, electrons are promoted from the valence band to the conduction band, generating electron–hole pairs. Electrons and holes can move to the semiconductor surface and generate oxidizing species such as hydroxyl radicals (OH), superoxide anions (O2−●) and hydrogen peroxide molecules (H2O2), which are able to react with the present chemical species (dyes, pollutants, and other undesired molecules) and degrade them [9]. Several materials have photocatalytic properties (GaP, GaAs, CdSe, CdS, Fe2O3, TiO2, WO3, ZnO, SnO2, and CdS, just to mention a few), however not all of them are sufficiently efficient and stable over time to be used. In fact, GaP, GaAs, CdSe, CdS, or Fe2O3 are less stable in the air and degrade more easily. ZnO forms a passivating layer of Zn(OH)2 on its surface, which seriously compromises its photocatalytic properties [9]. Another important factor determining the choice of a semiconductor is its band-gap value, which must be as small as possible in order to allow the use of electromagnetic radiation with larger wavelengths. Titanium dioxide, TiO2, and tungsten trioxide, WO3, are low-cost semiconductor materials characterized by reduced toxicity towards environment and health and relatively low energy band-gaps (3.2 eV and 2.6 eV, respectively), which allow their activation with UV-Vis light (387 nm and 476 nm, respectively) [10].
Further problems for the use of semiconductors in the photocatalytic processes are:
  • The need of high surface area, which can be overcome by using nanometer sized materials; and
  • The semiconductor recovery after their use, which can be solved, for example, by nano-semiconductors with a magnetic core, by chemically cross-linked semiconductor nanoparticles onto polymer or ceramic membranes and, more recently, by vapor deposition of thin semiconductor films onto suitable substrates [11].
Thin film deposition methods can be distinguished in physical vapor deposition, PVD, and chemical vapor deposition, CVD, processes. In both methods, atoms or molecules in their vapor phase are carried onto the substrate surface and settle to form a thin layer [11].
Food, pharmaceutical, and, more in general, chemical plants need efficient separation and purification processes in order to guarantee an efficient treatment of their wastewaters. The removal of toxic pollutants from industrial wastewaters is a challenge due to the facts that they could not be effectively removed by filtration, adsorption, sedimentation, bio-oxidation, chlorination, coagulation, UV, and other classical treatments [12,13] and could represent potential threats to environment and health even at low concentrations (few ng L−1) as a consequence of their bio-accumulation [14,15].
Recently, polymer membranes have been suggested as simple and efficient materials to be used in water treatments including separation, purification, desalinization, recovery of critical raw materials and AOPs [16,17,18,19]. In fact, photocatalytic membranes, i.e., membranes with embedded or supported semiconductors by chemical binding, physical blending and vapor deposition, have been prepared in order to reduce/mitigate membrane fouling [20,21], enhance filtration fluxes [22], degrade wastewater pollutants, and remediate the concentrate [23]. Nevertheless, the binding of photocatalysts and polymer functionalization could need several chemical reactions and long cleaning processes, while the physical blending generally alter the mechanical properties of membranes and reduce the photocatalytic performance, as only the catalysts onto the membrane surface can play their photocatalytic activity.
In addition to their potential applications as TV screens, fire protection systems, heat dispersion in microelectronics, electrical-conductive tissue engineering, electromagnetic interferences shielding, electrodes for batteries and supercapacitors, buckypapers (BPs) have been proposed as innovative, high-temperature resistant and lightweight filtration systems. They consist of an entangled assembly of carbon nanotubes (CNTs) obtained by filtration of CNT dispersions through a polymer membrane [24,25]. According to such simple procedure, it is possible to get large-scale BP membranes that merge the mechanical, electronic, and thermal properties of CNTs with the flexibility, porosity, and transport properties of polymer membranes [26]. At a microscopic level, BPs show a highly disordered porous morphology due to π–π and van der Waals interactions between and within bundles of carbon nanotubes [27,28]. Consequently, BPs can result brittle. Such a problem and the risk of nanotubes release can be overcome enhancing the mechanical properties of BPs by polymer intercalation [29,30].
In this work, flexible membranes of single wall carbon nanotubes, SWNT, (or buckypaper, BP) were prepared and characterized as efficient substrates to deposit by CVD thin layers of WO3 and obtain, in such a way, WO3/BP composite membranes for application in advanced oxidation processes. The photocatalytic efficiency of WO3/BP composite membranes was tested against model pollutants (Methylene Blue, Indigo Carmine, and Diclofenac Sodium) in a small continuous flow reactor and compared with the performance of an equivalent homogeneous WO3-based reactor.

2. Materials and Methods

2.1. Preparation of BP Membranes

Buckypaper membranes were obtained by filtration of SWNT dispersions through PTFE disks (diameter = 47 mm, average pore size = 5 μm, Durapore©, Merck KGaA, Darmstadt, Germany). The average diameter of SWNTs was 1.4 ± 0.1 nm and their length was longer than 5 µm as reported in the datasheet from Sigma-Aldrich, Milan, Italy. Thirty milligrams of SWNTs were dispersed in 200 mL of a 0.4% TRITON X100 water solution by an ultrasonic bath (model M1800H-E, Bransonic, Danbury, CT, USA) for 30 min. Then, solutions were filtered through the PTFE disks with a vacuum pump (pressure = −0.04 bar), washed with 20 mL of methanol and, finally, dried at room temperature. All chemicals were purchased from Sigma-Aldrich, Milan, Italy.

2.2. Deposition of WO3 onto BP Membranes

The deposition of nanostructured tungsten trioxide onto BP membranes was obtained by reactive RF sputtering using of a tungsten target (purity 99.999%, Goodfellow Cambridge Ltd., Huntingdon, England) in the presence of oxygen (purity 99.999%) as process and reactive gas under different conditions of oxygen flow, sample-target distance, sputtering time, and applied RF process power. The optimal process conditions in term of layer homogeneity and catalyst droplet size were found to be: Oxygen flow 35 mL min−1, sample-target distance 8 cm, sputtering time 30 min, applied RF process power 50 W.
The amorphous WO3 thin films deposited on BP membranes were converted in monoclinic WO3 thin films, which are characterized by a larger catalytic activity, by heat treatment at 350 °C for 30 min.

2.3. Characterization of BP and WO3/BP Membranes

The porosity, P, of BP and WO3/BP membranes was determined by gravimetric method at 25 °C, measuring the weight of a wetting liquid (3M-FC-40, 3M Italia Srl, Pioltello, Milan, Italy), contained in the membrane pores. The porosity was calculated according to the following Equation (1):
P = w w w d d w w w w d d w + w d d m
where ww is the weight of the wet samples, wd the weight of dry samples, dw the wetting liquid density (1.855 g·cm−3), and dm is the average membrane density (0.60 ± 0.03 g·cm−3 as calculated from measurements of buckypaper weight, thickness, and surface area).
Pore size distribution was evaluated by a capillary flow porometer (CFP-1500 AEXL, PMI Porous Materials Inc., Ithaca, NY, USA). Membranes were fully wetted by keeping them in Porewick® (Sigma-Aldrich, Milan, Italy) for 24 h. Then, nitrogen was gradually allowed to flow into the membrane by increasing its pressure and the registration of gas pressure and permeation flow rate allowed the calculation of the pore size distribution.
The electrical conductivity of membranes was determined from the BP electrical resistance in I–V (current–voltage) measurements by a waveform generator (33220A Agilent, Santa Clara, CA, USA) and a digital multimeter (34410A Agilent, Santa Clara, CA, USA) on BP rectangular strips (width 5 mm and length 3 cm).
The mechanical properties were measured with a Sauter TVO-S tensile tester equipped with a Sauter FH-1k digital dynamometer and AFH FAST software (Sauter GmbH, Balingen, Germany). The rectangular strips (width 5 mm and length 3 cm) were tested at a strain rate of 0.1 mm·min−1. The tests allowed the determination of the tensile strength as the maximum stress, the fracture strain as the percentage of elongation at the breaking point, and the Young’s modulus.
Thermogravimetric analysis (TGA, STA 2500 Regulus simultaneous thermal analyzer, Netzsch, Selb, Germany) was employed to assess the BP membrane thermal stability. TGA was carried out from room temperature to 750 °C with a heating rate of 5 °C/min in a flowing gas mixture consisting of 1% O2 and 99% Ar at a flow rate of 100 sccm. The average roughness of WO3/BP surfaces was evaluated by atomic force microscopy (Nanoscope III, Digital Instruments, Santa Barbara, CA, USA). Static contact angle measurements of BP and WO3/BP membranes were measured with a goniometer (Nordtest, Serravalle Scrivia AL, Italy) at 25 °C. A drop (2 µL) of water was put onto the sample surface by a micro-syringe and measurements were carried out by setting the tangents on both visible edges of the droplet on five different positions of each sample and calculating the average value of the measurements.
The permeation tests were carried out with distilled water using a filtration cell having an active area of 5 cm2. The feed solution at 25 ± 1 °C was pumped by a gear pump at a transmembrane pressure of 1 bar. The feed flow rate was 250 mL·min−1. Permeate samples were collected every 5 min in order to determine the transmembrane flux, J, defined as:
J = V p A Δ t
where Vp was the permeate volume passed through the membrane in the fixed time interval, Δt, and A was the effective membrane area.

2.4. Photodegradation Experiments

The photoactivity of WO3/BP membranes was investigated in a small continuous plant with model pollutant water solutions (250 mL) of a cationic dye (Methylene Blue, MB, 5, 10, and 20 ppm), an anionic dye (Indigo Carmine, IC, 20 ppm) and a drug (Diclofenac Sodium, DS, 20 ppm), which were recirculated by a peristaltic system (flow rate 16.6 mL·min−1, Masterflex® L/S®, Cole-Parmer Srl, Cernusco sul Naviglio, MI, Italy) through a round cell. All model pollutants were purchased from Sigma-Aldrich, Milan, Italy. The experiment temperature was 25 ± 1 °C being the becker with the pollutant solutions placed in a thermostatic bath (model 1225, VWR, Milan, Italy), which kept constant the flowing solution temperature and avoided the pollutant thermolysis. All model pollutans were purchased from Sigma Aldrich, Milan, Italy. The WO3/BP membranes divided the cell volume in two compartments: The upper one (thickness 5 mm, photocatalytic area 8 cm2, irradiated volume 4 cm3) was equipped with a N-BK7 optical glass window to allow UV-Vis irradiation from a Suntest CPS+ sun simulator (1.5 kW Xenon arc lamp, with an average irradiance of 500 W·m−2 in the wavelength range 300 nm–800 nm, see Figure S1 of SI, Atlas, Linsengericht-Altenhaßlau, Germany). The light power of sun simulator was calibrated by a FieldMaxII-TO digital power/energy meter (Coherent Italia S.r.l., Monza, Italy) equipped with a PM10 thermopile. The WO3 sputtered surface of membranes was exposed to UV light. After irradiation, the solution passed through a quartz flow cuvette placed inside a spectrophotometer able to read at regular intervals (5 min) the absorbance value at the maximum absorption wavelength of MB (665 nm), IC (610 nm), and DS (275 nm). Similarly, the photoactivity of 0.2 mg of monoclinic WO3 nano-powder (which was the same amount of WO3 sputtered onto BP membranes) was measured. As each experiment generally lasted 150 min and the recirculation time was around 15 min, the average contact time of solutions with the active photocatalysis region was extimated in 10 min.
The photodegradation of pollutants [31] is generally described by the first-order kinetics
d C d t = k C
where C is the pollutant concentration, k is the rate constant and t is the reaction time. After integration, the following equation is obtained:
l n C ( t ) C 0 = k t
where C0 and C(t) are the initial concentration and the concentration at time t of the pollutants. The rate constant can be obtained from the slope of the plot of l n C ( t ) C 0 as a function of t.
Experimental data were corrected by taking into account the effective photon fluence impinging on WO3 layer (see SI).
The percentage of pollutant removal, %R, was calculated as:
% R = C 0 C ( t ) C 0 × 100

3. Results and Discussion

Several factors influence the BP membrane properties including sonication time of the SWNT solution, the magnitude of the vacuum depression used to filter the SWNT solution, the porosity and material of the filtration membranes. After several trials, which gave unacceptable results, including un-detachable BP from polymer membranes (due to small pore size filtration membrane), and brittle and broken BP (due to fast solvent evaporation), Figure 1a, intact BP were obtained under the optimal conditions reported in the Materials and Methods, Figure 1b. Such BPs are easily detachable from the filtration membranes, Figure 1c, and look like free-standing and flexible disks (average thickness 45 ± 2 μm) as shown in Figure 1d.
At a microscopic level, BP membranes showed a highly disordered porous morphology due to π–π and van der Waals interactions between and within bundles and clusters of carbon nanotubes, Figure 2a,b.
The thermal stability of BP membranes was assessed by TGA. As reported in Figure 2c, after an initial weight loss of about 5% due to water evaporation, BP membranes were found to be stable up to 400 °C. For larger temperatures, the degradation of SWNTs is observed.
Table 1 reports some geometrical data and properties for BP membranes. In particular, density, porosity, and water flow rate values of BPs (0.60 ± 0.03 g·cm−3, 70 ± 5%, and 12,500 ± 100 L·m−2·h−1·bar−1 respectively) fall in the range of values shown by porous polymer membranes, generally used for filtration processes [32]. In addition, the electrical conductivity and the mechanical properties, namely tensile strenght, fracture strain and Young’s modulus, reported in Table 1, allow to consider BPs as strong and conductive membranes [33].
In order to give photocatalytic properties to BP membranes, they were covered with thin layers of WO3 by RF magnetron chemical vapor deposition. CVD is a well-known chemical process for the deposition of desired thin films onto substrate surfaces by chemical reactions among one or more volatile precursors. Nevertheless, the film quality is strongly dependent on the CVD process parameters. Consequently, in this work different sputtering conditions (oxygen flow, sample-target distance, sputtering time, and power) were tested in order to find the optimal set of parameters able to give a homogeneous BP coverage without cracks and small WO3 nanoparticles to avoid BP membrane occlusion and increase photoactivity.
The best results, in terms of both coverage quality and nanoparticle size, were obtained with the following conditions: Flow(O2) = 35 mL·min−1, d = 8 cm, t = 30 min, power = 50 W. The WO3/BP membranes looked like flexible, greenish/yellowish disks as shown in Figure 3a.
Figure 3b shows the morphology of the top surface of a WO3/BP membrane sputtered under the experimental conditions previously reported. A homogeneous layer of small nanoparticles, with a rather spherical shape and an average diameter of around 50 nm, constitutes the WO3 coating without cracks and pore occlusion. It is important to remind the presence of BP membrane under the WO3 layer. Figure 3c shows the picture of a particular faulty WO3/BP membrane with a small crack, where it is possible to see inside the crack the texture of SWNT bundles, which form the BP substrate.
Figure 4a,b report the pore size distribution of both a pristine BP and a WO3/BP photocatalytic membrane and the SEM cross section picture of a WO3/BP membrane, respectively. As shown in Figure 4a both membranes show similar pore size distribution (within experimental errors) with two size populations placed at around 0.160 μm (0.163 ± 0.016 μm and 0.155 ± 0.018 μm, respectively) and at around 0.035 μm (0.037 ± 0.003 μm and 0.035 ± 0.003 μm, respectively) accounting for the presence of a major macroporous structure and a mesoporous structure (inter-tube pores with a size between 2 and 50 nm) formed between SWNT criss-crossings in the sample [34].
It is evident from the cross section of WO3/BP membrane, that the WO3 layer is a few tens of nanometers thick, but WO3 nanoparticles penetrate the BP membrane for ≈ 2 μm, accounting, most likely, for the reduction in the mesopore average size.
However, all the membranes prepared are characterized by a porosity of 70 ± 5%, which is expected to favour the water permeability through them.
The homogeneous covering of BP membranes WO3 was further assessed by EDX spectroscopy. Figure 5 shows the EDX color mapping images of the border area between a WO3/BP membrane (lower area) and a BP membrane (i.e., the part of sputtered BP membrane, which was covered by a locking mask, upper area). BP membrane area looks like a red homogeneous region due to the presence of carbon and chemical impurities from SWNT, on the contrary WO3/BP membrane area looks like a red background covered by yellow and green spots, deriving by the covering of SWNT with WO3 nanoparticles.
The WO3 layer showed an average rms roughness of 0.268 μm as determined by AFM measurements, Figure 6a. Such roughness gives a hydrophilic character to the top surface of WO3/BP membranes, as confirmed by contact-angle measurements. In fact, the average contact-angle value of WO3/BP membranes was found to be equal to 57.0° ± 0.5°, which is significantly smaller than the average contact-angle value (119.0° ± 0.5°) shown by a BP, Figure 6b,c. The contact angle values of the WO3/BP membranes did not change after 3 h continuous irradiation by solar simulator, confirming the stability of WO3 layer under UV-Vis light. The hydrophilicity of WO3/BP membranes could result in a possible increase of membrane fouling, i.e., the deposition of organic cakes onto the surfaces, but such possible drawback is overcome by fouling mitigation deriving from the photoactivity of WO3 layers. Moreover, the increase in hydrophilicity is expected to have a positive effect in the membrane permeation properties and makes such membranes suitable for the filtration of aqueous solutions.
It is well known that CVD deposition of tungsten trioxide onto substrates gives amorphous WO3, which is about ten times less photoactive than monoclinic WO3 [35]. Consequently, WO3/BP membranes were thermal treated at 350 °C in order to convert the amorphous WO3 layer into the more photoactive monoclinic one. Obviously, such treatment was possible thanks to the enhanced thermal properties of BP compared to polymer membranes.
Figure 7a shows the thermal evolution of micro-Raman spectrum of WO3/BP membranes. The Raman spectrum of as-deposited WO3 layer shows three main vibrational bands in the range of 200–1000 cm−1 observed at 265, 781, and 969 cm−1. The first peak increases in height as a function of the temperature, while the second splits into two intense peaks at around 700 and 800 cm−1. These peaks are the typical Raman peaks of monoclinic crystalline WO3, which correspond to the stretching vibrations of the bridging oxygen [36,37], and are assigned to WO stretching (ν), WO bending (δ), and OWO deformation (γ) modes, respectively [38,39].
The change of amorphous structure of WO3 to monoclinic WO3 was further confirmed by XRD as shown in Figure 7b, where the reported peaks are related to the reflection planes of the monoclinic phase of WO3.
The transmembrane flux WO3/BP membranes was evaluated in a small continuous plant and found to be 9.4 × 10+3 L m−2·h−1·bar−1, a value which is slightly lower (−25%) than pristine BP membrane as a consequence of the deposition of WO3 layer.
The photoactivity of WO3/BP membranes was tested with model pollutant water solutions (250 mL) of a cationic dye (Methylene Blue, MB, 5, 10, and 20 ppm), an anionic dye (Indigo Carmine, IC, 20 ppm) and a drug (Diclofenac Sodium, DS, 20 ppm), which were recirculated by a peristaltic system through a round cell.
The effect of initial concentrations of Methylene Blue (5, 10, and 20 ppm) on the reaction rate is shown in Figure 8. It is evident that the kinetic constant values decrease with increasing initial concentration (k values were 0.122 ± 0.003, 0.113 ± 0.003, and 0.085 ± 0.002 min−1, respectively). The higher values for the kinetic constant obtained at lower MB concentrations are explained as a consequence of [31,40]:
-
The increase of the number of photons available per BM molecule;
-
the higher amount of available catalytically active sites per BM molecule; and
-
an easier penetration of photons through the less concentrated solutions.
Nevertheless, the reported rate constants were corrected for the different photon fluence and their values do not differ so much from the uncorrected ones (0.118 ± 0.003, 0.110 ± 0.002 and 0.082 ± 0.002 min−1, respectively, see SI). Accordingly, the different photon absorption from Methylene Blue solutions at different concentrations is not the major cause for the observed differences in the rate constants for Methylene Blue degradation. Most probably, such differences could arise from the competition of MB molecules towards active surface sites and reactive oxygen species [41].
In all cases the percentage of MB removal within 35 min was larger than 90%. The residual concentration of MB was respectively 0.3, 0.7, and 1.5 ppm, values in agreement with other data present in literature [40]. Removal experiments with no irradiation found very low pollutant adsorption by WO3/BP membranes. After a 3 h run a WO3/BP membrane was able to adsorb about 0.003 mg of MB, which was not a significant quantity compared to the weight amount of MB present in the used solutions.
Figure 9 reports the photocatalytical properties of WO3/BP membranes against water solutions of a cationic dye (Methylene Blue 20 ppm), an anionic dye (Indigo Carmine 20 ppm) and a drug (Diclofenac Sodium 20 ppm), generally used as model pollutants. In all cases WO3/BP membranes are able to efficiently degrade the water contaminants with a kinetic constant value of 0.085 ± 0.002, 0.064 ± 0.001, and 0.019 ± 0.001 min−1, respectively. Such values are of the same order of magnitude or lower than the kinetic constants against the same pollutants, found with WO3, TiO2, or other catalyst nanoparticles dispersed either in the solutions or casted on carbon nanotubes, flakes of graphene oxide or porous polymer membranes [42,43,44,45,46,47,48,49,50], as no BP bearing photocatalysts, to the knowledge of authors, was ever proposed in literature.
Dark changes in absorbance were less than 1%, while UV controls for all three pollutant solutions found that after three hours of irradiation the absorbance changes due to the photolysis through a BP membrane were less than 2%. Such results can be explained by the particular spectrum of solar simulators (see Figure S1), which have only UV-A and UV-B emissions, and by the particular transmittance of N-BK7 optical glass cover, which cuts UV-B emissions with wavelengths lower than 300 nm. The absence of UV-C and lower UV-B wavelengths remarkably reduces the molecular degradation of pollutants by photolysis.
The performance of WO3/BP membranes was also compared with the photoactivity of 0.2 mg of monoclinic WO3 nano-powder (the same amount of WO3 sputtered onto BP membranes).
As shown in Figure 10, the photodegradation of Methylene Blue by both systems (WO3/BP membrane and monoclinic WO3 nano-powder) follows a first order kinetics with a rate constant of 0.085 ± 0.002 min−1 and 0.029 ± 0.001 min−1, respectively. The enhancement of the photoactivity in WO3/BP membranes can be due to the presence of BP, as the SWNT substrate prevents the electron/hole pair recombination during photocatalysis and increases the kinetic rate constant [51]. An almost complete photodegradation of Methylene Blue was obtained within ≈ 50 min and ≈ 140 min by using WO3/BP membranes and WO3 nano-powder, respectively. Such relatively short degradation times make the WO3/BP membranes suitable for applications in advanced oxidation processes. In addition, the long-term stability of WO3/BP membranes was checked by ten cycles of successive photocatalysis processes. Figure 10 shows the morphology and the photocatalycal efficiency of a WO3/BP membrane after the tenth photocatalytical cycle of a 20 ppm BM solution, revealing no evident damage in the morphology of WO3/BP membranes and no important change in the degradation efficiency, being the rate constant value equal to the pristine one within experimental errors (0.081 ± 0.002 min−1). In addition, the morphology of the WO3/BP membrane, after the tenth photocatalytical cycle, reveals the absence of any cakes on the surface and a morphology similar to that shown in the pristine WO3/BP membrane (Figure 3b), thanks to its photoactivity and different surface chemistry preventing and destroying any deposition. Further investigations are in progress to test the antifouling activity of WO3/BP membranes on real industrial wastes rather than on model dye and drug water solutions.

4. Conclusions

A new flexible membrane, based on SWNT and with improved thermal and catalytic properties, was obtained by RF magnetron sputtering of a nanostructured thin layer of tungsten trioxide and successive conversion in the more photoactive monoclinic phase. The WO3/BP membrane was characterized by SEM, TGA, porosimetry, XRD, EDX, AFM, Raman, contact angle and permeation measurements. The photocatalytic activity of WO3/BP membranes was tested following the degradation of three different pollutant water solutions in a small continuous plant confirming the beneficial contribution of the hydrophilic WO3 layer. The degradation kinetics rate of the Methylene Blue by WO3/BP membranes was about three times that found by an equivalent amount of WO3 nano-powder.
The main advantages of the proposed WO3/BP membranes can be summarized in:
  • The possibility to make heterogeneous photocatalytical processes with an easier catalyst recovery and reuse;
  • their application in continuous flow plants;
  • a simpler and cleaner synthetic approach. Chemical vapor deposition processes do not require long and expensive purification procedures, which are necessary in other chemical syntheses, such as solvo-thermal processes. In addition, CVD allows the catalyst amount saving, avoiding its dispersion in the substrate bulk;
  • a higher photocatalytical efficiency, due to the facilitated electron-transfer between carbon nanostrucutres and catalyst nanoparticles, a reduced recombination between electrons and holes [51], and the presence of catalyst nanoparticles with small size just only on the top surface of substrates rather than in the polymer bulk (where they cannot play any catalytic action);
  • the possibility to change the photocatalyst crystal structure in a more photoactive one by thermal annealing processes at temperatures higher than the melting point of commonly used polymer substrate. PTFE, polytetrafluoroethylene, which has one of the highest melting points, melts at 327 °C, a temperature lower than the WO3 amorphous-monoclinic phase transition temperature. On the contrary, BP membranes result thermally stable up to 400 °C;
  • BPs have both light weight and strong mechanical resistance, and, consequently, are easy to handle. In addition, BPs are resistant to all organic solvents and acid and base solutions, while porous polymer membranes can be damaged; and
  • a green chemisty approach with an almost zero environmental footprint, as the BP preparation is based on rather simple and clean experimental set-ups, which allow the recovery and reuse of solvents, CNT processing waste, end of life BPs and photocatalysts for the preparation of new catalyst/BP membranes.
The improved photoactivity, long-term stability, solvent-free features, fast catalyst recovery and re-use, and the possibility of an easy up-scale make WO3/BP membranes efficient devices for the pollutant degradation by advanced oxidation processes.

Supplementary Materials

The following are available online at https://www.mdpi.com/2077-0375/10/7/157/s1, Figure S1: Spectrum of Suntest CPS+ sun simulator for three different irradiance values. Reprinted from [S1], with permission from Royal Society of Chemistry, Figure S2: Normalized fluence across solutions of Methylene Blue, Indigo Carmine, and Diclofenac Sodium, Table S1: Fluence uncorrected and fluence corrected rate constants.

Author Contributions

Conceptualization, G.D.F., A.I.M. and F.P.N.; Methodology, G.D.F. and F.P.N.; Supervision, G.D.F.; Writing—review and editing, G.D.F., A.I.M. and F.P.N.; Project administration G.D.F. and F.P.N.; Data curation E.P. and M.B.; Investigation E.P. and M.B.; Formal analysis E.P. and M.B.; Validation, F.P.N. All authors have read and agreed to the published version of the manuscript.

Funding

This research was funded by MIUR, Italian Ministry for University and Research, grant number EX-60/2019.

Acknowledgments

The PhD of M.B. is funded by a scholarship from Regione Calabria (grant POR Calabria 2014-2020—Azioni 10.5.6 e 10.5.12).

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Ollis, D.F.; Pelizzetti, E.; Serpone, N. Photo-Catalysis Fundamentals and Applications; Wiley: Hoboken, NJ, USA, 1989. [Google Scholar]
  2. Araña, J.; Herrera Melián, J.A.; Doña Rodríguez, J.M.; González Díaz, O.; Viera, A.; Pérez Peña, J.; Marrero Sosa, P.M.; Jiménez, V.E. TiO2-photocatalysis as a tertiary treatment of naturally treated wastewater. Catal. Today 2002, 76, 279–289. [Google Scholar] [CrossRef]
  3. Di Gioia, M.L.; Leggio, A.; Le Pera, A.; Liguori, A.; Siciliano, C. Optically pure N-hydroxy-O-triisopropylsilyl-α-L-amino acid methyl esters from AlCl3-assisted ring opening of chiral oxaziridines by nitrogen containing nucleophiles. J. Org. Chem. 2005, 70, 10494–10501. [Google Scholar] [CrossRef] [PubMed]
  4. Cho, M.; Chung, H.; Choi, W.; Yoon, J. Linear correlation between inactivation of E. coli and OH radical concentration in TiO2 photocatalytic disinfection. Water Res. 2004, 38, 1069–1077. [Google Scholar] [CrossRef] [PubMed]
  5. De Filpo, G.; Palermo, A.M.; Tolmino, R.; Formoso, P.; Nicoletta, F.P. Gellan gum hybrid hydrogels for the cleaning of paper artworks contaminated with Aspergillus versicolor. Cellulose 2016, 23, 3265–3279. [Google Scholar] [CrossRef]
  6. Huang, Z.; Maness, P.-C.; Blake, D.; Wolfrum, E.J.; Smolinski, S.L.; Jacoby, W.A. Bactericidal mode of titanium dioxide photocatalysis. J. Photochem. Photobiol. A 2000, 130, 163–170. [Google Scholar] [CrossRef]
  7. De Filpo, G.; Palermo, A.M.; Munno, R.; Molinaro, L.; Formoso, P.; Nicoletta, F.P. Gellan gum/titanium dioxide nanoparticle hybrid hydrogels for the cleaning and disinfection of parchment. Int. Biodeterior. Biodegrad. 2015, 103, 51–58. [Google Scholar] [CrossRef]
  8. De Filpo, G.; Palermo, A.M.; Rachiele, F.; Nicoletta, F.P. Preventing fungal growth in wood by titanium dioxide nanoparticles. Int. Biodeterior. Biodegrad. 2013, 85, 217–222. [Google Scholar] [CrossRef]
  9. Hoffmann, M.R.; Martin, S.T.; Choi, W.Y.; Bahnemann, D.W. Environmental applications of semiconductor photo-catalysis. Chem. Rev. 1995, 95, 69–96. [Google Scholar] [CrossRef]
  10. Bhatkhande, D.S.; Pangarkar, V.G.; Beenackers, A. Photocatalytic degradation for environmental applications: A review. J. Chem. Technol. Biotechnol. 2002, 77, 102–116. [Google Scholar] [CrossRef]
  11. De Filpo, G.; Pantuso, E.; Armentano, K.; Formoso, P.; Di Profio, G.; Poerio, T.; Fontananova, E.; Meringolo, C.; Mashin, A.I.; Nicoletta, F.P. Chemical vapor deposition of photocatalyst nanoparticles on PVDF membranes for advanced oxidation processes. Membranes 2018, 8, 35. [Google Scholar] [CrossRef] [Green Version]
  12. Bhattacharyya, D. Functionalized membranes and environmental applications. Clean Technol. Environ. Policy 2007, 9, 81–83. [Google Scholar] [CrossRef]
  13. Drioli, E.; Ali, A.; Macedonio, F. Membrane distillation: Recent developments and perspectives. Desalination 2015, 356, 56–84. [Google Scholar] [CrossRef]
  14. Jones, O.A.H.; Voulvoulis, N.; Lester, J.N. Human pharmaceuticals in the aquatic environment: A review. Environ. Technol. 2001, 22, 1383–1394. [Google Scholar] [CrossRef] [PubMed]
  15. Ziylan, A.; Ince, N.H. The occurrence and fate of anti-inflammatory and analgesic pharmaceuticals in sewage and fresh water: Treatability by conventional and non-conventional processes. J. Hazard. Mater. 2011, 187, 24–36. [Google Scholar] [CrossRef] [PubMed]
  16. Formoso, P.; Pantuso, E.; De Filpo, G.; Nicoletta, F.P. Electro-conductive membranes for permeation enhancement and fouling mitigation: A short review. Membranes 2017, 7, 39. [Google Scholar] [CrossRef] [PubMed] [Green Version]
  17. Nicoletta, F.P.; Cupelli, D.; Formoso, P.; De Filpo, G.; Colella, V.; Gugliuzza, A. Light responsive polymer membranes: A review. Membranes 2012, 2, 134–197. [Google Scholar] [CrossRef] [Green Version]
  18. Salehi, S.M.; Di Profio, G.; Fontananova, E.; Nicoletta, F.P.; Curcio, E.; De Filpo, G. Membrane distillation by novel hydrogel composite membranes. J. Membr. Sci. 2016, 504, 220–229. [Google Scholar] [CrossRef]
  19. Salminen, J.; Garbarino, E.; Orveillon, G.; Saveyn, H.; Mateos Aquilino, V.; Llorens González, T.; García Polonio, F.; Horckmans, L.; D’Hugues, P.; Balomenos, E.; et al. Recovery of Critical and Other Raw Materials from Mining Waste and Landfills: State of Play on Existing Practices; EUR 29744 EN; Blengini, G.A., Mathieux, F., Mancini, L., Nyberg, M., Viegas, H.M., Eds.; Publications Office of the European Union: Luxembourg, 2019; ISBN 978-92-76-08568-3. [Google Scholar] [CrossRef]
  20. Shon, H.K.; Vigneswaran, S.; Ngo, H.H.; Kim, J.H. Chemical coupling of photocatalysis with flocculation and adsorption in the removal of organic matter. Water Res. 2005, 39, 2549–2558. [Google Scholar] [CrossRef]
  21. Mozia, S.; Morawski, A.W. Hybridization of photocatalysis and membrane distillation for purification of wastewater. Catal. Today 2006, 118, 181–188. [Google Scholar] [CrossRef]
  22. Ho, D.P.; Vigneswaran, S.; Ngo, H.H. Integration of photocatalysis and microfiltration in removing effluent organic matter from treated sewage effluent. Sep. Sci. Technol. 2010, 45, 155–162. [Google Scholar] [CrossRef]
  23. Mendez-Arriaga, F.; Esplugas, S.; Gimenez, J. Photocatalytic degradation of nonsteroidal anti-inflammatory drugs with TiO2 and simulated solar irradiation. Water Res. 2008, 42, 585–594. [Google Scholar] [CrossRef] [PubMed]
  24. Kim, Y.A.; Muramatsu, H.; Hayashi, T.; Endo, M.; Terrones, M.; Dresselhaus, M.S. Fabrication of high-purity, double-walled carbon nanotube buckypaper. Chem. Vap. Depos. 2006, 12, 327–330. [Google Scholar] [CrossRef]
  25. Endo, M.; Muramatsu, H.; Hayashi, T.; Kim, Y.A.; Terrones, M.; Dresselhaus, M.S. Nanotechnology: ‘buckypaper’ from coaxial nanotubes. Nature 2005, 433, 476. [Google Scholar] [CrossRef] [PubMed]
  26. Rashid, M.H.-O.; Ralph, S.F. Carbon nanotube membranes: Synthesis, properties, and future filtration applications. Nanomaterials 2017, 7, 99. [Google Scholar] [CrossRef] [Green Version]
  27. Frizzell, C.J.; Coutinho, D.H.; Balkus, K.J.; Minett, A.I.; Blau, W.J.; Coleman, J.N. Reinforcement of macroscopic carbon nanotube structures by polymer intercalation: The role of polymer molecular weight and chain conformation. Phys. Rev. B 2005, 72, 245420. [Google Scholar] [CrossRef] [Green Version]
  28. Vohrer, U.; Kolaric, I.; Haque, M.H.; Roth, S.; Detlaff-Weglikowska, U. Carbon nanotube sheets for the use as artificial muscles. Carbon 2004, 42, 1159–1164. [Google Scholar] [CrossRef]
  29. Coleman, J.N.; Blau, W.J.; Dalton, A.B.; Muñoz, E.; Collins, S.; Kim, B.G.; Razal, J.; Selvidge, M.; Vieiro, G.; Baughman, R.H.; et al. Improving the mechanical properties of single-walled carbon nanotube sheets by intercalation of polymeric adhesives. Appl. Phys. Lett. 2003, 82, 1682–1684. [Google Scholar] [CrossRef]
  30. Boge, J.; Sweetman, L.J.; Ralph, S.F. The effect of preparation conditions and biopolymer dispersants on the properties of SWNT buckypapers. J. Mater. Chem. A 2009, 19, 9131–9140. [Google Scholar] [CrossRef] [Green Version]
  31. Zhang, N.; Li, J.M.; Liu, G.G.; Chen, X.L.; Jiang, K. Photodegradation of diclofenac in aqueous solution by simulated sunlight irradiation: Kinetics, thermodynamics and pathways. Water. Sci. Technol. 2017, 75, 2163–2170. [Google Scholar] [CrossRef]
  32. Russo, F.; Ursino, C.; Avruscio, E.; Desiderio, G.; Perrone, A.; Santoro, S.; Galiano, F.; Figoli, A. Innovative Poly (Vinylidene Fluoride) (PVDF) electrospun nanofiber membrane preparation using DMSO as a low toxicity solvent. Membranes 2020, 10, 36. [Google Scholar] [CrossRef] [Green Version]
  33. Ashrafi, B.; Guan, J.; Mirjalili, V.; Hubert, P.; Simard, B.; Johnston, A. Correlation between Young’s modulus and impregnation quality of epoxy-impregnated SWCNT buckypaper. Compos. Part A 2010, 41, 1184–1191. [Google Scholar] [CrossRef] [Green Version]
  34. Whitby, R.L.D.; Fukuda, T.; Maekawa, T.; James, S.L.; Mikhalovsk, S.V. Geometric control and tuneable pore size distribution of buckypaper and buckydiscs. Carbon 2008, 46, 946–956. [Google Scholar] [CrossRef]
  35. Nandiyanto, A.B.-D.; Oktiani, R.; Ragadhita, R.; Sukmafitri, A.; Zaen, R. Amorphous content on the photocatalytic performance of micrometer-sized tungsten. Arab. J. Chem. 2020, 13, 2912–2924. [Google Scholar] [CrossRef]
  36. de Wijs, G.A.; de Groot, R.A. Amorphous WO3: A first principles approach. Electrochim. Acta 2001, 46, 1989–1993. [Google Scholar] [CrossRef]
  37. Tagtstrom, P.; Jansson, U. Chemical vapour deposition of epitaxial WO3 films. Thin Solid Film. 1999, 352, 107–113. [Google Scholar] [CrossRef]
  38. Daniel, M.F.; Desbat, B.; Lassegues, J.C.; Gerand, B.; Figlarz, M. Infrared and Raman study of WO3 tungsten trioxides and WO3, xH2O tungsten trioxide tydrates. J. Solid State Chem. 1987, 67, 235–247. [Google Scholar] [CrossRef]
  39. Díaz-Reyes, J.; Castillo-Ojeda, R.; Galván-Arellano, M.; Zaca-Moran, O. Characterization of WO3 thin films grown on silicon by HFMOD. Adv. Condens. Matter Phys. 2013, 2013. [Google Scholar] [CrossRef] [Green Version]
  40. Srinivasan, M.; White, T. Degradation of methylene blue by three-dimensionally ordered macroporous titania. Environ. Sci. Technol. 2007, 41, 4405–4409. [Google Scholar] [CrossRef]
  41. Wang, W.-Y.; Ku, Y. Photocatalytic degradation of Reactive Red 22 in aqueous solution by UV-LED radiation. Water Res. 2006, 40, 2249–2258. [Google Scholar] [CrossRef]
  42. Mastropietro, T.F.; Meringolo, C.; Poerio, T.; Scarpelli, F.; Godbert, N.; Di Profio, G.; Fontananova, E. Multistimuli activation of TiO2/α-alumina membranes for degradation of methylene blue. Ind. Eng. Chem. Res. 2017, 56, 11049–11057. [Google Scholar] [CrossRef]
  43. Gómez-Solís, C.; Juárez-Ramírez, I.; Moctezuma, E.; Torres-Martínez, L.M. Photodegradation of indigo carmine and methylene blue dyes in aqueous solution by SiC–TiO2 catalysts prepared by sol–gel. J. Hazard. Mater. 2012, 217–218, 194–199. [Google Scholar] [CrossRef] [PubMed]
  44. Devarahosahalli Veeranna, K.; Theeta Lakshamaiah, M.; Thimmasandra Naraya, R. Photocatalytic degradation of indigo carmine dye using calcium oxide. Int. J. Photochem. 2014, 2014. [Google Scholar] [CrossRef] [Green Version]
  45. Sampaio, M.J.; Silva, C.G.; Marques, R.R.N.; Silva, A.M.T.; Faria, J.L. Carbon nanotube–TiO2 thin films for photocatalytic applications. Catal. Today 2011, 161, 91–96. [Google Scholar] [CrossRef]
  46. Singh, J.; Chang, Y.-Y.; Koduru, J.R.; Yang, J.-K. Potential degradation of methylene blue (MB) by nano-metallic particles: A kinetic study and possible mechanism of MB degradation. Environ. Eng. Res. 2018, 23, 1–9. [Google Scholar] [CrossRef] [Green Version]
  47. Sampaio, M.J.; Marques, R.R.N.; Tavares, P.B.; Faria, J.L.; Silva, A.M.T.; Silva, C.G. Tailoring the properties of immobilized titanium dioxide/carbon nanotube composites for photocatalytic water treatment. J. Environ. Chem. Eng. 2013, 1, 945–953. [Google Scholar] [CrossRef]
  48. Zhou, X.; Shia, T.; Zhou, H. Hydrothermal preparation of ZnO-reduced graphene oxide hybrid with high performance in photocatalytic degradation. Appl. Surf. Sci. 2012, 258, 6204–6211. [Google Scholar] [CrossRef]
  49. Tian, L.; Ye, L.; Deng, K.; Zan, L. TiO2/carbon nanotube hybrid nanostructures: Solvothermal synthesis and their visible light photocatalytic activity. J. Solid State Chem. 2011, 184, 1465–1471. [Google Scholar] [CrossRef]
  50. Bojarska, M.; Nowak, B.; Skowroński, J.; Piątkiewicz, W.; Gradoń, L. Growth of ZnO nanowires on polypropylene membrane surface—Characterization and reactivity. Appl. Surf. Sci. 2017, 391, 457–467. [Google Scholar] [CrossRef]
  51. Jeevitha, G.; Abhinayaa, R.; Mangalaraj, D.; Ponpandian, N. Tungsten oxide-graphene oxide (WO3-GO) nanocomposite as an efficient photocatalyst, antibacterial and anticancer agent. J. Phys. Chem. Solids 2018, 116, 137–147. [Google Scholar] [CrossRef]
Figure 1. Appearance of buckypaper (BP) membranes under different experimental preparation procedures: (a) Brittle and un-detachable BP membrane filtered through a poly (vinylidene fluoride) (PVDF) membrane with reduced pore size; (b) whole and detachable; (c) free-standing and (d) flexible BP membrane obtained under the optimal conditions reported in the Experimental section.
Figure 1. Appearance of buckypaper (BP) membranes under different experimental preparation procedures: (a) Brittle and un-detachable BP membrane filtered through a poly (vinylidene fluoride) (PVDF) membrane with reduced pore size; (b) whole and detachable; (c) free-standing and (d) flexible BP membrane obtained under the optimal conditions reported in the Experimental section.
Membranes 10 00157 g001
Figure 2. (a,b) Morphology of BP membranes at two different magnification; (c) Thermal stability of BP membranes. The initial weight loss is due to solvent evaporation, while the second one, which starts at around 400 °C, is due to the thermal degradation of single wall carbon nanotubes (SWNTs).
Figure 2. (a,b) Morphology of BP membranes at two different magnification; (c) Thermal stability of BP membranes. The initial weight loss is due to solvent evaporation, while the second one, which starts at around 400 °C, is due to the thermal degradation of single wall carbon nanotubes (SWNTs).
Membranes 10 00157 g002
Figure 3. (a) Flexible, greenish/yellowish WO3/BP membranes; (b) Morphology of the top surface of a WO3/BP. The WO3 coating is a homogeneous layer of small nanoparticles, without cracks and pore occlusion; (c) Crack of a faulty WO3/BP membrane, inside which it is possible to see the texture of BP substrate.
Figure 3. (a) Flexible, greenish/yellowish WO3/BP membranes; (b) Morphology of the top surface of a WO3/BP. The WO3 coating is a homogeneous layer of small nanoparticles, without cracks and pore occlusion; (c) Crack of a faulty WO3/BP membrane, inside which it is possible to see the texture of BP substrate.
Membranes 10 00157 g003
Figure 4. (a) Pore size distribution of both a BP membrane (black dots) and a WO3/BP photocatalytic membrane (red dots); (b) SEM cross section picture of a WO3/BP membrane.
Figure 4. (a) Pore size distribution of both a BP membrane (black dots) and a WO3/BP photocatalytic membrane (red dots); (b) SEM cross section picture of a WO3/BP membrane.
Membranes 10 00157 g004
Figure 5. EDX color mapping image and EDX spectra of the border area between a WO3/BP membrane (lower area) and a BP membrane (upper area).
Figure 5. EDX color mapping image and EDX spectra of the border area between a WO3/BP membrane (lower area) and a BP membrane (upper area).
Membranes 10 00157 g005
Figure 6. (a) AFM topology image of a WO3/BP membrane. The average rms roughness is 0.268 μm; (b) Average contact-angle value of a BP membrane; (c) Average contact-angle value of a WO3/BP membrane.
Figure 6. (a) AFM topology image of a WO3/BP membrane. The average rms roughness is 0.268 μm; (b) Average contact-angle value of a BP membrane; (c) Average contact-angle value of a WO3/BP membrane.
Membranes 10 00157 g006
Figure 7. (a) Thermal evolution of Raman spectrum of WO3 deposited onto BP membranes. The peaks at around 700 and 800 cm−1 are assigned to WO stretching (ν), WO bending (δ), and OWO deformation (γ) modes, respectively, confirming the monoclinic structure of WO3; (b) X-ray diffraction patterns of WO3 layer sputtered onto BP membranes. Peaks are related to the reflection planes of the monoclinic phase of WO3.
Figure 7. (a) Thermal evolution of Raman spectrum of WO3 deposited onto BP membranes. The peaks at around 700 and 800 cm−1 are assigned to WO stretching (ν), WO bending (δ), and OWO deformation (γ) modes, respectively, confirming the monoclinic structure of WO3; (b) X-ray diffraction patterns of WO3 layer sputtered onto BP membranes. Peaks are related to the reflection planes of the monoclinic phase of WO3.
Membranes 10 00157 g007
Figure 8. Effect of initial concentrations of Methylene Blue (5, 10, and 20 ppm) on the reaction rate.
Figure 8. Effect of initial concentrations of Methylene Blue (5, 10, and 20 ppm) on the reaction rate.
Membranes 10 00157 g008
Figure 9. Photoactivity of WO3/BP membranes against water solutions of a cationic dye (Methylene Blue 20 ppm), an anionic dye (Indigo Carmine 20 ppm) and a drug (Diclofenac Sodium 20 ppm).
Figure 9. Photoactivity of WO3/BP membranes against water solutions of a cationic dye (Methylene Blue 20 ppm), an anionic dye (Indigo Carmine 20 ppm) and a drug (Diclofenac Sodium 20 ppm).
Membranes 10 00157 g009
Figure 10. Photodegradation of Methylene Blue by a WO3/BP membrane (red dots) and by monoclinic WO3 nanopowder (black dots) in the same amount of WO3 present on WO3/BP membrane.
Figure 10. Photodegradation of Methylene Blue by a WO3/BP membrane (red dots) and by monoclinic WO3 nanopowder (black dots) in the same amount of WO3 present on WO3/BP membrane.
Membranes 10 00157 g010
Table 1. Physical-chemical properties of BPs.
Table 1. Physical-chemical properties of BPs.
PropertyValue
Thickness45 ± 2 μm
Diameter37.0 ± 0.1 mm
Density0.60 ± 0.03 g·cm−3
Porosity70 ± 5 %
Electrical Conductivity83 ± 4 S cm−1
Tensile strength11.8 ± 2.2 MPa
Fracture Strain2.6 ± 0.1%
Young’s Modulus0.9 ± 0.1 GPa
Water Flow Rate12,500 ± 100 L m−2·h−1·bar−1

Share and Cite

MDPI and ACS Style

De Filpo, G.; Pantuso, E.; Mashin, A.I.; Baratta, M.; Nicoletta, F.P. WO3/Buckypaper Membranes for Advanced Oxidation Processes. Membranes 2020, 10, 157. https://doi.org/10.3390/membranes10070157

AMA Style

De Filpo G, Pantuso E, Mashin AI, Baratta M, Nicoletta FP. WO3/Buckypaper Membranes for Advanced Oxidation Processes. Membranes. 2020; 10(7):157. https://doi.org/10.3390/membranes10070157

Chicago/Turabian Style

De Filpo, Giovanni, Elvira Pantuso, Aleksander I. Mashin, Mariafrancesca Baratta, and Fiore Pasquale Nicoletta. 2020. "WO3/Buckypaper Membranes for Advanced Oxidation Processes" Membranes 10, no. 7: 157. https://doi.org/10.3390/membranes10070157

APA Style

De Filpo, G., Pantuso, E., Mashin, A. I., Baratta, M., & Nicoletta, F. P. (2020). WO3/Buckypaper Membranes for Advanced Oxidation Processes. Membranes, 10(7), 157. https://doi.org/10.3390/membranes10070157

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop