Next Article in Journal
Optimization of the Production of Enzymatic Biodiesel from Residual Babassu Oil (Orbignya sp.) via RSM
Next Article in Special Issue
A Colorimetric Aptamer Sensor Based on the Enhanced Peroxidase Activity of Functionalized Graphene/Fe3O4-AuNPs for Detection of Lead (II) Ions
Previous Article in Journal
The Influence of Pluronic F-127 Modification on Nano Zero-Valent Iron (NZVI): Sedimentation and Reactivity with 2,4-Dichlorophenol in Water Using Response Surface Methodology
Previous Article in Special Issue
Effect of KCoMoS2 Catalyst Structures on the Catalytic Performance of Higher Alcohols Synthesis via CO Hydrogenation
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

NaBiS2 as a Novel Indirect Bandgap Full Spectrum Photocatalyst: Synthesis and Application

1
Shaanxi Engineering Laboratory for Advanced Energy Technology, School of Materials Science & Engineering, Shaanxi Normal University, Xi’an 710119, China
2
High-Tech Institute of Xi’an, Xi’an 710025, China
3
Shaanxi Key Laboratory of Special Fuel Chemistry and Material, Xi’an 710025, China
*
Authors to whom correspondence should be addressed.
Catalysts 2020, 10(4), 413; https://doi.org/10.3390/catal10040413
Submission received: 24 March 2020 / Revised: 2 April 2020 / Accepted: 5 April 2020 / Published: 9 April 2020
(This article belongs to the Special Issue Advanced Nanomaterials - Synthesis and Applications in Catalysis)

Abstract

:
Photocatalysts with a superior activity range, from ultraviolet (UV) to near-infrared (NIR) light, are attractive for solar utilization. From this perspective, sulfides are promising due to their narrower bandgap than oxides. In this report, NaBiS2 was synthesized hydrothermally under mild conditions by adjusting the alkaline amount. The rough NaBiS2 nanosheets possessed various surface atomic configurations on their surfaces, including amorphous clusters and amorphous nano-domains, revealed by HRTEM. A theoretical investigation of the band structure employing the density functional theory (DFT) method for the first time indicated that NaBiS2 is an indirect bandgap semiconductor with a narrow bandgap of 1.02 eV. Experimentally, it showed excellent photocatalytic activity for the degradation of methyl blue under UV, visible light and NIR light due to its experimental bandgap width of 1.32 eV. A degradation rate of 99.6% was reached after 80 min under full spectrum irradiation.

Graphical Abstract

1. Introduction

Though massive efforts have been made to conquer the predicament of environmental pollution and the energy crisis, it is still an arduous task to completely settle this dilemma worldwide. The utilization of solar energy in photocatalytic [1,2,3] and photovoltaic [4,5,6] manners is considered a promising strategy for green and sustainable development. The photocatalytic degradation of hazardous substances based on semiconductor catalysts could thoroughly decompose organic pollutants into inorganic molecules theoretically, and possesses the superiorities of low energy investment and being environmentally friendly. However, most research focuses on wide energy bandgap materials such as TiO2 [7], Bi2WO4 [8,9] and g-C3N4 [10,11], which only absorb ultraviolet (UV) and visible light. Recently, semiconductors with a narrow bandgap (Eg < 2.0 eV) have aroused extensive concern [12,13,14,15,16].
Unlike the classical UV light utilization mechanism, various mechanisms are involved for full solar light spectrum utilization [13,17] and the exploitation of broadband spectrum photocatalysts is still one of the most promising. The width of the bandgap is completely dependent on the composition of the valence band and the conduction band. Compared to oxides, sulfides have a shallower energy level and usually possess a narrower bandgap. This is beneficial for the development of near-infrared (NIR) active photocatalysts. Based on this assumption, a handful of materials with NIR photocatalytic activity were studied recently. An original WS2 (Eg = 1.35 eV) nanosheet, fabricated by pyrolysis of (NH4)WS4 in a hydrogen flow, was investigated as a full solar light spectrum photocatalyst for methyl orange (MO) photodegradation in various pH conditions [13]. As reported by the same group, β-In2S3 demonstrated an excellent broadband photocatalytic activity range, from ultraviolet to near-infrared, in degrading MO [15]. Recently, Sb2S3 with an Eg of 1.48 eV was deemed to have remarkable near-infrared-driven Cr(VI) reduction conversion efficiency in an aqueous solution, and this novel property could be further improved by being composited with MoS2 [18]. Additionally, by means of compositing with carbon or other materials, several binary sulfides revealed non-ignorable photocatalytic activity under full solar spectrum irradiation, though these sulfides showed no NIR photocatalytic activity intrinsically [19,20,21,22]. On account of their air-sensibility, those sulfides were usually fabricated through a rigorous process, which was an obstacle to their practical application for solar energy utilization.
Herein, we report a facile hydrothermal method for ternary sulfide NaBiS2 synthesis as a novel broadband spectrum photocatalyst, without a rigorous process or poisonous reagents. The alkaline amount is believed to be pivotal for NaBiS2 formation. The band structure was investigated theoretically by the density functional theory (DFT) method using a Vienna ab-initio simulation package (VASP), and NaBiS2 was deemed to be an indirect bandgap semiconductor. Its superior broadband spectrum photocatalytic activity and chemical stability were confirmed through a degradation test of methyl blue (MB). Both the experimental and theoretical results indicated the prospect of the application of NaBiS2 as a novel photocatalyst, and provided a new opportunity for expanding the utilization of solar light.

2. Results and Discussion

Figure 1a shows the XRD pattern of the sample synthesized through a typical hydrothermal procedure at 160 ℃. All of the diffraction peaks can be indexed to NaBiS2 without any impurity by careful comparison with JCPDS card file no. 08-0406, and agree well with NaCl-type structure. The sharp peaks indicate well-developed crystallinity and the grain size, evaluated by the Scherer equation, is 65.4 nm.
NaBiS2 was reported to be synthesized from mixtures of Bi(NO3)3 and L-cysteine [23], or by a two-step hydrothermal process from Bi(NO3)3·5H2O and Na2S·9H2O [24], both of which were reacted in NaOH aqueous solution. Nevertheless, NaBiS2 was believed not to be the most stable product in the hydrothermal process. The initially formed polycrystals would decompose in the following reaction and tended to transform into Bi2S3 [25,26]. A contradictory phenomenon indicated that the formation mechanism of NaBiS2 is still unclear, and an in-depth study on the conditions for NaBiS2 synthesis is necessary.
With an excess amount of Na2S for NaBiS2 stoichiometry and concentrated alkaline solutions provided by NaOH, NaBiS2 was obtained through the typical procedure. Fabrications with less Na2S or NaOH were also carried out, respectively. As shown in Figure 1b, the formation of NaBiS2 was strongly correlated to the amount of NaOH. Without plenty of NaOH in the solution (the mole ratio of Bi(NO3)3 to NaOH was less than 1:5), no NaBiS2 was detected by XRD, even if the amount of S2− was excessive (samples 1–3 in Figure 1b). The promiscuous diffraction peaks could be indexed to BiONO3, Bi2O3 or Bi2S3, which were hydrolysis products or the sulfide precipitation of Bi(NO3)3. Under a high alkalinity condition, crystalline NaBiS2 could be obtained easily even with a stoichiometric ratio of S2− (samples 4–6) and impurities were completely suppressed when Na2S was in excess (sample 6). An alkaline condition was found to be beneficial and crucial to the formation of crystalline NaBiS2. This might be due to the increased solubility of the hydrolysis product of Bi ions under the circumstance of an alkaline solution [27,28]. In this work, a mole ratio of 1:10 for Bi(NO3)3 to NaOH was found to be the critical concentration for NaBiS2 hydrothermal synthesis in the above mentioned procedure.
Morphologies were checked by employing SEM and TEM. As shown in Figure 2a, the as-fabricated sediments were nanoplates with a thickness less than 100 nm. These nanostructures were irregular in shape and their surfaces were rough. Obvious grain boundaries can be observed in a low magnified TEM image (Figure 2b), and the inhomogeneous contrast indicates the polycrystallinity of the as-prepared sheets. A high magnified TEM image (Figure 2c) reveals that these grain boundaries may be derived from the incomplete development of the crystal lattice. Several besieged nanoscale surface domains show different atomic configurations compared with the surface atomic arrangement of the matrix. For example, region 1 in Figure 1c shows more incompact surface atom arrangement than that of the matrix. The latter has the lattice distance of 0.4263 nm in [010] direction and 0.3612 nm in [ 1 1 ¯ 0 ] direction. As for region 3, though the atom arrangement is still uniform, the edge of it is amorphous. More amorphous nano-domains are shown in region 2 and region 4. The surface defects such as edges, corners, dopant atoms or heterogeneous domains usually serve as active sites in a photocatalytic reaction due to their particular electronic structure [29,30]. The selected area electron diffraction (SEAD) result (see the insert of Figure 2c) displayed discrete diffraction rings mixed with several diffraction spots. This means that the nanosheets are not homogeneous and monocrystalline. The inhomogeneity of the nanosheets’ surface is conducive to the absorption and surface chemical reaction of organic molecules, and will be beneficial for photocatalytic activity.
The surface chemical states of the sample were checked by employing X-ray photoelectron spectroscopy. As shown in Figure 3, the XPS survey spectra reveal that the sample was composed of Bi, S, and Na elements. The peaks located at 290 eV and 530 eV correspond to C and O, which originate from the conducting resin and moisture adsorbed by the sample [23]. Two strong symmetrical peaks, located at 158.3 eV and 163.4 eV in Figure 3b, are attributed to Bi4f7/2 and Bi4f5/2 signals because of the spin-orbit splitting of Bi4f. Coincidentally, the S2p peak located at 164.03 eV, corresponding to elementary sulfur, is covered by the strong peak of Bi4f5/2. Therefore, the S2p peak is hard to discern and accurately fit. Nevertheless, the S2s peaks can be fitted to 225.2 eV [31], though the intensity is weaker (Figure 3c). The XPS spectra reveal that sulfur exists in the form of S2−. All of the specific peaks can be ascribed to the elements comprising NaBiS2 properly.
NaBiS2 was previously reported as a promising visible-light-driven photocatalyst for rhodamine B(RhB) decomposition with the assistance of H2O2, and its bandgap was evaluated as 1.13 eV [24]. The modified augmented plane wave method (WIEN2k program) and HSE06 single-point calculations were employed to study the electronic energy structure of NaBiS2. According to the difference of the theoretical model, the bandgap value varied between 1.12 eV and 1.37 eV [32,33]. The optical properties of NaBiS2 were investigated first using diffuse-reflectance UV-Vis-NIR spectrophotometry. According to the diffuse reflection spectrum curve (Figure 4a), NaBiS2 shows strong absorption from UV light (200 nm) to near-infrared light (about 1000 nm). The experimental bandgap of NaBiS2 was estimated to be 1.32 eV, based on the absorption spectra according to the Kubelka-Munk theory, using the indirect bandgap semiconductor model. The details of DOS and band structures are shown in Figure 4b–d. The DFT calculation results reveal that the valence band consisted of Bi6p and S2p, indicating strong p–p hybridization between Bi6p and S2p, which originate from the bond of Bi and S in the crystal. The conduction band is mainly composed of S2p states, mixed with a few Bi6s states. In the conduction band, strong hybridization also appears between S2p and Bi6s, which results in the formation of the anti-bonding states. The energy band structure is shown in Figure 3c. The fermi level was set as zero, shown by a dashed line. A partial enlarged view of the conduction band minimum (CBM) and valence band maximum (VBM) (Figure 4d) gives more detailed information. A slight mismatch was noted between the conduction band minimum and the valence band maximum. This implies that NaBiS2 is an indirect bandgap semiconductor, and the indirect bandgap is defined to be 1.02 eV. The recombination of photo-induced carriers is a key factor that dramatically weakens the properties of a photocatalyst. The indirect nature of the bandgap was reported to be beneficial in suppressing the radiative recombination rate due to the momentum mismatch between the CBM and VBM [34]. Thus, the photocatalytic properties of NaBiS2 are expectable. The calculated bandgap width value is smaller than the experimental result, which is possibly due to the well-known drawback of the DFT method.
The photocatalytic activity of NaBiS2 was evaluated by monitoring the decoposition of methyl blue aqueous solution. A control experiment was carried out under the full spectrum of a xenon lamp without a photocatalyst, and negligible degradation of the methyl blue was observed after 120 min irradiation. It is reasonable to believe that methyl blue is stable in an aqueous solution even under light irradiation. Subsequently, degradation experimental measurements under UV (365 ± 5 nm) and visible light (420–800 nm) demonstrated the outstanding photocatalytic activity of NaBiS2 (Figure 5a). As evaluated by the decrease in the UV–vis absorption spectra of an MB solution (Figure S1a–c), the degradation rates of MB are 72.1% and 73.3% when irradiated for 120 min with UV and visible light, respectively. Most notably, NaBiS2 revealed impressive photocatalytic activity under NIR light. In total, 50.8% of the MB was degraded after 120min irradiation.
The broadband spectrum responsiveness performance was further assessed with photocurrent measurements. When NaBiS2 modified FTO substrates were used as the working electrodes, a response photocurrent with repeatable on/off cycles upon light irradiation was observed. The photocurrent density curves under chopper light illumination are shown in Figure 5b. A sharp increase in photocurrent was recorded when the irradiation was turned on. Photocurrent is usually supposed to be relevant to the effective charge separation and charge transport over a photocatalyst’s surface [35,36]. Various photocatalysts with photo-response activity display photocurrent response well. Photocurrent measurements indicate that, in NaBiS2, electron–hole pairs generate at the moment of irradiation and can separate effectively, then transport to the surface where photocatalytic reaction occurs.
For comparison, methyl blue photocatalytic degradations by NaBiS2 and P25 (Degussa, Germany) were carried out using a xenon lamp as a full spectrum light source (Figure 5c). NaBiS2 demonstrates superior photocatalytic activity under unfiltered irradiation. The degradation rate of methyl blue reaches 99.6% after 80 min with the assistance of NaBiS2, while P25 shows lower efficiency even after 90 min irradiation. Cycle runs under the full spectrum were also carried out to check the chemical stability of NaBiS2. Though its photocatalytic performance deteriorates gradually, the degradation rate of MB still remains more than 91% after five cycle runs. The XRD result (shown in Figure S2) indicates that NaBiS2 possesses good phase stability during a photocatalytic reaction. Negligible impurity was detected and the crystal structure of NaBiS2 remained unchanged. Based on the above experimental and theoretical results, NaBiS2 is confirmed as a novel stable photocatalyst with unexpected broadband spectrum photocatalytic activity.

3. Experimental Section

3.1. Preparation and Characterization of Photocatalyst

All the chemical reagents used in this work were analytical-grade reagents without any further purification. Na2S was dried in a vacuum oven at 120 °C for 8 h in advance. In a typical synthesis procedure of NaBiS2, 10 mmol Bi(NO)3·H2O was first dispersed into 40 mL deionized water and stirred for 10 min. NaOH (0.1 mol) and Na2S (0.1 mol) were dissolved in 20 mL deionized water. Then the above solutions were mixed and sealed in a Teflon-lined stainless steel autoclave, and treated at 160 °C under autogenous pressure for 12 h. After cooling to room temperature spontaneously, the sediment was separated and washed until the filtrate was neutral. After the sediment was dried in an electric oven, characterizations were conducted. In order to determine the optimal condition for NaBiS2 synthesis, various amounts of NaOH and Na2S were employed during fabrication, comparatively following the above procedure.
The samples were analyzed by powder X-ray diffraction (XRD) with a Bruker D8-Advance diffractometer using monochromatized Cu (λ = 1.54056 nm) radiation, with a scanning speed of 0.15°/s to check the phase firstly. The morphologies of the samples were observed by a field emission scanning electron microscope (JSM-7001F, JEOL) operating at a 5 kV accelerating voltage. UV-Vis-NIR diffuser reflectance (DRS) was conducted on a UV-Vis-NIR spectrometer (PerkinElmer, Lambda 950) to estimate the absorption spectra of NaBiS2. The chemical states of the elements were measured by X-ray photoelectron spectroscopy (XPS) on a Thermo Fisher ESCALAB 250Xi instrument. The TEM images were recorded on a JEOL-JEM 2100 transmission electron microscope, using an accelerating voltage of 200 kV. The samples used for TEM observations were dispersed in ethanol, followed by ultrasonic vibration for 30 min, then a drop of the dispersion was placed onto a copper grid coated with a layer of amorphous carbon.

3.2. Photocatalytic Activity and Photochemical Measurements

The photocatalytic properties of the specimen were inspected by the photocatalytic degradation of methyl blue aqueous solution. Prior to the reaction, a 0.1 g sample was dispersed in 100 mL methyl blue solution (100 mg·L−1) and stirred in the dark for 60 min to reach the adsorption-desorption equilibrium. A 10W LED with an emission wavelength of 365 ± 5 nm was used as the UV light. Visible light (420 nm < λ < 800 nm) and NIR light (λ > 800 nm) were obtained from a 300W xenon lamp with the assistance of cutoff filters. At regular time intervals, a certain amount of suspension was collected and centrifuged, and the residual supernatant was analyzed by UV-vis spectrophotometer (UV-3100, Hitachi). Finally, the photocatalytic efficiency was calculated by C/C0 × 100% (C is the final concentration and C0 is the initial concentration of methyl blue). For stability measurements, the photocatalyst was centrifuged and collected after one photocatalysis cycle was completed, followed by washing and drying. Stability measurements were carried out under the same procedure as mentioned above.
Electrochemical measurements were performed on an electrochemical workstation (CHI 660, ChenHua, Shanghai) in 0.5mol·L−1 Na2SO4 solution as the electrolyte. A standard three-electrode cell was used, employing a platinum wire as the counter electrode and a saturated calomel electrode in saturated KCl as the reference electrode. An NaBiS2 modified FTO glass was used as the work electrode. It was fabricated as follows: 15 mg NaBiS2 was first dispersed in 1 mL Nafion (1 wt%) solution and treated by ultrasonic scatter for 5 min. Then 0.5 mL solution was dropped on the FTO glass (1.5 cm × 1.5 cm) and dried in a vacuum oven to vaporize the solvent. During all of the measurements, the photocurrent was recorded at a bias of 0 V versus the reference electrode.

3.3. Theoretical Calculation

A theoretical investigation of the energy band of NaBiS2 will be beneficial to the deep understanding of its properties. In this work, the band structures of NaBiS2 crystal, including the project density of state (PDOS) and band width, were calculated. The geometry optimization and electronic properties of crystalline NaBiS2 were calculated under the density functional theory (DFT), as implemented in the Vienna ab-initio simulation package (VASP). The projector augmented wave (PAW) potentials were used as pseudopotentials to describe the interactions between the valence electrons and ions. The Perdew–Burke–Ernzerhof (PBE) functional [37] of generalized gradient approximation (GGA) was used to describe the exchange-correlation of the valence electrons. The computational procedures were carried out as follows: an optimization process was first performed using a conjugate gradient algorithm with a force tolerance of 0.02 eV/Å and a kinetic energy cutoff set at 500 eV. A Gamma k-point mesh of size 5 × 5 × 5 was used for sampling the Brillouin zone for geometry optimization and the subsequent static calculations. The volume of the supercell was kept fixed until all forces were smaller than 0.01 eV/Å, corresponding to an energy convergence smaller than 0.0001 eV. This was small enough for the survey of the electronic structures. In total, 120 k-points were sampled along the band path in the Brillouin zone for the band diagram calculation.

4. Conclusions

In summary, NaBiS2 nanosheets were synthesized facilely through a hydrothermal method at a low temperature, based on the experience of synthesis condition control. The alkaline amount is considered to play a key role in formation of NaBiS2 and a threshold amount is needed. The as-synthesized polycrystalline NaBiS2 shows multiple atomic configurations on the nanosheet’s surface, including amorphous clusters and amorphous nano-domains. Its excellent photocatalytic activity for the degradation of MB in the range from UV to NIR light was confirmed, as well as its unexpected chemical stability under full spectrum irradiation. The band structure was theoretically investigated for the first time under the density functional theory, and NaBiS2 is believed to be an indirect bandgap semiconductor. The present work gives the opportunity for the synthesis and application of NaBiS2 as a broadband spectrum light-absorbing material.

Supplementary Materials

The following are available online at https://www.mdpi.com/2073-4344/10/4/413/s1: Figure S1: UV–vis absorption spectra curves of MB solution irradiated under UV, visible and NIR light, Figure S2: XRD patterns of NaBiS2 before and after photocatalytic reaction.

Author Contributions

H.W. designed the project, conducted most of the experiments and wrote the manuscript; Z.X. performed part of the experiments and revised the manuscript with input from all the authors; X.W. and Y.J. took part in the discussion and revision of the manuscript. All authors have read and agreed to the published version of the manuscript.

Funding

This research was funded by National Natural Science Foundation of China, grant number 21875281.

Acknowledgments

This work was supported by National Natural Science Foundation of China (No. 21875281).

Data Availability Statement

The authors confirm that the data supporting the findings of this study are available within the article and its supplementary information.

Conflicts of Interest

The authors declare no competing financial interests.

References

  1. Kubacka, A.; Fernandez-Garcia, M.; Colon, G. Advanced nanoarchitectures for solar photocatalytic applications. Chem. Rev. 2012, 112, 1555–1614. [Google Scholar] [CrossRef] [PubMed]
  2. Tong, H.; Ouyang, S.X.; Bi, Y.P.; Umezawa, N.; Oshikiri, M.; Ye, J.H. Nano-photocatalytic materials: Possibilities and challenges. Adv. Mater. 2012, 24, 229–251. [Google Scholar] [CrossRef] [PubMed]
  3. Kisch, H. Semiconductor photocatalysis--mechanistic and synthetic aspects. Angew. Chem. Int. Ed. 2013, 52, 812–847. [Google Scholar] [CrossRef] [PubMed]
  4. Zuo, C.T.; Bolink, H.J.; Han, H.W.; Huang, J.S.; Cahen, D.; Ding, L.M. Advances in perovskite solar cells. Adv. Sci. 2016, 3, 1500324.1–1500324.16. [Google Scholar] [CrossRef]
  5. Shi, Z.J.; Guo, J.; Chen, Y.H.; Li, Q.; Huang, W. Lead-free organic-inorganic hybrid perovskites for photovoltaic applications: Recent advances and perspectives. Adv. Mater. 2017, 29, 1605005.1–1605005.28. [Google Scholar] [CrossRef]
  6. Chen, B.; Zheng, X.; Bai, Y.; Padture, N.P.; Huang, J. Progress in tandem solar cells based on hybrid organic-inorganic perovskites. Adv. Energy Mater. 2017, 7, 1602400.1–1602400.19. [Google Scholar] [CrossRef]
  7. Tang, Y.; Zhang, Y.; Deng, J.; Wei, J.; Le, T.H.; Chandran, B.K.; Dong, Z.; Chen, Z.; Chen, X.D. Mechanical force-driven growth of elongated bending TiO2 -based nanotubular materials for ultrafast rechargeable lithium ion batteries. Adv. Mater. 2014, 26, 6111–6118. [Google Scholar] [CrossRef]
  8. Peng, Y.; Chen, Q.G.; Wang, D.; Zhou, H.Y.; Xu, A.W. Synthesis of one-dimensional WO3–Bi2WO6 heterojunctions with enhanced photocatalytic activity. CrystEngComm 2015, 17, 569–576. [Google Scholar] [CrossRef]
  9. Zhang, L.; Wang, W.; Zhou, L.; Xu, H. Bi2WO6 nano- and microstructures: Shape control and associated visible-light-driven photocatalytic activities. Small 2007, 3, 1618–1625. [Google Scholar] [CrossRef]
  10. Hou, Y.; Wen, Z.H.; Cui, S.M.; Guo, X.R.; Chen, J.H. Constructing 2D porous graphitic C3N4 nanosheets/nitrogen-doped graphene/layered MoS2 ternary nanojunction with enhanced photoelectrochemical activity. Adv. Mater. 2013, 25, 6291–6297. [Google Scholar] [CrossRef]
  11. Wang, S.P.; Li, C.J.; Wang, T.; Zhang, P.; Li, A.; Gong, J.L. Controllable synthesis of nanotube-type graphitic C3N4 and their visible-light photocatalytic and fluorescent properties. J. Mater. Chem. A 2014, 2, 2885–2890. [Google Scholar] [CrossRef]
  12. Wang, G.; Huang, B.; Ma, X.; Wang, Z.; Qin, X.; Zhang, X.; Dai, Y.; Whangbo, M.H. Cu2(OH)PO4, a near-infrared-activated photocatalyst. Angew. Chem. Int. Ed. 2013, 52, 4810–4813. [Google Scholar] [CrossRef] [PubMed]
  13. Sang, Y.; Zhao, Z.; Zhao, M.; Hao, P.; Leng, Y.; Liu, H. From UV to near-infrared, WS2 nanosheet: A novel photocatalyst for full solar light spectrum photodegradation. Adv. Mater. 2015, 27, 363–369. [Google Scholar] [CrossRef] [PubMed]
  14. Li, J.; Wu, X.; Pan, W.; Zhang, G.; Chen, H. Vacancy-rich monolayer BiO2-x as a highly efficient UV, visible, and near-infrared responsive photocatalyst. Angew. Chem. Int. Ed. 2018, 57, 491–495. [Google Scholar] [CrossRef]
  15. Gao, W.W.; Liu, W.X.; Leng, Y.H.; Wang, X.M.; Wang, X.Q.; Hu, B.; Yu, D.H.; Sang, Y.H.; Liu, H. In2S3 nanomaterial as a broadband spectrum photocatalyst to display significant activity. Appl. Catal. B Environ. 2015, 176, 83–90. [Google Scholar] [CrossRef]
  16. Cui, G.W.; Wang, W.; Ma, M.Y.; Xie, J.F.; Shi, X.F.; Deng, N.; Xin, J.P.; Tang, B. IR-driven photocatalytic water splitting with WO2-NaxWO3 hybrid conductor material. Nano Lett. 2015, 15, 7199–7203. [Google Scholar] [CrossRef]
  17. Sang, Y.; Liu, H.; Umar, A. Photocatalysis from UV/vis to near-infrared light: Towards full solar-light spectrum activity. ChemCatChem 2015, 7, 559–573. [Google Scholar] [CrossRef]
  18. Yuan, X.Z.; Wang, H.; Wang, J.J.; Zeng, G.M.; Chen, X.H.; Wu, Z.B.; Jiang, L.B.; Jin, T.X.; Zhang, J.; Wang, H. Near-infrared-driven Cr(vi) reduction in aqueous solution based on a MoS2/Sb2S3 photocatalyst. Catal. Sci. Technol. 2018, 8, 1545–1554. [Google Scholar] [CrossRef]
  19. Zhu, M.S.; Zhai, C.Y.; Fujitsuka, M.; Majima, T. Noble metal-free near-infrared-driven photocatalyst for hydrogen production based on 2D hybrid of black Phosphorus/WS2. Appl. Catal. B Environ. 2018, 221, 645–651. [Google Scholar] [CrossRef]
  20. Zhi, L.; Zhang, H.; Yang, Z.; Liu, W.; Wang, B. Interface coassembly of mesoporous MoS2 based-frameworks for enhanced near-infrared light driven photocatalysis. Chem. Commun. 2016, 52, 6431–6434. [Google Scholar] [CrossRef]
  21. Wu, J.; Liu, B.; Ren, Z.; Ni, M.; Li, C.; Gong, Y.; Qin, W.; Huang, Y.; Sun, C.Q.; Liu, X. CuS/RGO hybrid photocatalyst for full solar spectrum photoreduction from UV/vis to near-infrared light. J. Colloid Interface Sci. 2018, 517, 80–85. [Google Scholar] [CrossRef]
  22. Ren, Z.X.; Lei, L.; Liu, B.B.; Liu, X.J.; Li, Z.; Lei, X.; Li, C.; Gong, Y.Y.; Niu, L.Y.; Pan, l.K. Cr(VI) reduction in presence of ZnS/RGO photocatalyst under full solar spectrum radiation from UV/vis to near-infrared light. Catal. Today 2018, 315, 46–51. [Google Scholar] [CrossRef]
  23. Kang, S.; Hong, Y.; Jeon, Y. A facile synthesis and characterization of sodium bismuth sulfide (NaBiS2) under hydrothermal condition. Bull. Korean Chem. Soc. 2014, 35, 1887–1890. [Google Scholar] [CrossRef] [Green Version]
  24. Guo, J.; Ge, Z.H.; Hu, M.Y.; Qin, P.; Feng, J. Facile synthesis of NaBiS2 nanoribbons as a promising visible light-driven photocatalyst. Phys. Status Solidi-Rapid Res. Lett. 2018, 12, 1800135.1–1800135.4. [Google Scholar] [CrossRef]
  25. Liu, Z.P.; Liang, J.B.; Li, S.; Peng, S.; Qian, Y.T. Synthesis and growth mechanism of Bi2S3 nanoribbons. Chemistry 2004, 10, 634–640. [Google Scholar] [CrossRef] [PubMed]
  26. Liu, Z.; Peng, S.; Xie, Q.; Hu, Z.; Yang, Y.; Zhang, S.; Qian, Y. Large scale synthesis of ultralong Bi2S3 nanoribbon via a solvothermal process. Adv. Mater. 2003, 15, 936–940. [Google Scholar] [CrossRef]
  27. Sheets, W.C.; Stampler, E.S.; Kabbour, H.; Bertoni, M.I.; Cario, L.; Mason, T.O.; Marks, T.J.; Poeppelmeier, K.R. Facile synthesis of BiCuOS by hydrothermal methods. Inorg. Chem. 2007, 46, 10741–10748. [Google Scholar] [CrossRef]
  28. Wang, H.; Ding, J.; Xu, H.; Qiao, L.; Wang, X.; Lin, Y. One-pot synthesis of BiCuSO nanosheets under ambient atmosphere as broadband spectrum photocatalyst. Nanomaterials 2019, 9, 540. [Google Scholar] [CrossRef] [Green Version]
  29. Bi, Y.; Hu, H.; Ouyang, S.; Lu, G.; Cao, J.; Ye, J. Photocatalytic and photoelectric properties of cubic Ag3PO4 sub-microcrystals with sharp corners and edges. Chem. Commun. 2012, 48, 3748–3750. [Google Scholar] [CrossRef]
  30. Liu, C.; Kong, D.; Hsu, PC.; Yuan, H.; Lee, HW.; Liu, Y.; Wang, H.; Wang, S.; Yan, K.; Lin, D.; et al. Rapid water disinfection using vertically aligned MoS2 nanofilms and visible light. Nat. Nanotechnol. 2016, 11, 1098–1104. [Google Scholar] [CrossRef]
  31. Chang, C.; Teng, F.; Liu, Z. Fully understanding the photochemical properties of Bi2O2(CO3)1-xSx nanosheets. Langmuir 2016, 32, 3811–3819. [Google Scholar] [CrossRef] [PubMed]
  32. BaQais, A.; Nina, T.; Tangui, L.B.; Kazuhiro, T. Optoelectronic structure and photocatalytic applications of Na(Bi,La)S2 solid solutions with tunable band gaps. Chem. Mater. 2019, 31, 3211–3220. [Google Scholar] [CrossRef]
  33. Gabrel’yan, B.V.; Lavrentiev, A.A.; Nikiforov, I.Y.; Sobolev, V.V. Electronic energy structure of MBiS2 (M = Li, Na, K) calculated with allowance for the difference between the M-S and Bi-S bond lengths. J. Struct. Chem. 2008, 49, 788–794. [Google Scholar] [CrossRef]
  34. Zhang, X.; Shen, J.X.; Wang, W.N.; Van de Walle, C.G. First-principles analysis of radiative recombination in lead-halide perovskites. ACS Energy Lett. 2018, 3, 2329–2334. [Google Scholar] [CrossRef]
  35. Li, J.; Zhang, L.; Li, Y.; Yu, Y. Synthesis and internal electric field dependent photoreactivity of Bi3O4Cl single-crystalline nanosheets with high {001} facet exposure percentages. Nanoscale 2014, 6, 167–171. [Google Scholar] [CrossRef]
  36. Di, J.; Xia, J.X.; Ge, Y.P.; Li, H.P.; Ji, H.Y.; Zhang, Q.; Li, H.M.; Li, M.N. Novel visible-light-driven CQDs/Bi2WO6 hybrid materials with enhanced photocatalytic activity toward organic pollutants degradation and mechanism insight. Appl. Catal. B Environ. 2015, 168–169, 51–61. [Google Scholar] [CrossRef]
  37. Perdew, J.P.; Burke, K.; Ernzerhof, M. Generalized gradient approximation made simple. Phys. Rev. Lett. 1996, 77, 3865–3868. [Google Scholar] [CrossRef] [Green Version]
Figure 1. XRD patterns of NaBiS2. (a) a typical XRD result of NaBiS2; (b) XRD results of samples fabricated at various mole ratios of Bi(NO3):Na2S:NaOH, (1)1:2:2; (2)1:5:2; (3)1:5:5; (4)1:2:10; (5)1:5:10; (6)1:10:10.
Figure 1. XRD patterns of NaBiS2. (a) a typical XRD result of NaBiS2; (b) XRD results of samples fabricated at various mole ratios of Bi(NO3):Na2S:NaOH, (1)1:2:2; (2)1:5:2; (3)1:5:5; (4)1:2:10; (5)1:5:10; (6)1:10:10.
Catalysts 10 00413 g001
Figure 2. The morphology characterization of NaBiS2. (a) SEM pattern; (b) low magnified TEM graph; (c) high magnified TEM graph, with nano-domains labelled.
Figure 2. The morphology characterization of NaBiS2. (a) SEM pattern; (b) low magnified TEM graph; (c) high magnified TEM graph, with nano-domains labelled.
Catalysts 10 00413 g002
Figure 3. XPS spectra patterns of (a) full span, (b) Bi4f, (c) S2s, and (d) Na1s.
Figure 3. XPS spectra patterns of (a) full span, (b) Bi4f, (c) S2s, and (d) Na1s.
Catalysts 10 00413 g003
Figure 4. (a) UV-vis-NIR absorbance spectra of NaBiS2. Insert shows the bandgap estimated by the Kubelka–Munk method. (b) Density of states near the Fermi level and (c,d) the valence band maximum and the conduction band minimum.
Figure 4. (a) UV-vis-NIR absorbance spectra of NaBiS2. Insert shows the bandgap estimated by the Kubelka–Munk method. (b) Density of states near the Fermi level and (c,d) the valence band maximum and the conduction band minimum.
Catalysts 10 00413 g004
Figure 5. Photocatalytic activity and photocurrent measurement. (a) Degradation of MB with the irradiation of UV, visible and NIR light; (b) photocurrent density under UV, visible and NIR light; (c) degradation of MB with the full spectrum, compared with P25 without any other additive; (d) cycle runs under the full spectrum.
Figure 5. Photocatalytic activity and photocurrent measurement. (a) Degradation of MB with the irradiation of UV, visible and NIR light; (b) photocurrent density under UV, visible and NIR light; (c) degradation of MB with the full spectrum, compared with P25 without any other additive; (d) cycle runs under the full spectrum.
Catalysts 10 00413 g005

Share and Cite

MDPI and ACS Style

Wang, H.; Xie, Z.; Wang, X.; Jia, Y. NaBiS2 as a Novel Indirect Bandgap Full Spectrum Photocatalyst: Synthesis and Application. Catalysts 2020, 10, 413. https://doi.org/10.3390/catal10040413

AMA Style

Wang H, Xie Z, Wang X, Jia Y. NaBiS2 as a Novel Indirect Bandgap Full Spectrum Photocatalyst: Synthesis and Application. Catalysts. 2020; 10(4):413. https://doi.org/10.3390/catal10040413

Chicago/Turabian Style

Wang, Huanchun, Zheng Xie, Xuanjun Wang, and Ying Jia. 2020. "NaBiS2 as a Novel Indirect Bandgap Full Spectrum Photocatalyst: Synthesis and Application" Catalysts 10, no. 4: 413. https://doi.org/10.3390/catal10040413

APA Style

Wang, H., Xie, Z., Wang, X., & Jia, Y. (2020). NaBiS2 as a Novel Indirect Bandgap Full Spectrum Photocatalyst: Synthesis and Application. Catalysts, 10(4), 413. https://doi.org/10.3390/catal10040413

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop