Next Article in Journal
Gold in the Farallones Block of the Shale-Hosted, Clastic-Dominated Castellanos Zinc-Lead Deposit (Northwest Cuba)
Next Article in Special Issue
Fe(III)–Chitosan Microbeads for Adsorptive Removal of Cr(VI) and Phosphate Ions
Previous Article in Journal
Metasediments Covering Ophiolites in the HP Internal Belt of the Western Alps: Review of Tectono-Stratigraphic Successions and Constraints for the Alpine Evolution
Previous Article in Special Issue
Synthesis and Application of FeCu Bimetallic Nanoparticles in Coal Mine Wastewater Treatment
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Laboratory Study on the Effectiveness of Limestone and Cementitious Industrial Products for Acid Mine Drainage Remediation

by
Abdellatif Elghali
1,2,*,
Mostafa Benzaazoua
2,3,*,
Hassan Bouzahzah
2,4 and
Bruno Bussière
2
1
Geology and Sustainable Mining Department, Mohammed VI Polytechnic University, Lot 660. Hay Moulay Rachid, 43150 Ben Guerir, Morocco
2
Research Institute on Mines and Environment, University of Québec in Abitibi-Témiscamingue, 445 boul. de l’Université, Rouyn-Noranda, QC J9X 5E4, Canada
3
Mining Environment and Circular Economy, Mohammed VI Polytechnic University, Lot 660. Hay Moulay Rachid, 43150 Ben Guerir, Morocco
4
Génie Minéral, Matériaux et Environnement, Université de Liège, Allée de la découverte, 13/A. Bât. B52/3 Sart-Tilman, 4000 Liège, Belgium
*
Authors to whom correspondence should be addressed.
Minerals 2021, 11(4), 413; https://doi.org/10.3390/min11040413
Submission received: 22 March 2021 / Revised: 8 April 2021 / Accepted: 10 April 2021 / Published: 14 April 2021

Abstract

:
Acid mine tailings may affect several environmental matrices. Here, we aimed to stabilize acid-generated mine tailings using several alkaline and cementitious amendments, which were tested in columns for 361 days. The alkaline amendments consisted of 10 and 20 wt.% limestone, while the cementitious amendments consisted of different binders at a total dosage of 5 wt.% binder. The different formulations for the cementitious amendments were: 50% Kruger fly ash and 50% class F fly ash; 20% ordinary Portland cement, 40% Kruger fly ash, and 40% class F fly ash; 80% ordinary Portland cement and 20% Kruger fly ash; and 20% ordinary Portland cement, 40% Kruger fly ash, and 40% fly ash. Kinetic testing on the amendment formulations showed that the pH values increased from <2.5 to circumneutral values (~7.5). The mobility of various chemical species was greatly reduced. Cumulative Fe released from the unamended tailings was ~342.5 mg/kg, and was <22 mg/kg for the amended tailings. The main mechanisms responsible for metal(loid) immobilization were the precipitation of secondary phases, such as Fe-oxyhydroxides, physical trapping, and tailing impermeabilization.

Graphical Abstract

1. Introduction

Mining activities generate large quantities of solid wastes such as waste rocks and tailings. Tailings are generated after ore treatment and processing, and are characterized by fine grain-size distributions and high specific surface areas [1,2,3]. The majority of tailings are stored at the surface in a tailing storage facility (TSF). Mine tailings often contain non-negligible amounts of iron sulfide minerals such as pyrite and pyrrhotite [4,5,6]. The oxidation of sulfide minerals occurs when they are exposed to water and oxygen, both in the presence or absence of microorganisms [5]. Sulfide oxidation can involve various and complex processes, including chemical, biological, and electrochemical reactions [7]. Sulfide oxidation increases the acidity of leachate waters, which can lead to the formation of acid mine drainage (AMD). The overall reaction of pyrite oxidation result produces four moles of H+ (Equation (1)).
FeS2 + 3.75O2 + 3.5H2O → Fe(OH)3 + 2 SO42− + 4H+
Consequently, various metals and metalloids (e.g., As, Cd), iron, and sulfate could be released into the environment due to sulfide oxidation [8]. The mobility of metals is mainly influenced by pH conditions [9]. Depending on the mineralogical composition of tailings, acid production by sulfide oxidation can be partially neutralized by carbonate, hydroxide, and, to a lesser extent, silicate dissolution [10,11,12,13]. An example of acid buffering by calcite dissolution under acidic conditions (pH < 6.3) is illustrated in Equation (2):
CaCO3(s) + 2H+ → H2CO3(aq) + Ca2+
Contamination of the environment caused by acid-generating tailings represents a serious global issue for the mining industry. Consequently, numerous techniques have been developed to prevent and mitigate AMD [14]. Stabilization/solidification (S/S) using cementitious and alkaline amendments is one method that was successfully used in various case studies related to contaminated geological materials, such as: (i) acid-generating tailings [15,16,17,18,19,20,21,22,23,24,25,26], (ii) contaminated soils and sediments [27,28,29,30,31,32,33,34,35,36,37,38,39], and (iii) mine backfills [4,40,41,42,43,44]. Various cementitious and alkaline materials were used as amendments to stabilize contaminated materials. The most used materials in the stabilization/solidification of hazardous wastes are presented in Table 1. Within alkaline amendments, limestone is one of the most used materials to neutralize and stabilize acid-generating materials. However, there are no specific formulations for either alkaline or cementitious amendments due to the wide range of geochemical and mineralogical properties of mine tailings. In the category of cementitious amendments, ordinary Portland cement (OPC) in combination with pozzolanic and industrial byproducts is widely used. Moreover, numerous studies were conducted to substitute OPC by industrial byproducts to reduce costs related to cement (Table 1).
Alkaline amendments consist of added materials with a high neutralization potential (NP) to buffer the acidity produced by tailing oxidation [15,22,45]. The main objective of alkaline amendments is to take tailings with a high acid-generating potential (AP) and add NP until the material is no longer acid-generating. When alkaline materials dissolve under acidic conditions, they provide alkalinity and neutralize acidity [46]. Consequently, contaminants such as arsenic (As), lead (Pb), iron (Fe), zinc (Zn), and copper (Cu) can be immobilized through mechanisms such as: (i) precipitation of low-solubility secondary phases like iron oxyhydroxides, (ii) coprecipitation of contaminants or their adsorption onto newly formed secondary phases, and (iii) reduction of sulfide oxidation under circumneutral conditions and their passivation.
Cementitious amendments consist of added cementitious materials to increase tailing cohesion and mechanical resistance. They are commonly used for the treatment of hazardous contaminated materials before their disposal. Cementitious additives reduce the hydraulic conductivity, porosity, and available surface area of the mixture. Consequently, many inorganic contaminants can be immobilized into the solidified matrix through a number of physical and chemical mechanisms [15,23,27,35,47]. Contaminant immobilization with cementitious amendments is ensured through the following processes: (i) the same chemical mechanisms as alkaline amendments; (ii) a reduction of the available surface area of the tailings, which decreases their reactivity; (iii) a physical encapsulation of contaminants due to the tailings’ cementation; and (iv) a reduction of the contact between water and the tailings.
The main objective of this study was to stabilize highly oxidized acid-generating tailings from a closed mine site located in Quebec Canada. The effectiveness of alkaline and cementitious amendments was studied based on laboratory column tests. Limestone was used as an alkaline material, while ordinary Portland cement, fly ash (FA), Kruger fly ash (KFA), and class F fly ash (FAF) were used in various combinations as cementitious amendments. The effectiveness of the used amendments was tested in a laboratory column for 361 days. The geochemical behavior of each amendment’s formulation was compared to that of oxidized tailings. Consequently, the reduction factor of each chemical element was calculated. At the end of column tests, the reduction of hydraulic conductivity was evaluated using infiltration tests. At the local scale, this technology studied in this paper can be used as an option for the mitigation of the studied mine site. Moreover, this technique can be easily used for other problematic mine tailings in other countries.

2. Materials and Methods

2.1. Materials and Study Site

The tailings used in this study were collected from the Joutel mine site, which is an inactive mine site located in Quebec, Canada. During operation, the Joutel mine extracted gold via floatation and cyanidation [57], with the waste tailings from this process being deposited in a 120 ha TSF. Operations at Joutel ended in 1994, which has allowed for significant oxidation and acid generation to occur in some localized areas of the TSF [58]. The tailings used in this study were collected from an acidic oxidized zone in the TSF. The samples were homogenized in situ and shipped to the laboratory.
The materials used as amendments in this study were limestone (LS); fly ash (FA) that was collected from the Boralex thermal energy station in Sennterre, Quebec; ordinary Portland cement (OPC); Kruger fly ash (CVK) that was collected from the biomass cogeneration power plant at the Kruger paper mill in Brompton, Quebec; and class F fly ash (FAF), which was provided by LafargeHolcim Canada. Limestone was formed mainly by calcite and dolomite [15]; fly ash was mainly composed of plagioclases and carbonates [15]; FAF contained mainly quartz [59], plagioclase, and mullite; and CVK was composed of lime, gehlenite, quartz, and calcite.

2.2. Physical, Chemical, and Mineralogical Material Characterizations

The grain-size distribution (GSD) of all samples was analyzed using a laser analyzer (Malvern Mastersizer, Malvern Panalytical, Rouyn-Noranda, Quebec, Canada). The chemical composition of the solid samples was evaluated using inductively coupled plasma atomic emission spectroscopy (ICP-AES) (Perkin Elmer Optima 3100 RL, USA) following complete digestion by HNO3/Br2/HF/HCl (HF and HCL to dissolve silicates; HNO3 and Br2 to oxidize sulfur). The ICP-AES was calibrated using an international standard (SY-4). The detection limits of ICP-AES are variable and depend on the analyzed element (60 ppm for Al and Ca, 15 ppm for Mg, 5 ppm for Mn, 1 ppm for Na and K, 10 ppm for Fe, 5 ppm for Li, Pb, As and Cr, 10 ppm for Cu and 55 ppm for Zn). Total carbon and sulfur were analyzed in pulverized samples to <74 µm via infrared spectroscopy following combustion in an induction furnace (ELTRA CS-2000; detection limit = 0.09%). During sulfur and carbon (S/C) analysis, blank samples consisted of samples containing only iron and tungsten. Calibration of the induction furnace was done using four standards: low carbon standard ([C] = 0.5 wt.%), high carbon standard ([C] = 11.97 wt.%), low sulfur standard ([S] = 0.28 wt.%), and high sulfur standard ([S] = 18.03 wt.%).
The mineralogical composition of tailings was investigated thoroughly using mineral-liberation analysis (MLA). MLA is technique based on scanning electron microscopy with an energy dispersive spectrometer (SEM-EDS) that uses special software to automate mineral abundance quantification [60]. This technique also enables quantitative analyses of mineral liberation, mineral association, and elemental deportment. In this study, MLA was used to quantify modal mineralogy; calcite and pyrite liberation; and Ca, Mg, Fe, and S deportments.

2.3. Toxicity Characteristic Leaching Procedure and Kinetic Column Tests

Toxicity characteristic leaching procedure (TCLP) was used as preliminary test to evaluate metal(loid) mobility within the different amendment formulations (Table 2). TCLP was primarily designed to simulate the release of heavy metal(loid)s and organics from municipal wastes [61], but is frequently used on mine tailings. In brief, around 20 g of each sample was added to 400 mL of a leaching solution composed of acetic acid [62]. Each mixture was then placed in a high-density polyethylene (HDPE) bottle, and the bottles were tumbled for 18 h at a 30 ± 2 rpm. Samples were filtered through a 0.45 µm nylon filter, and the leachates were analyzed for their pH, electrical conductivity (EC), and chemical composition (by ICP-AES).
Kinetic column tests (KCTs) are widely used to predict the environmental behavior of mine tailings, as well as to test different reclamation scenarios for acid-generating tailings [63]. Column tests are recognized as reproducible tests [64], and under the right conditions, they may be able to provide insight into the environmental behavior of wastes under field conditions. The column tests were monitored for more than 365 days. The long-term geochemical monitoring of columns presents several advantages, such as: (i) considering the possible dynamic changes, (ii) using a large quantity of sample (around 10 kg in this study), and (iii) allowing possible precipitation reactions. Seven amendment formulations were selected based on laboratory batch tests and tested in KCTs as indicated in Table 2. Each sample was placed in an acrylic column with a diameter of 14 cm and a height of 100 cm. Each column’s inner wall was covered with grease to avoid the creation of preferential flow paths during the flushing of the samples [65]. Column C1 contained a reference sample of pure mine tailings. Columns C2 and C3 contained alkaline amendments based on the LS addition.
The limestone dosage was about 20 wt.% for C2 and 10 wt.% for C3. All the cementitious amendments were added to mine tailings at a total dosage of 5 wt.%. Column C4 contained 50%FAF-50%CVK, C5 contained 20%OPC-40%CVK-40%FAF, C6 contained 80%OPC-20%CVK, and C7 contained 20%OPC-40%CVK-40%FA.
The leachates from each column were analyzed for pH and EC using individual probes, while the acidity and alkalinity were analyzed using an automated titrator (Metrohm Binkmann, 716 DMS Trinitro, Rouyn-Noranda, Canada). The chemical composition of the leachates was determined by ICP-AES for samples filtered to 0.45 µm and acidified to 2% v/v HNO3. The chemical quality of the leachates from the column tests was integrated in Visual Minteq (Version 3.1) to calculate the saturation indexes of the ferrihydrite and goethite [66]. Saturation indexes were calculated using the standard database of Visual Minteq.

3. Results and Discussion

3.1. Physical and Chemical Characteristics

The GSDs and chemical characteristics of the studied samples are presented in Table 3. Grain-size distributions were relatively heterogeneous. The D90 values, which correspond to the diameter at which 90% of particles pass on the cumulative grain-size distribution curve, were about 30.4, 4500, 46.7, 1500, 104.2, and 89.1 µm for the mine tailings, LS, OPC, FA, CVK, and FAF, respectively. The mine tailings had a similar GSD to that of the OPC.
Chemical compositions of the bulk samples are shown in Table 3. The aluminum content was about 1.73, 0.30, 2.75, 4.69, 3.84, and 11.91 wt.% for the mine tailings, LS, OPC, FA, CVK, and FAF, respectively. Calcium concentrations were between 2.87 wt.% for the FAF and 49.07 wt.% for the OPC. Magnesium concentrations were below 2.5 wt.%, with the highest concentration of about 2.35 wt.% found within the LS sample. Iron concentrations were about 19.30 wt.% and 13.43 wt.% for the mine tailings and FAF, respectively, and <3.5 wt.% for all other samples. Total S contents were <4.5 wt.% for all samples. Concentrations of other species, including K, Na, Mn, Li, Pb, Cr, Cu, and Zn, are presented in Table 3.

3.2. Mineralogical Composition of the Mine Tailings

The mineralogical composition of the highly oxidized mine tailings was investigated using mineral-liberation analysis. The tailings’ modal mineralogy and mineral-liberation degrees are presented in Figure 1. The tailings sample contained approximately 31 wt.% of secondary iron oxides, 20 wt.% of quartz, 16 wt.% of albite, 11 wt.% of chlorite, and 9 wt.% of gypsum. Secondary iron oxides were present as a cementitious material that coated various minerals, especially pyrite and silicates (Figure 2A–D). Other minerals were detected in varying concentrations, such as pyrite, chalcopyrite, and calcite. The pyrite content was about 0.44 wt.%, despite a total S content of about 4.36 wt.%. This suggests that a major part of pyrite was oxidized in situ and that the resulting sulfate precipitated as gypsum. As a result of sulfide oxidation, carbonates dissolved to buffer the produced acidity. Thus, residual calcite was present in trace amounts of about 0.19 wt.%. Comparing the sulfide content with the carbonate content allows prediction of the acid-generating behavior for the mine tailings, since it is recognized that the balance between acid-forming and acid-consuming minerals can inform on the environmental behavior of mine tailings (acid-generating or not) [13,67,68]. However, the reactivity of these minerals is influenced by several parameters, such as their available reactive surface area [69,70,71,72,73]. Therefore, the degree of liberation for calcite and pyrite was analyzed by MLA, as shown in Figure 1B. The degrees of liberation for calcite and pyrite were only slightly different. Free (liberation degree = 100%) calcite and pyrite represented around 47.6 and 55.5% of the total calcite and pyrite, respectively, which meant that the completely available reactive surface of pyrite was slightly higher than that of calcite. The locked part of calcite and pyrite was about 23 and 20%, respectively. Around 7.5% of calcite and pyrite were mid-liberated (between 20 and 70%).
Calcium, iron, magnesium, and sulfur deportments within the tailings sample are presented in Figure 3. The mineralogical composition of the studied sample showed Ca mainly occurring in three minerals: calcite [CaCO3]—3%, gypsum [CaSO4.2(H2O)]—81%, and actinolite [Ca2(Mg,Fe++)5Si8O22(OH)2]—15.5%. Iron occurred mostly in iron oxides, followed by chlorite, actinolite, and pyrite. Around 84% of iron was present in iron oxides, 11% came from chlorite, and small amounts of iron were associated with actinolite and pyrite (<2%). Magnesium mainly occurred in chlorite and actinolite; 74% of magnesium came from chlorite, and 26% came from actinolite. Sulfur was mainly associated with gypsum and pyrite; 87.5% of S came from gypsum, and 12% of S came from pyrite. Small amounts of S were also associated with chalcopyrite (<0.2%).

3.3. Comparison of the Geochemical Behavior of Unamended and Amended Tailings

3.3.1. Results of Toxicity Characteristic Leaching Procedure

Table 4 presents results of TCLP tests that were carried out to evaluate metal(loid) mobility following different amendment treatments. The performance of each amendment formulation was slightly different. Both alkaline (C2 and C3) and cementitious formulations (C3, C4, C5, C6, and C7) increased the pH of the leachates compared to the unamended tailings, indicating the dissolution of alkaline phases that buffered the produced acid. The pH of the leachates from the unamended tailings was about 2.5, while pH values of that from amended tailings ranged from 4.92 for C6 (80%OPC-20%CVK) to 6.46 for C2 (20 wt.% LS). The analyzed EC was similar for all samples, ranging between 7.81 mS/cm for C1 and 9.37 mS/cm for C2.
The application of the different amendment formulations reduced Al, Fe, Ni, and Zn releases compared to the unamended tailings. Aluminum release from the unamended tailings was about 0.4 mg/L, but did not exceed 0.05 mg/L in any of the amended tailings. Iron releases were reduced from 0.5 mg/L from the unamended tailings to a maximum of 0.08 mg/L from C6. Nickel releases were around 0.01 mg/L for the unamended tailings and less than the detection limit of the analytical method for all amended tailings. Zinc concentrations were about 0.6, 0.34, 0.33, 0.30, 0.60, 0.31, and 0.30 for C1, C2, C3, C4, C5, C6, and C7, respectively. Finally, S releases were between a minimum value of 567 mg/L from C2 to a maximum value of 766 mg/L from the unamended tailings.

3.3.2. Kinetic Column Tests

The water quality of leachates from the KCTs are presented in Figure 4, Figure 5, and Figure 6. The evolution of pH in the leachates from the KCTs (Figure 4A) varied widely among the tested samples. The mine tailings showed an acidic behavior characterized by pH values ranging between 2.1 and 2.8. Thus, there was a relatively small variation in pH values from the beginning to the end of the tests. However, the amended formulations raised pH values to circumneutral values. Average pH values were about 7.7, 7.2, 7.7, 7.4, 7.7, and 7.5 for C2, C3, C4, C5, C6, and C7, respectively, and these values were stable throughout the duration of the KCTs. Average EC values (Figure 4B) were about 4.2, 4.24, 4.93, 5.7, 6.8, 5.3, and 5.2 mS/cm for C1, C2, C3, C4, C5, C6, and C7, respectively. At the beginning of the leaching tests, EC values were notably higher than at the end of the tests. This is likely due to the redissolution and release of secondary mineral phases that are naturally present in preoxidized tailings. Acidity and alkalinity values were in stark contrast between the amended and unamended materials (Figure 4C,D). Acidity in leachates from unamended tailings started at around 1400 mg CaCO3/L, then stabilized at around 300 mg CaCO3/L. However, average acidity values in the amended tailings were 23, 60, 33, 45, 31, and 42 mg CaCO3/L for C2, C3, C4, C5, C6, and C7, respectively. The results for acidity were mirrored by the results for alkalinity (Figure 4D). Leachates from the unamended tailings (C1) showed negligible alkalinity values. The amended tailings showed leachates with non-negligible values. Average alkalinity values were about 144, 141, 359, 232, 307, and 264 mg CaCO3/L for C2, C3, C4, C5, C6, and C7, respectively. In general, the cement-based amendments showed higher alkalinity values compared to the limestone-based amendments.
Concentrations of the chemical species in Figure 5 and Figure 6 are presented as cumulative, mass-normalized releases (mg/kg) to avoid effects due to leachate volumes and the samples’ initial weights. Calcium, magnesium, and manganese were chosen to indicate dissolution of neutralizing minerals [74], and aluminum was chosen to indicate aluminosilicate dissolution [74]. Calcium releases (Figure 5A) were variable among the KCTs. The unamended tailings released higher concentrations of Ca compared to the amended tailings. Over 361 days, cumulative Ca release was about 2203, 713, 664, 849, 750, 937, and 969 mg/kg for C1, C2, C3, C4, C5, C6, and C7, respectively. Magnesium release was the lowest for the unamended tailings (~105.5 mg/kg). In contrast, Mg release was about 699, 972, 1634, 1588, 1524, and 1456 mg/kg for C2, C3, C4, C5, C6, and C7, respectively. Manganese releases were similar in all columns, being about 41, 97, 85, 24, 167, 29, and 70 mg/kg for C1, C2, C3, C4, C5, C5 and C7, respectively. Aluminum releases were negligible for the amended tailings, not exceeding 0.5 mg/kg. However, for the unamended tailings, Al release was about 98 mg/kg.
Iron (Figure 6A) was released more from the unamended tailings compared to the amended tailings. Iron release was about 342.5, 0.2, 22.2, 0.4, 3.9, 0.3, and 0.3 mg/kg for C1, C2, C3, C4, C5, C6, and C7, respectively. In general, Fe release is greatly influenced by pH/Eh conditions. Under circumneutral conditions, Fe precipitates as Fe-oxyhydroxides, thus explaining the low Fe concentrations observed in leachates from the amended tailings [75]. Sulfur was the most released element (Figure 6B). Cumulative S concentrations were about 3022, 1511, 1912, 2915, 2981, 2721, and 2616 mg/kg for C1, C2, C3, C4, C5, C6, and C7, respectively. Copper and zinc concentrations were negligible for the amended tailings, suggesting that they were largely immobile under these conditions (Figure 6C,D). Copper and zinc releases from the unamended tailings were about 81 and 44.50 mg/kg, respectively.
At the end of the KCTs, water-infiltration speed was measured for the different column tests. The main objective was to compare the hydraulic conductivity reduction of the different formulations. The results from the water-infiltration tests are presented in Figure 7. Samples C1, C2, and C3 drained water more quickly than the other samples. At 4000 min, about 68 mL was drained from C1, 69 mL was drained from C2, and 60 mL was drained from C3. In contrast, 30 mL was drained from C4, 49 mL was drained from C5, 48 mL was drained from C6, and 38 mL was drained from C7. In general, the cementitious amendments decreased water-infiltration rates through the tailings the most. This is likely explained by tailing cementation and cohesion processes that reduced the hydraulic conductivity of the amended materials [76].

4. Discussion

The unamended tailings (C1) showed an acidic behavior; pH values were lower than 3 from the very first stages of leaching (Figure 4). Consequently, the acidity of the leachates from the unamended tailings reached high levels compared to that of the amended tailings. This could be explained by the mineralogical composition of the mine tailings. Their carbonate content was lower than 0.2 wt.%, and the calcite liberation degree was around 50%. This meant that the reactive surface of calcite was reduced by half, as suggested by several authors who demonstrated that a mineral’s reactivity is influenced by its liberation degree [69,70,71,72,77]. Consequently, the tailings’ neutralization potential was likely negligible, assuming that the NP was influenced mainly by its carbonate content [5,11]. Mineralogical analyses of the mine tailings revealed that the acidity could be from two sources: (i) pyrite oxidation and (ii) latent acidity due to the release of exchangeable Fe [65,78,79]. Exchangeable Fe explains the high concentrations of Fe released within the unamended tailings during the first stages of the leaching tests. Moreover, considering environmental regulations in Canada, such as Directive 019 in Quebec [80], the mine tailings used in this study are considered as problematic and require a reclamation scenario to prevent environment contamination. Instantaneous Fe concentrations in leachates from the unamended tailings were around 78 mg/L, which exceeded the regulatory limit of 3 mg/L set by Directive 019 (Quebec, Canada). The same tendency was observed for Cu, Pb, and Zn, which also exceeded regulatory limits. Average instantaneous concentrations of Cu, Pb, and Zn were 20.3, 1, and 11.35 mg/L, respectively; while their average concentrations should not exceed 0.3, 0.2, and 0.5, respectively.
The geochemical behavior of limestone- and cement-based amendments (Table 2) enabled the neutralization of acidity in the Joutel mine tailings. Following the amendment, pH values were maintained at circumneutral values (around 7.5), and the leachates of the amended tailings were less concentrated in several significant, toxic metals. The two categories of amendments used in this study were: (i) alkaline amendments (10% and 20% limestone) and (ii) cementitious amendments (based on OPC, FAF, CVK, and FA). Acid buffering by all amendments was performed through carbonate dissolution [48,81,82,83]. Depending on the pH of the system, two reactions of calcite (carbonate) dissolution could occur (Equations (3) and (4)):
C a C O 3 s + 2 H aq + H 2 C O 3 aq + C a 2 +
C a C O 3 s + H aq + H C O 3 aq + C a 2 +
For the cement-based amendments, cement hydration and the precipitation of hydrated phases could produce additional alkalinity [23,43]. For example, the dissolution of two moles of tricalcium silicate (C3S) produced by cement hydration produces 8 moles of OH- following the reaction (Equation (5)):
2 C a 3 S i O 5 + 6 H 2 O 6 C a 2 + + 8 O H + 2 H 2 S i O 4 2
The mobilities of the chemical species, including Al, Cr, Cu, Fe, Pb, S, and Zn, were greatly reduced through the use of both the alkaline and cementitious amendments. Reduction factors, calculated using Equation (6), are presented for Al, Cr, Cu, Fe, Pb, S, and Zn in Figure 8. The reduction factor for each element was calculated based on its average concentration in leachates from the unamended and amended tailings [15]:
RF i = 100 × 1 C a C 0
where RFi is the reduction factor for element i; Ca is the cumulative concentration (mg/kg) for the element i from amended column (C2 to C7); and C0 is the cumulative concentration (mg/kg) for the element i in the leachates from oxidized tailings (control column; C1).
The RFAl was around 100% for all amendments tested in this study. The RFCr was about 100%, 81%, 100%, 100%, 100%, and 85 % for C2, C3, C4, C5, C6, and C7, respectively. RFCu, RFFe, RFPb, and RFZn values were >95% for all amendment formulations tested in this study. Sulfur was immobilized less compared to other elements. Indeed, S immobilization was only about 50%, 37%, 4%, 97%, 10%, and 13% for C2, C3, C4, C5, C6, and C7, respectively. Metals immobilization within cementitious and alkaline amendments is ensured by several chemical and physical mechanisms [15,27,48,84]:
i.
Alkaline amendments: adding alkaline materials, such as limestone, enhances the neutralization potential of the mixture. This shifts the balance between the acid-generating potential and neutralization potential in a given tailing [20,85]. Acid buffering is reflected by an increase in the alkalinity and pH of the leachates (Figure 4). Changing the geochemical conditions of the system influences the elemental deportment. This means that a number of secondary phases may precipitate [13], the most notable of which are Fe-oxyhydroxides such as ferrihydrite and goethite, and sulfates such as jarosite [68,86]. Although several mechanisms are responsible for metal(loid) attenuation, the most discussed mechanisms are Fe-oxyhydroxide precipitation, and sorption mechanisms [87,88,89]. Moreover, saturation indexes for ferrihydrite and goethite calculated using Visual Minteq (V3.1) showed that these two minerals will likely precipitate (saturation index >0) for the amended tailings (Figure 9A,B). However, for the unamended tailings, these two mineral species will remain in solution (saturation index <0). Dissolution for Fe-oxyhydroxides within the unamended tailings and their precipitation within the amended tailings explains the high concentrations of Fe analyzed within the leachates from the Joutel tailings (Figure 6A).
ii.
Cementitious amendments: the same mechanisms discussed within alkaline amendments also occur within cementitious amendments, as they also neutralize acid and increase pH (Figure 4). However, the use of cementitious additives also improves the mechanical properties of the mixtures [23,47,50]. The use of cement and industrial byproducts increases the cohesion and the long-term impermeabilization of the mixture [15]. Consequently, contaminant mobility and diffusion are significantly limited by (i) physical trapping, and (ii) reducing the reactive surface area of the mixture. Tailing solidification reduces the available surface area of sulfide minerals, and thus their reactivity [35,36].
Figure 9. Saturation index for (A) ferrihydrite and (B) goethite.
Figure 9. Saturation index for (A) ferrihydrite and (B) goethite.
Minerals 11 00413 g009
Performances of the tested amendments were significantly different considering results of the TCLP tests and KCTs. Column tests are more realistic than TCLP tests due to several factors: (i) sample size—within column tests, higher sample masses (>10 kg) are used compared to those used in TCLP tests (20 g); (ii) liquid/solid ratios (LSR)—the LSR in TCLP tests is about 20, while in column tests it is around 0.2; thus, dilution of elements may occur within the TCLP tests; (iii) test duration—KCTs and TCLP tests are performed on different time scales (18 h for TCLP tests and 361 days for columns); and (iv) leaching solutions—the solution used for the KCTs was deionized water, and that used for the TCLP tests was acetic acid. Therefore, the reactivity of the mineralogical phases will be different. For these reasons, KCTs may represent more accurate tests for evaluating the performance of amendments to stabilize acid-generating tailings. Moreover, Ghosh, Mukiibi [90] showed that TCLP tests may underestimate leaching of some chemical species such as arsenic.
Considering metal(loid) immobilization, both the alkaline and cementitious amendments showed relatively similar effectiveness. However, several factors make the formulations based on industrial byproducts better. The formulations based on limestone require a quarry for carbonate extraction. This represents an additional environmental impact to resolve another environmental problem (AMD). Consequently, the formulations based on industrial byproducts (e.g., fly ashes) could be more interesting. Substitution of byproducts for OPC could also reduce costs related to cement production and valorize some industrial wastes. Teixeira, Mateus [91] showed that the substitution of cement with fly ashes is a viable alternative because it allows the reduction of the environmental footprint of cement production. The use of industrial byproducts in the S/S technology is an ecofriendly option, but it must not affect the contaminants stabilization. This study proved that acid-generating and contaminated tailings can be stabilized using limestone and cementitious additives. Similarly, the use of industrial by-products in the stabilization of mine tailings needs more considerations during the rehabilitation of mine sites. Moreover, a technical and economic study is required to select the best scenario among those tested in this study. Additionally, geochemical modeling of the leachates from the different columns can be useful to predict the long-term efficiency (>10 y) of the tested formulations. Similarly, field tests are required to test the in situ effectiveness of the formulations used in this study. However, Elghali et al. (2019) [15] have already demonstrated that alkaline and cementitious amendments are efficient to neutralize acid-generating tailings and prevent contaminants release by AMD.

5. Conclusions

The reclamation and management of tailing storage facilities is a crucial step in the life cycle of a mine. The objective of TSF reclamation is to reduce or eliminate the risk of environment contamination due to acid and/or metal(loid) release. The mine tailings characterized in this study were acid-generating. Their neutralization potential was negligible due to carbonate depletion (calcite content <0.2 wt.%). Consequently, kinetic tests showed that the mine tailings generated AMD with no lag time. The mine tailings presented the risk of releasing Al, Cr, Cu, Fe, Pb, and Zn into the environment. Iron concentrations were significantly higher (78 mg/L) than the limit set by current regulations (3 mg/L). To stabilize these acid-generating tailings, amendments based on limestone, ordinary Portland cement, and fly ash were tested. All amendments showed promising results with respect to immobilizing potentially harmful chemical species. Indeed, pH values of the amended tailings immediately increased to circumneutral values (around 7.5). Moreover, the reduction factors of Al, Cr, Cu, Fe, Pb, and Zn releases were all higher than 80%. Application of this technique in the field at full scale will require a thorough economic evaluation of individual amendment formulations.

Author Contributions

Conceptualization, A.E.; formal analysis, A.E.; funding acquisition, B.B.; investigation, A.E.; methodology, A.E., M.B. and H.B.; supervision, M.B. and B.B.; validation, M.B., B.B. and H.B.; writing—original draft, A.E and M.B.; writing—review and editing, A.E., M.B., H.B. and B.B. All authors have read and agreed to the published version of the manuscript.

Funding

Funding for this study was provided by Mitacs (https://www.mitacs.ca/fr) and the NSERC-UQAT Industrial Research Chair on Mine Site Reclamation and its partners.

Data Availability Statement

Data sharing not applicable.

Acknowledgments

The authors thank the URSTM staff for their support with laboratory work.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Bussière, B.; Aubertin, M.; Mbonimpa, M.; Molson, J.W.; Chapuis, R.P. Field experimental cells to evaluate the hydrogeological behaviour of oxygen barriers made of silty materials. Can. Geotech. J. 2007, 44, 245–265. [Google Scholar] [CrossRef]
  2. Amar, H.; Benzaazoua, M.; Edahbi, M.; Villeneuve, M.; Joly, M.-A.; Elghali, A. Reprocessing feasibility of polymetallic waste rock for cleaner and sustainable mining. J. Geochem. Explor. 2021, 220, 106683. [Google Scholar] [CrossRef]
  3. Amar, H.; Elghali, A.; Benzaazoua, M. Geochemical behaviour of benign desulphurised waste rocks for mine drainage control and sustainable management. J. Geochem. Explor. 2021, 225, 106767. [Google Scholar] [CrossRef]
  4. Belem, T.; Benzaazoua, M.; Bussière, B. Mechanical behaviour of cemented paste backfill. In Proceedings of the 53rd Candadian Geotechnical Conference, Montreal, QC, Canada, 15–18 October 2000; pp. 373–380. [Google Scholar]
  5. Blowes, D.W.; Ptacek, C.J.; Jambor, J.L.; Weisener, C.G.; Paktunc, D.; Gould, W.D.; Johnson, D.B. The geochemistry of acid mine drainage. In Treatise on Geochemistry; Elsevier Science: Amsterdam, The Netherlands, 2014. [Google Scholar]
  6. Amar, H.; Benzaazoua, M.; Elghali, A.; Bussière, B.; Duclos, M. Upstream environmental desulphurisation and valorisation of waste rocks as a sustainable AMD management approach. J. Geochem. Explor. 2020, 215, 106555. [Google Scholar] [CrossRef]
  7. Evangelou, V.; Zhang, Y. A review: Pyrite oxidation mechanisms and acid mine drainage prevention. Crit. Rev. Environ. Sci. Technol. 1995, 25, 141–199. [Google Scholar] [CrossRef]
  8. Dmitrijeva, M.; Cook, N.J.; Ehrig, K.; Ciobanu, C.L.; Metcalfe, A.V.; Kamenetsky, M.; Kamenetsky, V.S.; Gilbert, S. Multivariate Statistical Analysis of Trace Elements in Pyrite: Prediction, Bias and Artefacts in Defining Mineral Signatures. Minerals 2020, 10, 61. [Google Scholar] [CrossRef] [Green Version]
  9. Cravotta, C.A., III. Dissolved metals and associated constituents in abandoned coal-mine discharges, Pennsylvania, USA. Part 1: Constituent quantities and correlations. Appl. Geochem. 2008, 23, 166–202. [Google Scholar] [CrossRef]
  10. España, J.S.; Pamo, E.L.; Pastor, E.S.; Andrés, J.R.; Rubí, J.A.M. The Removal of Dissolved Metals by Hydroxysulphate Precipitates during Oxidation and Neutralization of Acid Mine Waters, Iberian Pyrite Belt. Aquat. Geochem. 2006, 12, 269–298. [Google Scholar] [CrossRef]
  11. Jambor, J.; Dutrizac, J.; Groat, L.; Raudsepp, M. Static tests of neutralization potentials of silicate and aluminosilicate minerals. Environ. Geol. 2002, 43, 1–17. [Google Scholar]
  12. Parbhakar-Fox, A.; Lottermoser, B.G. A critical review of acid rock drainage prediction methods and practices. Miner. Eng. 2015, 82, 107–124. [Google Scholar] [CrossRef]
  13. Dold, B. Acid rock drainage prediction: A critical review. J. Geochem. Explor. 2017, 172, 120–132. [Google Scholar] [CrossRef]
  14. Aubertin, M.; McKenna, G. Tailings disposal challenges and prospects for oil sands mining operations. In Geo-Chicago 2016; Geo-Institute of ASCE: Reston, VA, USA, 2016; pp. 359–371. [Google Scholar]
  15. Elghali, A.; Benzaazoua, M.; Bussière, B.; Genty, T. In Situ Effectiveness of Alkaline and Cementitious Amendments to Stabilize Oxidized Acid-Generating Tailings. Minerals 2019, 9, 314. [Google Scholar] [CrossRef] [Green Version]
  16. Forján, R.; Asensio, V.; Rodríguez-Vila, A.; Covelo, E.F. Effect of amendments made of waste materials in the physical and chemical recovery of mine soil. J. Geochem. Explor. 2014, 147, 91–97. [Google Scholar] [CrossRef]
  17. Hakkou, R.; Benzaazoua, M.; Bussière, B. Laboratory evaluation of the use of alkaline phosphate wastes for the control of acidic mine drainage. Mine Water Environ. 2009, 28, 206. [Google Scholar] [CrossRef]
  18. Jang, A.; Kim, I.S. Solidification and stabilization of Pb, Zn, Cd and Cu in tailing wastes using cement and fly ash. Miner. Eng. 2000, 13, 1659–1662. [Google Scholar] [CrossRef]
  19. Kim, J.W.; Jung, M.C. Solidification of arsenic and heavy metal containing tailings using cement and blast furnace slag. Environ. Geochem. Health 2011, 33 (Suppl. 1), 151–158. [Google Scholar] [CrossRef]
  20. Komnitsas, K.; Bartzas, G.; Paspaliaris, I. Efficiency of limestone and red mud barriers: Laboratory column studies. Miner. Eng. 2004, 17, 183–194. [Google Scholar] [CrossRef]
  21. Mackie, A.L.; Walsh, M.E. Investigation into the use of cement kiln dust in high density sludge (HDS) treatment of acid mine water. Water Res. 2015, 85, 443–450. [Google Scholar] [CrossRef]
  22. Mylona, E.; Xenidis, A.; Paspaliaris, I. Inhibition of acid generation from sulphidic wastes by the addition of small amounts of limestone. Miner. Eng. 2000, 13, 1161–1175. [Google Scholar] [CrossRef]
  23. Nehdi, M.; Tariq, A. Stabilization of sulphidic mine tailings for prevention of metal release and acid drainage using cementitious materials: A review. J. Environ. Eng. Sci. 2007, 6, 423–436. [Google Scholar] [CrossRef]
  24. Rodríguez, L.; Gómez, R.; Sánchez, V.; Villaseñor, J.; Alonso-Azcárate, J. Performance of waste-based amendments to reduce metal release from mine tailings: One-year leaching behaviour. J. Environ. Manag. 2018, 209, 1–8. [Google Scholar] [CrossRef] [PubMed]
  25. Sarkkinen, M.; Kujala, K.; Gehör, S. Efficiency of MgO activated GGBFS and OPC in the stabilization of highly sulfidic mine tailings. J. Sustain. Min. 2019, 18, 115–126. [Google Scholar] [CrossRef]
  26. Stouraiti, C.; Xenidis, A.; Paspaliaris, I. Reduction of Pb, Zn and Cd Availability from Tailings and Contaminated Soils by the Application of Lignite Fly Ash. Water Air Soil Pollut. 2002, 137, 247–265. [Google Scholar] [CrossRef]
  27. Falciglia, P.P.; Romano, S.; Vagliasindi, F.G. Stabilisation/Solidification of soils contaminated by mining activities: Influence of barite powder and grout content on γ-radiation shielding, unconfined compressive strength and 232Th immobilisation. J. Geochem. Explor. 2017, 174, 140–147. [Google Scholar] [CrossRef]
  28. Kumpiene, J.; Lagerkvist, A.; Maurice, C. Stabilization of As, Cr, Cu, Pb and Zn in soil using amendments—A review. Waste Manag. 2008, 28, 215–225. [Google Scholar] [CrossRef]
  29. Li, X.D.; Poon, C.S.; Sun, H.; Lo, I.M.C.; Kirk, D.W. Heavy metal speciation and leaching behaviors in cement based solidified/stabilized waste materials. J. Hazard. Mater. 2001, 82, 215–230. [Google Scholar] [CrossRef]
  30. Mitchell, K.; Trakal, L.; Sillerova, H.; Avelar-González, F.J.; Guerrero-Barrera, A.L.; Hough, R.; Beesley, L. Mobility of As, Cr and Cu in a contaminated grassland soil in response to diverse organic amendments; a sequential column leaching experiment. Appl. Geochem. 2018, 88, 95–102. [Google Scholar] [CrossRef]
  31. Mu, Y.; Saffarzadeh, A.; Shimaoka, T. Utilization of waste natural fishbone for heavy metal stabilization in municipal solid waste incineration fly ash. J. Clean. Prod. 2018, 172, 3111–3118. [Google Scholar] [CrossRef]
  32. Park, C.-K. Hydration and solidification of hazardous wastes containing heavy metals using modified cementitious materials. Cem. Concr. Res. 2000, 30, 429–435. [Google Scholar] [CrossRef]
  33. Pesonen, J.; Yliniemi, J.; Illikainen, M.; Kuokkanen, T.; Lassi, U. Stabilization/solidification of fly ash from fluidized bed combustion of recovered fuel and biofuel using alkali activation and cement addition. J. Environ. Chem. Eng. 2016, 4, 1759–1768. [Google Scholar] [CrossRef]
  34. Simon, L. Stabilization of metals in acidic mine spoil with amendments and red fescue (Festuca rubra L.) growth. Environ. Geochem. Health 2005, 27, 289–300. [Google Scholar] [CrossRef]
  35. Wang, F.; Shen, Z.; Al-Tabbaa, A. PC-based and MgO-based binders stabilised/solidified heavy metal-contaminated model soil: Strength and heavy metal speciation in early stage. Géotechnique 2018, 68, 1025–1030. [Google Scholar] [CrossRef]
  36. Wang, F.; Wang, H.; Jin, F.; Al-Tabbaa, A. The performance of blended conventional and novel binders in the in-situ stabilisation/solidification of a contaminated site soil. J. Hazard. Mater. 2015, 285, 46–52. [Google Scholar] [CrossRef] [Green Version]
  37. Xia, M.; Muhammad, F.; Zeng, L.; Li, S.; Huang, X.; Jiao, B.; Shiau, Y.; Li, D. Solidification/stabilization of lead-zinc smelting slag in composite based geopolymer. J. Clean. Prod. 2019, 209, 1206–1215. [Google Scholar] [CrossRef]
  38. Xia, W.-Y.; Du, Y.-J.; Li, F.-S.; Li, C.-P.; Yan, X.-L.; Arulrajah, A.; Wang, F.; Song, D.-J. In-situ solidification/stabilization of heavy metals contaminated site soil using a dry jet mixing method and new hydroxyapatite based binder. J. Hazard. Mater. 2019, 369, 353–361. [Google Scholar] [CrossRef]
  39. Zanuzzi, A.; Faz, A.; Acosta, J.A. Chemical stabilization of metals in the environment: A feasible alternative for remediation of mine soils. Environ. Earth Sci. 2013, 70, 2623–2632. [Google Scholar] [CrossRef]
  40. Belem, T.; Benzaazoua, M. Design and application of underground mine paste backfill technology. Geotech. Geol. Eng. 2008, 26, 147–174. [Google Scholar] [CrossRef]
  41. Benzaazoua, M.; Belem, T.; Bussière, B. Chemical factors that influence the performance of mine sulphidic paste backfill. Cem. Concr. Res. 2002, 32, 1133–1144. [Google Scholar] [CrossRef]
  42. Benzaazoua, M.; Bussière, B.; Demers, I.; Aubertin, M.; Fried, É.; Blier, A. Integrated mine tailings management by combining environmental desulphurization and cemented paste backfill: Application to mine Doyon, Quebec, Canada. Miner. Eng. 2008, 21, 330–340. [Google Scholar] [CrossRef]
  43. Benzaazoua, M.; Marion, P.; Picquet, I.; Bussière, B. The use of pastefill as a solidification and stabilization process for the control of acid mine drainage. Miner. Eng. 2004, 17, 233–243. [Google Scholar] [CrossRef]
  44. Peyronnard, O.; Benzaazoua, M. Alternative by-product based binders for cemented mine backfill: Recipes optimisation using Taguchi method. Miner. Eng. 2012, 29, 28–38. [Google Scholar] [CrossRef]
  45. Duchesne, J.; Reardon, E. Determining controls on element concentrations in cement kiln dust leachate. Waste Manag. 1998, 18, 339–350. [Google Scholar] [CrossRef]
  46. Nicholson, R.V.; Gillham, R.W.; Reardon, E.J. Pyrite oxidation in carbonate-buffered solution: 1. Experimental kinetics. Geochim. Cosmochim. Acta 1988, 52, 1077–1085. [Google Scholar] [CrossRef]
  47. Kogbara, R.B.; Yi, Y.; Al-Tabbaa, A. Process envelopes for stabilisation/solidification of contaminated soil using lime–slag blend. Environ. Sci. Pollut. Res. 2011, 18, 1286–1296. [Google Scholar] [CrossRef]
  48. Holmström, H.; Ljungberg, J.; Öhlander, B. Role of carbonates in mitigation of metal release from mining waste. Evidence from humidity cells tests. Environ. Geol. 1999, 37, 267–280. [Google Scholar] [CrossRef]
  49. Ichrak, H.; Mostafa, B.; Abdelkabir, M.; Bruno, B. Effect of cementitious amendment on the hydrogeological behavior of a surface paste tailings’ disposal. Innov. Infrastruct. Solut. 2016, 1, 19. [Google Scholar] [CrossRef] [Green Version]
  50. Kogbara, R.B.; Al-Tabbaa, A. Mechanical and leaching behaviour of slag-cement and lime-activated slag stabilised/solidified contaminated soil. Sci. Total Environ. 2011, 409, 2325–2335. [Google Scholar] [CrossRef]
  51. Moreno-Jiménez, E.; Sepúlveda, R.; Esteban, E.; Beesley, L. Efficiency of organic and mineral based amendments to reduce metal[loid]mobility and uptake (Lolium perenne) from a pyrite-waste contaminated soil. J. Geochem. Explor. 2017, 174, 46–52. [Google Scholar] [CrossRef]
  52. Paradis, M.; Duchesne, J.; Lamontagne, A.; Isabel, D. Using red mud bauxite for the neutralization of acid mine tailings: A column leaching test. Can. Geotech. J. 2006, 43, 1167–1179. [Google Scholar] [CrossRef]
  53. Srivastava, S.; Chaudhary, R.; Khale, D. Influence of pH, curing time and environmental stress on the immobilization of hazardous waste using activated fly ash. J. Hazard. Mater. 2008, 153, 1103–1109. [Google Scholar] [CrossRef] [PubMed]
  54. Wan, Q.; Rao, F.; Song, S.; Zhang, Y. Immobilization forms of ZnO in the solidification/stabilization (S/S) of a zinc mine tailing through geopolymerization. J. Mater. Res. Technol. 2019. [Google Scholar] [CrossRef]
  55. Woldetsadik, D.; Drechsel, P.; Keraita, B.; Marschner, B.; Itanna, F.; Gebrekidan, H. Effects of biochar and alkaline amendments on cadmium immobilization, selected nutrient and cadmium concentrations of lettuce (Lactuca sativa) in two contrasting soils. SpringerPlus 2016, 5, 397. [Google Scholar] [CrossRef] [PubMed] [Green Version]
  56. Yi, Y.; Wen, J.; Zeng, G.; Zhang, T.; Huang, F.; Qin, H.; Tian, S. A comparative study for the stabilisation of heavy metal contaminated sediment by limestone, MnO2 and natural zeolite. Environ. Sci. Pollut. Res. 2017, 24, 795–804. [Google Scholar] [CrossRef] [PubMed]
  57. Blowes, D.W.; Jambor, J.L.; Hanton-Fong, C.J.; Lortie, L.; Gould, W.D. Geochemical, mineralogical and microbiological characterization of a sulphide-bearing carbonate-rich gold-mine tailings impoundment, Joutel, Québec. Appl. Geochem. 1998, 13, 687–705. [Google Scholar] [CrossRef]
  58. Elghali, A.; Benzaazoua, M.; Bussière, B.; Genty, T. Spatial Mapping of Acidity and Geochemical Properties of Oxidized Tailings within the Former Eagle/Telbel Mine Site. Minerals 2019, 9, 180. [Google Scholar] [CrossRef] [Green Version]
  59. Ahmaruzzaman, M. A review on the utilization of fly ash. Prog. Energy Combust. Sci. 2010, 36, 327–363. [Google Scholar] [CrossRef]
  60. Miller, P.; Zuiderwyk, M.; Reid, A. SEM Image Analysis in the Determination of Modal Assays, Mineral Associations and Mineral Liberation. 1983. Available online: http://pdf.library.laurentian.ca/medb/conf/Sudbury99/AcidicDrainage/AD8.PDF (accessed on 15 March 2021).
  61. Halim, C.E.; Amal, R.; Beydoun, D.; Scott, J.A.; Low, G. Evaluating the applicability of a modified toxicity characteristic leaching procedure (TCLP) for the classification of cementitious wastes containing lead and cadmium. J. Hazard. Mater. 2003, 103, 125–140. [Google Scholar] [CrossRef]
  62. US EPA. EPA Method 1311; United States Environmental Protection Agency: Washington, DC, USA, 2012.
  63. Bussière, B.; Benzaazoua, M.; Aubertin, M.; Mbonimpa, M. A laboratory study of covers made of low-sulphide tailings to prevent acid mine drainage. Environ. Geol. 2004, 45, 609–622. [Google Scholar] [CrossRef]
  64. Demers, I.; Bussière, B.; Aachib, M.; Aubertin, M. Repeatability evaluation of instrumented column tests in cover efficiency evaluation for the prevention of acid mine drainage. Water Air Soil Pollut. 2011, 219, 113–128. [Google Scholar] [CrossRef]
  65. Elghali, A.; Benzaazoua, M.; Bussière, B.; Kennedy, C.; Parwani, R.; Graham, S. The role of hardpan formation on the reactivity of sulfidic mine tailings: A case study at Joutel mine (Québec). Sci. Total Environ. 2019, 654, 118–128. [Google Scholar] [CrossRef]
  66. Gustafsson, J.P. Visual MINTEQ 3.0 User Guide; KTH, Department of Land and Water Recources: Stockholm, Sweden, 2011. [Google Scholar]
  67. Adam, K.; Kourtis, A.; Gazea, B.; Kontopoulos, A. Evaluation of static tests used to predict the potential for acid drainage generation at sulphide mine sites. Min. Technol. IMM Trans. Sect. A 1997, 106, A1–A8. [Google Scholar]
  68. Nordstrom, D.K.; Blowes, D.W.; Ptacek, C.J. Hydrogeochemistry and microbiology of mine drainage: An update. Appl. Geochem. 2015, 57, 3–16. [Google Scholar] [CrossRef]
  69. Brough, C.; Strongman, J.; Bowell, R.; Warrender, R.; Prestia, A.; Barnes, A.; Fletcher, J. Automated environmental mineralogy; the use of liberation analysis in humidity cell testwork. Miner. Eng. 2017, 107, 112–122. [Google Scholar] [CrossRef]
  70. Elghali, A.; Benzaazoua, M.; Bouzahzah, H.; Bussière, B.; Villarraga-Gómez, H. Determination of the available acid-generating potential of waste rock, part I: Mineralogical approach. Appl. Geochem. 2018, 99, 31–41. [Google Scholar] [CrossRef]
  71. Elghali, A.; Benzaazoua, M.; Bussière, B.; Bouzahzah, H. Determination of the available acid-generating potential of waste rock, part II: Waste management involvement. Appl. Geochem. 2019, 100, 316–325. [Google Scholar] [CrossRef]
  72. Erguler, Z.A.; Kalyoncu Erguler, G. The effect of particle size on acid mine drainage generation: Kinetic column tests. Miner. Eng. 2015, 76, 154–167. [Google Scholar] [CrossRef]
  73. Paktunc, A.; Davé, N. Mineralogy of pyritic waste rock leached by column experiments and prediction of acid mine drainage. In Applied Mineralogy; Rammlmair, D., Ed.; Balkema: Rotterdam, The Netherlands, 2000; pp. 621–623. [Google Scholar]
  74. Benzaazoua, M.; Bussière, B.; Dagenais, A.-M.; Archambault, M. Kinetic tests comparison and interpretation for prediction of the Joutel tailings acid generation potential. Environ. Geol. 2004, 46, 1086–1101. [Google Scholar] [CrossRef]
  75. Cravotta, C.A., III. Dissolved metals and associated constituents in abandoned coal-mine discharges, Pennsylvania, USA. Part 2: Geochemical controls on constituent concentrations. Appl. Geochem. 2008, 23, 203–226. [Google Scholar] [CrossRef]
  76. Godbout, J.; Bussière, B.; Belem, T. Evolution of Cemented Paste Backfill Saturated Hydraulic Conductivity at Early Curing Time. 2007. Available online: http://citeseerx.ist.psu.edu/viewdoc/download?doi=10.1.1.484.1839&rep=rep1&type=pdf (accessed on 15 March 2021).
  77. Lapakko, K.A.; Engstrom, J.N.; Antonson, D.A. Effects of particle size on drainage quality from three lithologies. In Proceedings of the 7th International Conference on Acid Rock Drainage (ICARD), St. Louis, MO, USA, 26–30 March 2006; pp. 1026–1050. [Google Scholar]
  78. Cravotta, C., III. Secondary iron-sulfate minerals as sources of sulfate and acidity: Geochemical evolution of acidic ground water at a reclaimed surface coal mine in Pennsylvania. In Environmental Geochemistry of Sulfide Oxidation; ACS Symposium Series; American Chemical Society: Washington, DC, USA, 1994. [Google Scholar]
  79. Fox, L.E. The solubility of colloidal ferric hydroxide and its relevance to iron concentrations in river water. Geochim. Cosmochim. Acta 1988, 52, 771–777. [Google Scholar] [CrossRef]
  80. Québec, G.d. Directive 019 sur L’Industrie Minière; Ministère Du Développement Durableenvironement Et Parcsgouvernement Du Québec: Quebec City, QC, Canada, 2012; p. 105. [Google Scholar]
  81. Doye, I.; Duchesne, J. Neutralisation of acid mine drainage with alkaline industrial residues: Laboratory investigation using batch-leaching tests. Appl. Geochem. 2003, 18, 1197–1213. [Google Scholar] [CrossRef]
  82. Kalia, N.; Balakotaiah, V. Effect of medium heterogeneities on reactive dissolution of carbonates. Chem. Eng. Sci. 2009, 64, 376–390. [Google Scholar] [CrossRef]
  83. Li, M.G.; Bernier, L. Contributions of Carbonates and Silicates to Neutralization Observed in Laboratory Tests and Their Field Implications; Belzile, N., Yearwood, P., Goldsack, D., Eds.; CIM: Montreal, QC, Canada, 1999; pp. 59–68. [Google Scholar]
  84. Fatahi, B.; Khabbaz, H. Influence of Chemical Stabilisation on Permeability of Municipal Solid Wastes. Geotech. Geol. Eng. 2015, 33, 455–466. [Google Scholar] [CrossRef]
  85. De Andrade, R.P.; Figueiredo, B.R.; de Mello, J.W.V.; Santos, J.C.Z.; Zandonadi, L.U. Control of geochemical mobility of arsenic by liming in materials subjected to acid mine drainage. J. Soils Sediments 2008, 8, 123–129. [Google Scholar] [CrossRef]
  86. Nordstrom, D.K.; Southam, G. Geomicrobiology of sulfide mineral oxidation. Rev. Mineral. 1997, 35, 361–390. [Google Scholar]
  87. Manceau, A. The mechanism of anion adsorption on iron oxides: Evidence for the bonding of arsenate tetrahedra on free Fe(O, OH)6 edges. Geochim. Cosmochim. Acta 1995, 59, 3647–3653. [Google Scholar] [CrossRef]
  88. Manceau, A.; Charlet, L.; Boisset, M.C.; Didier, B.; Spadini, L. Sorption and speciation of heavy metals on hydrous Fe and Mn oxides. From microscopic to macroscopic. Appl. Clay Sci. 1992, 7, 201–223. [Google Scholar] [CrossRef]
  89. Manceau, A.; Combes, J.M. Structure of Mn and Fe oxides and oxyhydroxides: A topological approach by EXAFS. Phys. Chem. Miner. 1988, 15, 283–295. [Google Scholar] [CrossRef]
  90. Ghosh, A.; Mukiibi, M.; Ela, W. TCLP underestimates leaching of arsenic from solid residuals under landfill conditions. Environ. Sci. Technol. 2004, 38, 4677–4682. [Google Scholar] [CrossRef]
  91. Teixeira, E.R.; Mateus, R.; Camões, A.F.; Bragança, L.; Branco, F.G. Comparative environmental life-cycle analysis of concretes using biomass and coal fly ashes as partial cement replacement material. J. Clean. Prod. 2016, 112, 2221–2230. [Google Scholar] [CrossRef] [Green Version]
Figure 1. (A) Mineralogical composition of mine tailings; (B) calcite and pyrite liberation degrees.
Figure 1. (A) Mineralogical composition of mine tailings; (B) calcite and pyrite liberation degrees.
Minerals 11 00413 g001
Figure 2. Backscattered electron (BSE) images showing the precipitation of secondary iron oxides on the surfaces of pyrite and silicates (Py = pyrite, Fe-oxi = iron oxides). (AD) examples of pyrite and silicates coated by iron oxides.
Figure 2. Backscattered electron (BSE) images showing the precipitation of secondary iron oxides on the surfaces of pyrite and silicates (Py = pyrite, Fe-oxi = iron oxides). (AD) examples of pyrite and silicates coated by iron oxides.
Minerals 11 00413 g002
Figure 3. Elemental deportment of Ca, Fe, Mg, and S within the Joutel mine tailings.
Figure 3. Elemental deportment of Ca, Fe, Mg, and S within the Joutel mine tailings.
Minerals 11 00413 g003
Figure 4. Evolution of (A) pH, (B) electrical conductivity, (C) acidity, and (D) alkalinity within the leachates from the kinetic column tests.
Figure 4. Evolution of (A) pH, (B) electrical conductivity, (C) acidity, and (D) alkalinity within the leachates from the kinetic column tests.
Minerals 11 00413 g004
Figure 5. Evolution of cumulative concentrations of (A) Ca, (B) Mg, (C) Mn, and (D) Al.
Figure 5. Evolution of cumulative concentrations of (A) Ca, (B) Mg, (C) Mn, and (D) Al.
Minerals 11 00413 g005
Figure 6. Evolution of cumulative concentrations of (A) Fe, (B) S, (C) Cu, and (D) Zn.
Figure 6. Evolution of cumulative concentrations of (A) Fe, (B) S, (C) Cu, and (D) Zn.
Minerals 11 00413 g006
Figure 7. Results of water infiltration through the different kinetic column tests.
Figure 7. Results of water infiltration through the different kinetic column tests.
Minerals 11 00413 g007
Figure 8. Reduction factors for selected elements in comparison to initial concentrations within unamended tailings.
Figure 8. Reduction factors for selected elements in comparison to initial concentrations within unamended tailings.
Minerals 11 00413 g008
Table 1. Some case studies of alkaline and cementitious amendments used to stabilize contaminated materials.
Table 1. Some case studies of alkaline and cementitious amendments used to stabilize contaminated materials.
ProblematicAmendmentsCountryReference
Acid-generating tailings5% and 10% limestone, 5% OPC, 5% (1/2 OPC-1/2 FA)Canada[15]
Contaminated mine soilsSludges from a purification plant and a bleach plantSpain[16]
Acid-generating mine tailingsAlkaline phosphate wastesMorocco[17]
Contaminated mine tailingsOrdinary Portland cement and furnace slagKorea[18,19]
Synthetic-acid-generating tailingsLimestone and red mudGreece[20]
Acid mine drainageCement kiln dustCanada[21]
Sulfidic mine wasteLimestoneCanada[22]
Acid-generating mine wastesCementitious materialsReview paper[23]
Contaminated mine tailingsSugar foam, lime-rich waste, drinking-water-treatment sludge, olive mill waste and paper mill sludgeSpain[24]
Highly sulfidic mine tailingsMgO-activated ground granulated blast-furnace slag and ordinary Portland cementFinland[25]
Tailings and contaminated soilsFly ashGreece[26]
Radioactive-contaminated soilsPortland cement and barite powderItaly[27]
Contaminated materialsOrganic matter, alkaline materialReview paper[28]
Waste materialsOrdinary Portland cement and pulverized fly ashNot indicated[29]
Wood-ash-contaminated grassland soilBiocharNot indicated[30]
Municipal solid-waste incinerationWaste fishboneJapan[31]
Synthetic-contaminated materialsOrdinary Portland cement, clinker kiln dust modified OPC, cement kiln dustSouth Korea[32]
Fuel–biofuel fly ashOrdinary Portland cement and alkali activationFinland[33]
Acidic and phytotoxic mine spoilLime and nitrogen (NH4NO3)Hungary[34]
Contaminated soilsPortland cement, MgO-based cement, ground granulated blast-furnace slagUnited Kingdom[35]
Contaminated soilsPortland cement, ground granulated blast-furnace slag, pulverized fuel ash, MgO, and zeoliteUnited Kingdom[36]
Lead–zinc smelting slagGeopolymerizationChina[37]
Contaminated soilsSuperphosphate and calcium oxideChina[38]
Mine soilsLime, organic amendmentsSpain[39]
Mine backfillOrdinary Portland cement, cement kiln dust, ground granulated blast furnace slag, waste glass, copper slag, wood bottom ash and coal fly ashCanada[44]
Synthetic-contaminated soilsLime-slagUnited Kingdom[47]
Acid generating mine tailings
CarbonatesSweden[48]
Acid-generating mine tailings2% Portland cementCanada[49]
Synthetic-contaminated soilsGround granulated blast-furnace slag and hydrated limeUnited Kingdom[50]
Pyrite-waste-contaminated soilIron- and phosphorus-based amendmentsSpain[51]
Acid-generating mine tailingsRed mud bauxiteCanada[52]
Contaminated sludge generated from common effluent treatment plantOrdinary Portland cement, fly ash and sludgeIndia[53]
Zinc mine tailingsGeopolymerizationChina[54]
Cadmium-spiked soilsBiochar and alkaline amendmentsEthiopia[55]
Contaminated sedimentsLimestone, MnO2, and natural zeoliteChina[56]
Table 2. Formulations used for the alkaline and cementitious amendments.
Table 2. Formulations used for the alkaline and cementitious amendments.
ColumnAmendment TypeFormulation
C1ReferenceMine tailings
C2Alkaline amendment20 wt.% LS
C3Alkaline amendment10 wt.% LS
C4Cementitious amendment5 wt.% (50%FAF-50%CVK)
C5Cementitious amendment5 wt.% (20%OPC-40%CVK-40%FAF)
C6Cementitious amendment5 wt.% (80%OPC-20%CVK)
C7Cementitious amendment5 wt.% (20%OPC-40%CVK-40%FA)
Table 3. Grain-size distribution and chemical composition of the studied samples (MT = mine tailing, LS = limestone, OPC = ordinary Portland cement, FA = fly ash, CVK = Kruger fly ash, FAF = fly ash class F, and DL = detection limit).
Table 3. Grain-size distribution and chemical composition of the studied samples (MT = mine tailing, LS = limestone, OPC = ordinary Portland cement, FA = fly ash, CVK = Kruger fly ash, FAF = fly ash class F, and DL = detection limit).
UnitsDL (ppm)MTLSOPCFACVKFAF
Chemical compositionAl%601.730.302.754.693.8411.91
Ca603.0033.8249.077.5834.882.87
Mg150.272.351.181.051.560.58
Mn50.2310.030.060.420.120.02
Na10.9720.1250.161.960.450.45
K10.2670.2450.431.850.321.38
Fe1019.300.4832.232.243.3113.43
Li5≤DL≤DL≤DL0.002≤DL≤DL
Pb50.042≤DL≤DL≤DL0.05≤DL
As5≤DL≤DL0.005≤DL0.006≤DL
Cr50.010.0040.0070.0060.0140.02
Cu100.001≤DL0.007≤DL0.031≤DL
Zn550.007≤DL0.0490.0700.150.19
S (total)2004.36NA1.7370.4313.330.38
S (sulfates) 4.20NANANA3.330.38
C9000.2NANANA1.292.69
Physical characteristicsD10µm 1.8504.2825.786.07
D30 4.725011.318014.312.8
D90 30.4450046.71500104.1789.12
Table 4. Results of the TCLP tests performed on unamended and amended tailings. Concentrations are presented in ppm. <DL indicates concentrations lower than the detection limit of the method.
Table 4. Results of the TCLP tests performed on unamended and amended tailings. Concentrations are presented in ppm. <DL indicates concentrations lower than the detection limit of the method.
pHEC (mS/cm)AlFeNiSZn
C12.507.810.400.500.017660.60
C26.469.370.010.06<DL5670.34
C35.588.840.010.05< DL6080.33
C45.008.150.040.05< DL6640.30
C55.058.250.020.05< DL6690.60
C64.928.170.030.08< DL6960.31
C74.938.050.050.04< DL6950.30
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Elghali, A.; Benzaazoua, M.; Bouzahzah, H.; Bussière, B. Laboratory Study on the Effectiveness of Limestone and Cementitious Industrial Products for Acid Mine Drainage Remediation. Minerals 2021, 11, 413. https://doi.org/10.3390/min11040413

AMA Style

Elghali A, Benzaazoua M, Bouzahzah H, Bussière B. Laboratory Study on the Effectiveness of Limestone and Cementitious Industrial Products for Acid Mine Drainage Remediation. Minerals. 2021; 11(4):413. https://doi.org/10.3390/min11040413

Chicago/Turabian Style

Elghali, Abdellatif, Mostafa Benzaazoua, Hassan Bouzahzah, and Bruno Bussière. 2021. "Laboratory Study on the Effectiveness of Limestone and Cementitious Industrial Products for Acid Mine Drainage Remediation" Minerals 11, no. 4: 413. https://doi.org/10.3390/min11040413

APA Style

Elghali, A., Benzaazoua, M., Bouzahzah, H., & Bussière, B. (2021). Laboratory Study on the Effectiveness of Limestone and Cementitious Industrial Products for Acid Mine Drainage Remediation. Minerals, 11(4), 413. https://doi.org/10.3390/min11040413

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop